CHARACTERIZATION OF ELECTRON BEAM WELDED 17-4 PH STAINLESS STEEL

被引:0
|
作者
Wanjara, P. [1 ]
Jahazi, M. [1 ]
机构
[1] Natl Res Council Canada, Inst Aerosp Res, Aerosp Mfg Technol Ctr, Montreal, PQ, Canada
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The Canadian Department of National Defence (DND) currently has a requirement for a fully automated captive trajectory system (CTS) with six degrees of freedom, all of which are to be motorized, to study the movement of stores (such as missiles) during carriage/release testing of F-18 and other military aircraft in the National Research Council (NRC) trisonic blowdown wind tunnel. In the CTS, one of the joints providing linear motion is designed and fabricated with a linkage (telescoping inner strut (TIS)) in two halves, split along its neutral plane, to allow machining of the internal geometry. To support the dynamic, kinematic and aerodynamic loads induced, the two halves must be welded together while maintaining high tolerances on the inner geometry. The designed weld areas on the neutral plane require a penetration of 17.1 mm from each face in 17-4 precipitation hardening (PH) martensitic stainless steel (SS). Using conventional joining techniques, such as tungsten inert gas TIG welding, the fabrication of a thick section requires a V groove joint design and multiple passes to achieve the required penetration. However, exposure to a substantial heat input through this process renders large weld and heat affected zones on either face of the strut as well as distortion of the component, which poses considerable difficulties for assembly and motion. The application of a high energy density technique, namely electron beam (EB) welding, was utilized to penetrate the thick section with a single pass, while minimizing the weld region, heat affected zone (HAZ) and distortion of the strut (low heat input).
引用
收藏
页码:413 / 435
页数:23
相关论文
共 50 条
  • [1] APPLICATION OF SHEAR PUNCH TESTING TO STUDY MICROSTRUCTURE-PROPERTY RELATIONSHIPS IN ELECTRON BEAM WELDED 17-4 PH STAINLESS STEEL
    Wanjara, P.
    Jahazi, M.
    CANADIAN METALLURGICAL QUARTERLY, 2009, 48 (03) : 317 - 326
  • [2] Aging reactions in a 17-4 PH stainless steel
    Hsiao, CN
    Chiou, CS
    Yang, JR
    MATERIALS CHEMISTRY AND PHYSICS, 2002, 74 (02) : 134 - 142
  • [3] Aging kinetics of 17-4 PH stainless steel
    Mirzadeh, H.
    Najafizadeh, A.
    MATERIALS CHEMISTRY AND PHYSICS, 2009, 116 (01) : 119 - 124
  • [4] Hydrogen susceptibility of 17-4 PH stainless steel
    Chiang, WC
    Pu, CC
    Yu, BL
    Wu, JK
    MATERIALS LETTERS, 2003, 57 (16-17) : 2485 - 2488
  • [5] Characterization of simultaneous aged and plasma nitrided 17-4 PH stainless steel
    Riazi, Hamidreza
    Ashrafizadeh, Fakhreddin
    Hosseini, Sayed Rahman
    Ghomashchi, Reza
    Liu, Rong
    MATERIALS CHARACTERIZATION, 2017, 133 : 33 - 43
  • [6] KINETICS OF PRECIPITATION IN 17-4 PH STAINLESS-STEEL
    VISWANATHAN, UK
    NAYAR, PKK
    KRISHNAN, R
    MATERIALS SCIENCE AND TECHNOLOGY, 1989, 5 (04) : 346 - 349
  • [7] Effect of Post-Weld Heat Treatment on Microstructure and Hardness of Laser Beam Welded 17-4 PH Stainless Steel
    Tuz, Lechoslaw
    Sokolowski, Lukasz
    Stano, Sebastian
    MATERIALS, 2023, 16 (04)
  • [8] ON THE HOMOGENIZATION OF COBALT MODIFIED 17-4 PH STAINLESS STEEL
    Murthy, Arpana S.
    Lekakh, Simon
    Richards, Von L.
    Van Aken, David
    EPD CONGRESS 2011, 2011, : 651 - 658
  • [9] The rate of dynamic recrystallization in 17-4 PH stainless steel
    Mirzadeh, H.
    Najafizadeh, A.
    MATERIALS & DESIGN, 2010, 31 (10): : 4577 - 4583
  • [10] Activated gas nitriding of 17-4 PH stainless steel
    Kochmanski, P.
    Nowacki, J.
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (22-23): : 6558 - 6562