Effect of nitrogen ion implantation on corrosion inhibition of nickel coated 316 stainless steel and correlation with nano-structure

被引:23
|
作者
Grayeli-Korpi, Ali-Reza [1 ]
Savaloni, Hadi [1 ]
机构
[1] Univ Tehran, Dept Phys, Tehran, Iran
基金
美国国家科学基金会;
关键词
Ion implantation; Stainless steel; Corrosion; Ni thin film; BEHAVIOR; SURFACE; FILM;
D O I
10.1016/j.apsusc.2012.06.060
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The influence of implantation of N+ with 20 keV energy and different fluences in the range of 1 x 10(17) and 5 x 10(18) ions/cm(2) in the nickel coated type 316 stainless steel (SS) on the corrosion inhibition of SS in 3.5 wt% NaCl solution is investigated. The highest available N+ fluence showed highest corrosion inhibition. X-ray diffraction (XRD) analysis showed formation of nickel nitride phases that enhanced by increasing the N+ fluence. Surface morphology was studied by atomic force microscope (AFM) and scanning electron microscope (SEM) before and after corrosion test, respectively. AFM results showed that by increasing N+ fluence surface of the sample becomes smoother that may be the result of heat accumulation during implantation causing higher rate of diffusion in the sample. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:9982 / 9988
页数:7
相关论文
共 50 条
  • [41] INFLUENCE OF NITROGEN AND MOLYBDENUM ION-IMPLANTATION OF AUSTENITIC STAINLESS-STEEL ON STRESS-CORROSION CRACKING
    SARRAZIN, C
    DESJARDINS, D
    OLIVE, JM
    KARRAY, R
    MEMOIRES ET ETUDES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1991, 88 (11): : 761 - 769
  • [42] CAVITATION EROSION OF AUSTENITIC STAINLESS-STEEL AND EFFECT OF BORON AND NITROGEN ION-IMPLANTATION
    KARIMI, A
    ACTA METALLURGICA, 1989, 37 (04): : 1079 - 1088
  • [43] Structure and composition effects on pitting corrosion resistance of austenitic stainless steel after molybdenum ion implantation
    Mottu, N
    Vayer, M
    Dudognon, J
    Erre, R
    SURFACE & COATINGS TECHNOLOGY, 2005, 200 (07): : 2131 - 2136
  • [44] Effect of sandblasting, annealing and hydrophobic treatment on the nano-mechanical and corrosion behaviour of n-TiO2-coated 316L stainless steel
    Ahmad, Zaki
    Patel, Faheemuddin
    Mastoi, Naila Riaz
    Saddiqa, Ayesha
    CURRENT SCIENCE, 2016, 110 (03): : 353 - 362
  • [45] Effect of temperature on pitting corrosion resistance of 316 stainless steel coated by cerium oxide film in 3.5% NaCl solution
    Hasannejad, H.
    Shahrabi, T.
    Rouhaghdam, A. Sabour
    Aliofkhazraei, M.
    Journal of Materials Science and Technology, 2008, 24 (05): : 715 - 717
  • [46] Effect of Temperature on Pitting Corrosion Resistance of 316 Stainless Steel Coated by Cerium Oxide Film in 3.5% NaCl Solution
    H.Hasannejad
    T.Shahrabi
    A.Sabour Rouhaghdam
    M.Aliofkhazraei
    JournalofMaterialsScience&Technology, 2008, (05) : 715 - 717
  • [47] Effect of Temperature on Pitting Corrosion Resistance of 316 Stainless Steel Coated by Cerium Oxide Film in 3.5% NaCl Solution
    Hasannejad, H.
    Shahrabi, T.
    Rouhaghdam, A. Sabour
    Aliofkhazraei, M.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2008, 24 (05) : 715 - 717
  • [48] Effect of nitrogen concentration on nano-structure and high-temperature strength of 9Cr-ODS steel
    Oka, Hiroshi
    Tanno, Takashi
    Ohtsuka, Satoshi
    Yano, Yasuhide
    Kaito, Takeji
    NUCLEAR MATERIALS AND ENERGY, 2018, 16 : 230 - 237
  • [49] Effect of grain size on the corrosion resistance of a high nitrogen-low nickel austenitic stainless steel
    Di Schino, A
    Kenny, JM
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2002, 21 (24) : 1969 - 1971
  • [50] Corrosion inhibition of AISI 304-and AISI 316-type stainless steel coated with nickel oxide in H2SO4 as a function of annealing temperature
    Savaloni, Hadi
    Kazemi, Zahra Sadat
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2021, 127 (06):