Phase development and critical current density of Bi-2223 tapes fabricated by groove rolling

被引:8
|
作者
Iyer, AN [1 ]
Salib, S
Vipulanandan, C
Salama, K
Balachandran, U
机构
[1] Univ Houston, Texas Ctr Superconduct, Houston, TX 77204 USA
[2] McDermott Energy Serv, Houston, TX 77079 USA
[3] Argonne Natl Lab, Div Energy Technol, Argonne, IL 60439 USA
来源
SUPERCONDUCTOR SCIENCE & TECHNOLOGY | 1999年 / 12卷 / 07期
关键词
D O I
10.1088/0953-2048/12/7/306
中图分类号
O59 [应用物理学];
学科分类号
摘要
The powder-in-tube technique is the most widely used method for fabricating silver-clad Bi-2223 wires and tapes. In this method the silver biller containing the precursor material is transformed to the final shape using metallurgical deformation techniques such as wire drawing and flat rolling. In the present study, a modified version of the powder-in-tube technique was adopted where the silver biller was reduced in size by groove rolling instead of wire drawing. Microstructural analysis during the initial deformation stage revealed crack formation in the superconductor core. Stress conditions during groove rolling were analysed and appropriate changes were incorporated in the deformation process. After groove rolling the wires were flat rolled to a final thickness of 250 mu m. Subsequent thermomechanical treatment resulted in tapes with critical current density of approximate to 19 700 A cm(-2) (critical current of approximate to 40 A).
引用
收藏
页码:436 / 441
页数:6
相关论文
共 50 条
  • [31] Critical current density and current-voltage characteristics in Ag-sheathed Bi-2223 tapes
    Mawatari, Y.
    Yamasaki, H.
    Kosaka, S.
    Umeda, M.
    Denshi Gijutsu Sogo Kenkyusho Iho/Bulletin of the Electrotechnical Laboratory, 1995, 59 (11-12): : 75 - 84
  • [32] Critical current and strain tolerance of Bi-2223/Ag multifilament tapes
    Savvides, N
    Thorley, A
    Reilly, D
    ADVANCES IN CRYOGENIC ENGINEERING MATERIALS, VOL 44, PTS A AND B, 1998, 44 : 569 - 576
  • [33] Effects of precursor powder calcination on critical current density and microstructure of Bi-2223/Ag tapes
    Jiang, J
    Abell, JS
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1997, 10 (09): : 678 - 685
  • [34] Transverse compressive stress effects on the critical current of Bi-2223 tapes
    Li, C. S.
    Mossang, E.
    Bellin, B.
    Sulpice, A.
    Antonevici, A.
    Zhang, P. X.
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 1923 - +
  • [35] Response of Bi-2223 tapes to over-critical current excursions
    Stavrev, S
    Dutoit, B
    Friend, C
    PHYSICA C, 2000, 339 (02): : 69 - 74
  • [36] Multifracture and strain effects on the critical current of Bi-2223 superconducting tapes
    Lu, ZY
    Huang, XQ
    He, YF
    Li, JH
    Sun, J
    Wang, YN
    Zong, XH
    Wang, JX
    Chen, LY
    Li, CS
    Zhang, PX
    Feng, Y
    Zhou, L
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2003, 386 : 150 - 153
  • [37] Temperature-dependent critical current anisotropy in Bi-2223 tapes
    Lehndorff, B
    Hortig, M
    Piel, H
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1998, 11 (11): : 1261 - 1265
  • [38] Effects of mechanical deformation on critical current of Bi-2223/Ag tapes
    Horvat, J
    Guo, YC
    Bhasale, R
    Ionescu, M
    Dou, SX
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1998, 11 (10): : 1098 - 1100
  • [39] Critical current density significantly enhanced by hot pressing in Bi-2223/Ag multifilamentary tapes
    Zeng, R
    Ye, B
    Horvat, J
    Guo, YC
    Zeimetz, B
    Yang, XF
    Beales, TP
    Liu, HK
    Dou, SX
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1998, 11 (10): : 1101 - 1104
  • [40] Significantly enhanced critical current density in Bi-2223/Ag multifilamentary tapes by hot pressing
    Zeng, R
    Ye, B
    Horvat, J
    Guo, YC
    Zeimetz, B
    Yang, XF
    Beales, TP
    Liu, HK
    Dou, SX
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1999, 9 (02) : 2742 - 2745