Long-term Bond of Glass Ceramic and Resin Cement: Evaluation of Titanium Tetrafluoride as an Alternative Etching Agent for Lithium Disilicate Ceramics

被引:23
|
作者
Klosa, Karsten [1 ]
Boesch, Ineke [1 ]
Kern, Matthias [1 ]
机构
[1] Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, D-24105 Kiel, Germany
来源
JOURNAL OF ADHESIVE DENTISTRY | 2013年 / 15卷 / 04期
关键词
tensile bond strength; etching; lithium disilicate ceramic; titanium tetrafluoride; artificial aging; COMPOSITE FILLING MATERIALS; WATER SORPTION; EROSION; ENAMEL; DURABILITY; STRENGTH; TIF4;
D O I
10.3290/j.jad.a29381
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate in vitro the effect of using titanium tetrafluoride as an alternative etchant prior to the silanization of the bonding surface on the long-term resin bond strength to lithium disilicate ceramic. Materials and Methods: Disk-shaped specimens made of lithium disilicate ceramic were ground with abrasive paper, then etched with aqueous solutions (2.5% and 5%) of titanium tetrafluoride for 60 s, 120 s and 240 s. Positive control specimens were etched with 5% hydrofluoric acid for 20 s and negative control specimens were not etched. Afterwards, bonding surfaces of all specimens were silanized. Plexiglas tubes filled with a composite resin were bonded to the specimens using an alignment apparatus and a composite luting resin. After storage in 37 degrees C tap water for three days (n = 8) and after storage in 37 degrees C tap water for 150 days interrupted by 5 x 7500 thermal cycles (n = 8), tensile bond strength (TBS) was measured in a universal testing machine at a crosshead speed of 2 mm/min. Results: After artificial aging, all specimens etched with titanium tetrafluoride debonded spontaneously resulting in a TBS of 0 MPa. Therefore, statistical analysis revealed a highly significant difference between the positive control and the test groups after 150 days storage. Conclusion: Etching the bonding surface of lithium disilicate ceramic restorations with hydrofluoric acid is still a "gold standard" and cannot be replaced by titanium tetrafluoride.
引用
收藏
页码:377 / 383
页数:7
相关论文
共 50 条
  • [21] Effect of reaction layer removal methods on bond strength of pressed lithium disilicate ceramic to resin cement
    Bauken, Gabriel
    Packaeser, Maria Gabriela
    Pilecco, Rafaela Oliveira
    Machry, Renan Vaz
    Pereira, Gabriel Kalil Rocha
    Valandro, Luiz Felipe
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2025, 140
  • [22] Influence of cleaning methods on the bond strength of resin cement to saliva-contaminated lithium disilicate ceramic
    Yoshida, Keiichi
    CLINICAL ORAL INVESTIGATIONS, 2020, 24 (06) : 2091 - 2097
  • [23] Influence of cleaning methods on the bond strength of resin cement to saliva-contaminated lithium disilicate ceramic
    Keiichi Yoshida
    Clinical Oral Investigations, 2020, 24 : 2091 - 2097
  • [24] Impact of various surface treatments on the shear bond strength between lithium disilicate ceramics and resin cement
    Alrabeah, Ghada
    Alhamid, Reem F.
    Alamer, Buthainah A.
    Alrajhi, Farah N.
    Binrayes, Abdulaziz
    Habib, Syed Rashid
    FRONTIERS IN MATERIALS, 2024, 11
  • [25] Long-term retention of lithium disilicate crowns with a current bioactive cement
    Streiff, Kerry R.
    Lepe, Xavier
    Johnson, Glen H.
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2021, 33 (04) : 621 - 627
  • [26] Long-term resin bond strength to Procera ceramic
    Hummel, M
    Wegner, SM
    Kern, M
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A35 - A35
  • [27] Effects of Hydrofluoric Acid Concentrations, Commercial Brands, and Adhesive Application on the Bond Strength of a Resin Luting Agent to Lithium Disilicate Glass Ceramic
    dos Santos, D. R. C.
    Pacheco, R. R.
    Komegae, G. H.
    da Silva, J. A.
    Lima, D. A. N. L.
    Pini, N. I. P.
    Sundfeld, D.
    OPERATIVE DENTISTRY, 2023, 48 (06) : 700 - 710
  • [28] Recycling CAD/CAM Lithium Disilicate Ceramic: Effect of Surface Treatment and Aging on the Bond Strength to Resin Cement
    de Miranda, Larissa Mendonca
    Caldas, Aparecida TharIla Leite
    Moura, Dayanne Monielle Duarte
    Souza, Karina Barbosa
    de Assuncao, Isauremi Vieira
    Ozcan, Mutlu
    de Assuncao e Souza, Rodrigo Othavio
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2024, 37 (06) : 675 - 685
  • [29] Different Etching Times of a One-step Ceramic Primer: Effect on the Resin Bond Strength Durability to a CAD/CAM Lithium-Disilicate Glass-Ceramic
    Dapieve, Kiara Serafini
    Aragonez, Gabriela Carrao
    Prochnow, Catina
    de Lima Burgo, Thiago Augusto
    Rippe, Marilia Pivetta
    Rocha Pereira, Gabriel Kalil
    Venturini, Andressa Borin
    Valandro, Luiz Felipe
    JOURNAL OF ADHESIVE DENTISTRY, 2021, 23 (02): : 133 - 143
  • [30] Resin cement coating reverts the machining damage on the flexural fatigue strength of lithium disilicate glass-ceramic
    May, Michele Mirian
    Machry, Renan Vaz
    Fraga, Sara
    de Andrade, Guilherme Schmitt
    Bottino, Marco Antonio
    Valandro, Luiz Felipe
    May, Liliana Gressler
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2023, 111 (04) : 971 - 980