Effects of cold rolling on microstructure and mechanical properties of Fe-30Mn-3Si-4Al-0.093C TWIP steel

被引:47
|
作者
Shen, Y. F. [1 ,3 ]
Qiu, C. H. [1 ]
Wang, L. [2 ]
Sun, X. [3 ]
Zhao, X. M. [4 ]
Zuo, L. [1 ]
机构
[1] Key Lab Anisotropy & Texture Mat MOE, Shenyang 110004, Peoples R China
[2] Baoshan Iron & Steel Co LTD, R&D Ctr, Automobile Steel Dept, Shanghai 201900, Peoples R China
[3] Pacific NW Natl Lab, Computat Sci & Math Div, Richland, WA 99352 USA
[4] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110004, Peoples R China
基金
中国国家自然科学基金;
关键词
Fe-30Mn-3Si-4Al steel; Cold rolling; Mechanical properties; Deformation twinning; STACKING-FAULT ENERGY; DEFORMATION-BEHAVIOR; TRIP/TWIP STEELS; TEXTURE; SINGLE; MODEL; SLIP;
D O I
10.1016/j.msea.2012.10.020
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of cold rolling on microstructure evolution and the associated mechanical properties of Fe-30Mn-3Si-4Al-0.093C twinning-induced plasticity (TWIP) steel are examined in this work with reduction levels of 10%, 20%, 30%, 40%, 50%, 60%, and 70%. Through texture analysis and transmission electron microscopy (TEM) observations, it is suggested that slip, mechanical twinning, the interaction between dislocation/twin boundaries (TB), and shear band formation have influenced the observed mechanical behavior and development of texture. Special components of weak initial textures are preferential for mechanical twinning, resulting in an increase in strain hardening rate. By mechanical twinning, the {1 1 1} < 1 1 2 > orientation is rotated into a position at the vicinity of the {1 1 0} < 0 0 1 > Goss orientation, and the {5 5 2} < 1 1 5 > (Cu-twin) texture is transformed to the {1 1 0} < 0 0 1 > orientation. The evolution of texture is closely related to the onset of shear banding resulting from deformation twinning. The sample with 10% cold reduction exhibits a favorable combination of yield strength and ductility, indicating a considerable capacity for energy absorption. With increasing rolling reductions, the deformation of the samples becomes inhomogeneous due to the high anisotropy of the microstructure. The localized shear bands resulting from the excessive cold rolling are detrimental to the ductility of the present TWIP steel. (C) 2012 Elsevier B.V. All rights reserved.
引用
下载
收藏
页码:329 / 337
页数:9
相关论文
共 50 条
  • [41] Microstructural evolution and crystallographic texture formation of cold rolled austenitic Fe-30Mn-3Al-3Si TWIP-steel
    Vercammen, S
    De Cooman, BC
    Akdut, N
    Blanpain, B
    Wollants, P
    STEEL RESEARCH INTERNATIONAL, 2003, 74 (06): : 370 - 375
  • [42] Effect of Solution Treatment on Structure and Mechanical Properties of Fe-Mn-Al-Si Light Steel After Cold Rolling
    Yao, Liang
    Shi, Wen
    PROCEEDINGS OF SAE-CHINA CONGRESS 2016: SELECTED PAPERS, 2017, 418 : 313 - 325
  • [43] Microstructure and mechanical properties of C-Si-Mn TRIP steel prepared by hot rolling
    Faculty of Material and Chemical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, China
    不详
    Cailiao Kexue yu Gongyi, 2008, 3 (319-321):
  • [44] Effects of strain rate on mechanical properties and deformation behavior of an austenitic Fe-25Mn-3Al-3Si TWIP-TRIP steel
    Benzing, J. T.
    Poling, W. A.
    Pierce, D. T.
    Bentley, J.
    Findley, K. O.
    Raabe, D.
    Wittig, J. E.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 711 : 78 - 92
  • [45] Microstructures and Mechanical Properties of Fe-Mn-(Al, Si) TRIP/TWIP Steels
    DING Hua~1
    2. Continuous Casting Center
    Journal of Iron and Steel Research(International), 2006, (06) : 66 - 70
  • [46] Microstructures and Mechanical Properties of Fe-Mn-(Al, Si) TRIP/TWIP Steels
    Hua Ding
    Zheng-You Tang
    Wei Li
    Mei Wang
    Dan Song
    Journal of Iron and Steel Research International, 2006, 13 : 66 - 70
  • [47] Microstructures and mechanical properties of Fe-Mn-(Al, Si) TRIP/TWIP steels
    Ding Hua
    Tang Zheng-you
    Li Wei
    Wang Mei
    Song Dan
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2006, 13 (06) : 66 - 70
  • [48] Adjusting the microstructure evolution, mechanical properties and deformation behaviors of Fe-5.95Mn-1.55Si-1.03Al-0.055C medium Mn steel by cold-rolling reduction ratio
    Yan, Shu
    Li, Tianle
    Liang, Taosha
    Liu, Xianghua
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (02): : 1314 - 1324
  • [49] Effect of Temperature on Microstructure and Deformation Mechanism of Fe-30Mn-3Si-4Al TWIP Steel at Strain Rate of 700 s-1
    Zhi-ping XIONG
    Xue-ping REN
    Jian SHU
    Zhe-lei WANG
    Wei-ping BAO
    Shu-xia LI
    Journal of Iron and Steel Research(International), 2015, 22 (02) : 179 - 184
  • [50] Influence of cold forging and annealing on microstructure and mechanical properties of a high-Mn TWIP steel
    Kusakin, P.
    Kalinenko, A.
    Tsuzaki, K.
    Belyakov, A.
    Kaibyshev, R.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2017, 55 (03): : 161 - 167