Smelting of a flotation gold-containing concentrate with the use of a copper collector and slag of the four-component system SiO(2)-FeO-Na(2)O-CaO is studied. Optimum parameters are determined for the preliminary roasting of the concentrate (t = 750-800 degrees C, tau = 45-60 min) and its smelting (t = 1200-1250 degrees C, tau = 50-60 min, time of metal-slag stratification is 45 min, concentrate-to-carbon ratio is 10 : 1). It is shown that as the last parameter decreases (below 10 : 1), reduction of hematite and magnetite to metal iron starts with the subsequent transfer of iron into copper. For a fourfold recycling of the copper collector, the extraction of gold was 99.5% and that of silver was 77.7%.
机构:
Moscow Institute of Steel and Alloys, Leninskii pr. 4, MoscowMoscow Institute of Steel and Alloys, Leninskii pr. 4, Moscow
Boboev I.R.
Strizhko L.S.
论文数: 0引用数: 0
h-index: 0
机构:
Moscow Institute of Steel and Alloys, Leninskii pr. 4, MoscowMoscow Institute of Steel and Alloys, Leninskii pr. 4, Moscow
Strizhko L.S.
Bobozoda S.
论文数: 0引用数: 0
h-index: 0
机构:
Moscow Institute of Steel and Alloys, Leninskii pr. 4, Moscow
Ministry of Industry and New Technologies of Tajikistan, DushanbeMoscow Institute of Steel and Alloys, Leninskii pr. 4, Moscow
Bobozoda S.
Gorbunov E.P.
论文数: 0引用数: 0
h-index: 0
机构:
Moscow Institute of Steel and Alloys, Leninskii pr. 4, MoscowMoscow Institute of Steel and Alloys, Leninskii pr. 4, Moscow