Electrophoretic deposition of mullite based oxygen diffusion systems on C/C-Si-SiC composites

被引:3
|
作者
Damjanovic, T.
Argirusis, Chr.
Jokanovic, B.
Borchardt, G.
Moritz, K.
Mueller, E.
Herbig, R.
Weiss, R.
机构
[1] Tech Univ Clausthal, Inst Met, D-38678 Clausthal Zellerfeld, Germany
[2] TU Bergakad Freiberg, Inst Keram Werkstoffe, D-09596 Freiberg, Germany
[3] Schunk Kohlenstofftech GmbH, D-35452 Heuchelheim, Germany
关键词
mullite; EPD; C/C-Si-SiC composites; cyclic oxidation;
D O I
10.4028/www.scientific.net/KEM.314.201
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Combining sol-gel synthesis of 3/2 mullite through hydrolysis and condensation of tetraethoxysilane and aluminum-tri-sec-butylate with electrophoretic deposition (EPD) yields sufficiently thick and homogeneous layers which transform into mullite at T ? 1000 degrees C. The characterisation of the mullite precursor during synthesis was performed through electroacustic measurements. The protectiveness of the deposited mullite layers was tested in air in the temperature range 1200 degrees C <= T <= 1550 degrees C by means of isothermal thermogravimetric analysis for up to 200 hours. Comparing the oxidation rate of mullite coated C/C-Si-SiC samples to that of uncoated reference samples clearly demonstrated that mullite offers a significant improvement to the oxidation resistance of the uncoated material. At temperatures above 1600 degrees C the protectiveness of the deposited layer is reduced due to the existence of a liquid phase and the formation of CO bubbles above the cracks in the SiC layer. In order to prolong the protectiveness of our mullite layers at higher temperatures we deposited an additional layer from a suspension of mullite precursor with 5 wt. % of Al2O3 powder. The protectiveness of so obtained mullite and mullite/ Al2O3 layers was also tested under cyclic conditions at 1500 degrees C and 1550 degrees C. These experiments clearly demonstrated that all samples withstood at least for 4-10 cycles which were performed subsequently in different time intervals (from 2-3 days to 1 h).
引用
收藏
页码:201 / 206
页数:6
相关论文
共 50 条
  • [31] Controlling the Si/C ratio in SiC matrix based on the modified polymethysilane for C/C-SiC composites with enhanced mechanical properties
    Liao, Mingdong
    Hu, Xiebo
    Zhong, Chenghao
    Xu, Ping
    Wang, Xiaodong
    Zhang, Ze
    Zhou, Peng
    Zhang, Mingyu
    Su, Zhean
    Huang, Qizhong
    JOURNAL OF ADVANCED CERAMICS, 2024, 13 (02): : 220 - 236
  • [32] Mechanism of synthesizing dense Si–SiC matrix C/C composites
    Shigeru Hanzawa
    Journal of Materials Science, 2012, 47 : 833 - 844
  • [33] Fabrication and properties of SiC/Zr-Si-C/SiC coated on the surface of C/SiC composites
    Li, W. (liwei3205@163.com), 2013, Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China (42):
  • [34] Oxidation protection and behavior of C/C composites with an in situ SiC nanowire-SiC-Si/SiC-Si coating
    Chu, Yanhui
    Li, Hejun
    Fu, Qiangang
    Qi, Lehua
    Li, Lu
    Liu, Yangtong
    CORROSION SCIENCE, 2013, 70 : 285 - 289
  • [35] Simulation of hyperthermal deposition of Si and C on SiC surfaces
    Alfonso, DR
    Ulloa, SE
    APPLIED PHYSICS LETTERS, 1999, 74 (01) : 55 - 57
  • [36] C/C-SiC composites for advanced friction systems
    Krenkel, W
    Heidenreich, B
    Renz, R
    ADVANCED ENGINEERING MATERIALS, 2002, 4 (07) : 427 - 436
  • [37] Electrophoretic Deposition of the Thiophene-Based Copolymer and Its Composites with C60
    Tada, Kazuya
    JOURNAL OF PHYSICAL CHEMISTRY B, 2013, 117 (06): : 1628 - 1632
  • [38] Effects of electrophoretic deposition time and heat treatment on mechanical properties of carbon nanotubes reinforced C/SiC composites
    Mei, Hui
    Xiao, Shanshan
    Bai, Qianglai
    Li, Haiqing
    Cheng, Laifei
    Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2014, 42 (12): : 1479 - 1486
  • [39] Oxidation Resistant Behaviour of Mullite/Yttrium Silicate Multilayer Coating for C/SiC Composites at 1500 °C
    Zhao, Shuang
    Zhou, Xingui
    Wang, Honglei
    HIGH-PERFORMANCE CERAMICS VIII, 2014, 602-603 : 430 - 433
  • [40] Oxidation protection of C/C composites with a multilayer coating of SiC and Si plus SiC plus SiC nanowires
    Chu Yanhui
    Li Hejun
    Fu Qiangang
    Wang Haipeng
    Hou Xianghui
    Zou Xu
    Shang Gunan
    CARBON, 2012, 50 (03) : 1280 - 1288