Grain refinement of AZ91D alloy by intensive melt shearing and its persistence after remelting and isothermal holding

被引:0
|
作者
Zuo Yubo [1 ,2 ]
Fan Zhongyun [2 ]
Cui Jianzhong [1 ]
机构
[1] Northeastern Univ, Minist Educ, Key Lab Electromagnet Proc Mat, Shenyang 110819, Peoples R China
[2] Brunel Univ, BCAST, LiME, EPSRC Ctr Innovat Mfg Liquid Met Engn, Uxbridge UB8 3PH, Middx, England
基金
中国国家自然科学基金; 英国工程与自然科学研究理事会;
关键词
magnesium alloy; microstructure; intensive melt shearing; remelting; isothermal holding; ENHANCED HETEROGENEOUS NUCLEATION; MAGNESIUM ALLOYS; AL-ALLOYS; ADDITIONS; MECHANISM;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Intensive melt shearing has a significant grain refining effect on some light alloys. However, the persistence of the grain refining effect during isothermal holding and remelting is still unclear, although it is very important for the practical application. In this study, intensive melt shearing was achieved in a twin-screw mechanism to investigate its grain refining effect on AZ91D magnesium alloy. The refinement mechanism was discussed and the persistence of grain refinement after remelting and isothermal holding was also studied. A Zeiss imaging system with polarized light was used for quantitative measurement of grain size. The results show that the intensive melt shearing has a significant grain refining effect on AZ91D magnesium alloy. With the application of intensive melt shearing, the grain size of AZ91D magnesium alloy can be reduced from 530 mu m (for a typical as-cast microstructure) to 170 mu m, which is about 70% size reduction. The grain refinement achieved by the intensive melt shearing can be partially kept after isothermal holding and remelting. It is believed that the refinement effect was mainly due to the finer and well dispersed oxide particles formed by high intensive shearing. The smaller size of oxide particles and their slow motion velocity in the sheared melt could make important contributions to the remained grain refinement.
引用
收藏
页码:39 / 42
页数:4
相关论文
共 50 条
  • [21] Time evolution of agglomerate size of semisolid magnesium alloy AZ91D during a real isothermal shearing
    Li, Liang
    Zheng, Mian
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2017, 108 (08) : 643 - 647
  • [22] Grain refinement of AZ91D magnesium alloy by Al-Ti-B master alloy and its effect on mechanical properties
    Chen, T. J.
    Wang, R. Q.
    Ma, Y.
    Hao, Y.
    MATERIALS & DESIGN, 2012, 34 : 637 - 648
  • [23] Effect of isothermal holding parameters on the solid particles evolution of semisolid AZ91D alloy produced by SIMA
    Zhang, Qianqian
    Cao, Zhanyi
    ADVANCED MATERIALS AND PROCESSES, PTS 1-3, 2011, 311-313 : 1901 - +
  • [24] High energy impact techniques application for surface grain refinement in AZ91D magnesium alloy
    Hou, Li-feng
    Wei, Ying-hui
    Liu, Bao-sheng
    Xu, Bing-she
    JOURNAL OF MATERIALS SCIENCE, 2008, 43 (13) : 4658 - 4665
  • [25] Grain refinement of magnesium alloy AZ91D cast in permanent mold using mechanical vibrations
    Maltais, A
    Fiset, M
    Dubé, D
    THERMEC'2003, PTS 1-5, 2003, 426-4 : 527 - 532
  • [26] High energy impact techniques application for surface grain refinement in AZ91D magnesium alloy
    Li-feng Hou
    Ying-hui Wei
    Bao-sheng Liu
    Bing-she Xu
    Journal of Materials Science, 2008, 43 : 4658 - 4665
  • [27] Superplastic anisotropic behavior in magnesium alloy of AZ91D grain refined by isothermal-rolling
    Torisaka, Y
    Fudetani, S
    Horihata, M
    Hirohasi, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2005, 91 (08): : 647 - 654
  • [28] Microstructure refinement of AZ91D alloy solidified with pulsed magnetic field
    汪彬
    杨院生
    周吉学
    童文辉
    Transactions of Nonferrous Metals Society of China, 2008, (03) : 536 - 540
  • [29] Microstructure refinement of AZ91D alloy solidified with pulsed magnetic field
    Wang Bin
    Yang Yuan-sheng
    Zhou Ji-xue
    Tong Wen-hui
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2008, 18 (03) : 536 - 540
  • [30] Superplastic behavior in Mg-Al alloy, AZ91D grain refined by isothermal-rolling
    Torisaka, Y
    Fudetani, S
    Hirohashi, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2004, 90 (01): : 21 - 26