Influence of microstructure and strain rate on adiabatic shearing behavior in Ti-6Al-4V alloys

被引:83
|
作者
Liu, Xinqin [1 ]
Tan, Chengwen [1 ,2 ,3 ]
Zhang, Jing [1 ]
Hu, Yangguang [1 ]
Ma, Honglei [2 ,3 ]
Wang, Fuchi [1 ]
Cai, Hongnian [1 ]
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, Beijing 100081, Peoples R China
[2] Beijing Inst Technol, Lab Adv Mat Behav Characterist, Beijing 100081, Peoples R China
[3] Inst Space Medicoengn, Beijing 100081, Peoples R China
关键词
Ti-6Al-4V; Microstructure; Strain rate; Adiabatic shear band; Fracture; DYNAMIC DEFORMATION-BEHAVIOR; IMPACT; BANDS;
D O I
10.1016/j.msea.2008.09.076
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Adiabatic shearing behavior of Ti-6Al-4V alloys with bimodal and lamellar microstructures is investigated at strain rates ranging from 10(3) s(-1) to 10(4) s(-1) by Spilt Hopkinson Pressure Bar and Taylor impact. The characteristic of fracture is closely related with the behavior of adiabatic shear band in Ti-6Al-4V alloys. In bimodal microstructure at strain rate of 10 3 s(-1), the adiabatic shear bands are regularly spaced and orientated along the maximum shear stress plane. In case of the lamellar microstructure, when the strain rates increase from 4000 s(-1) to 6000 s(-1), the adiabatic shear bands go through the transition from self-organization to branching off and interconnecting into a net-like structure. At strain rate of 10(4) s(-1) by Taylor impact, the regularly spaced adiabatic shearing cracks cause that the fracture surface makes an an angle of 45 degrees with the impacted end of the projectile in bimodal microstructure. The net-like adiabatic shearing cracks in lamellar microstructure result in the fragmentation of the projectile head, the angle is about 0 degrees. (c) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:30 / 36
页数:7
相关论文
共 50 条
  • [31] Deformation Mechanisms of Ti-6Al-4V During Tensile Behavior at Low Strain Rate
    M. Vanderhasten
    L. Rabet
    B. Verlinden
    Journal of Materials Engineering and Performance, 2007, 16 : 208 - 212
  • [32] Modification of the MTS model for high strain-rate behavior of TI-6AL-4V
    Allen, Jason
    Garmestani, Hamid
    MATERIALS RESEARCH EXPRESS, 2023, 10 (08)
  • [33] STRAIN BEHAVIOR OF THE HYDROGENATED SUBMICROCRYSTALLINE Ti-6Al-4V ALLOY
    Stepanova, E. N.
    Grabovetskaya, G. P.
    Zabudchenko, O. V.
    Mishin, I. P.
    RUSSIAN PHYSICS JOURNAL, 2011, 54 (06) : 690 - 696
  • [34] Distribution and evolution of strain and temperature in adiabatic shear band for Ti-6Al-4V
    Wang Xuebin
    RARE METAL MATERIALS AND ENGINEERING, 2006, 35 (12) : 1854 - 1858
  • [35] THE STRAIN-HARDENING BEHAVIOR OF SUPERPLASTIC TI-6AL-4V
    MEIER, M
    MUKHERJEE, AK
    SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (02): : 331 - 336
  • [36] Effects of microstructure on the subsurface crack initiation of Ti-6Al-4V alloys
    Umezawa, O
    Nagai, K
    Yokoyama, H
    Suzuki, T
    HIGH CYCLE FATIGUE OF STRUCTURAL MATERIALS, 1997, : 287 - 298
  • [37] Effect of microstructure on the fatigue properties of Ti-6Al-4V titanium alloys
    Wu, G. Q.
    Shi, C. L.
    Sha, W.
    Sha, A. X.
    Jiang, H. R.
    MATERIALS & DESIGN, 2013, 46 : 668 - 674
  • [38] Effect of Microstructure on the Creep Properties of Ti-6Al-4V Alloys: An Analysis
    Sahoo, R.
    Jha, B. B.
    Sahoo, T. K.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (07) : 1573 - 1582
  • [39] THE EFFECT OF STRAIN, STRAIN RATE AND TEMPERATURE ON FORMABILITY OF TI-6AL-4V ALLOY
    ELDOMIATY, A
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1992, 32 (1-2) : 243 - 251
  • [40] Influence of Annealing Treatment on Microstructure and Mechanical Properties of Graded Structure Ti-6Al-4V Alloys
    Zhao Shuo
    Hou Wentao
    Hao Yulin
    Liu Yujing
    Zhang Laichang
    Li Shujun
    Yang Rui
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 : 195 - 199