Impact of homogenization heat treatment on the high temperature deformation behavior of cast AZ31B magnesium alloy

被引:16
|
作者
Wong, Tsz Wun [1 ]
Hadadzadeh, Amir [1 ]
Benoit, Michael J. [1 ]
Wells, Mary A. [1 ]
机构
[1] Univ Waterloo, 200 Univ Ave West, Waterloo, ON N2L 3G1, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Deformation; Magnesium; Cast; Homogenization; AZ31B; Hot compression; Dynamic recrystallization;
D O I
10.1016/j.jmatprotec.2017.11.039
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Uniaxial isothermal compression tests were conducted on cylindrical specimens extracted from a DC cast AZ31B ingot with and without a homogenization treatment in the temperature range of 300 degrees C-500 degrees C, at strain rates of 10(-3) s(-1)-1.0 s-(1). As-cast specimens (without a homogenization treatment) exhibited cracking at a strain rate of 1.0 s(-1) for deformation temperatures of 400 degrees C and above. The cracking is believed to be associated with incipient melting of the gamma-Mg17Al12 phase. Homogenization of the specimens at 450 degrees C for 5 h improved the hot workability and no cracking was observed under the investigated conditions. Deformation of the cast-homogenized material was successfully conducted at 500 degrees C and 1.0 s(-1), to a final strain of 1.0. The volume fraction of dynamically recrystallized (DRX) grains was observed to increase with strain, but the DRX grain size exhibited little to no change. The DRX grain size however did increase with deformation temperature and with decreasing strain rate. Increasing the deformation temperature from 350 degrees C to 500 degrees C increased the maximum allowable strain before cracks were observed at the surface. Additional specimens were homogenized at temperatures of 400 degrees C or 500 degrees C, for times of 3 h or 5 h, followed by a water quench or air cooling. Under all circumstances, incipient melting of the gamma-Mg17Al12 phase was no longer observed upon heating using differential scanning calorimetry (DSC). Furthermore, homogenization at a temperature of 350 degrees C for up to 8 h resulted in partial dissolution of the gamma-Mg17Al12 phase, and an increase in incipient melting onset temperature was observed by DSC.
引用
收藏
页码:238 / 247
页数:10
相关论文
共 50 条
  • [21] Shear-Coupled Multiaxial Deformation Behavior of Rolled AZ31B Magnesium Alloy
    Zhu, Xianyun
    Carneiro, Luiz
    Wang, Huamiao
    Wu, Yunxin
    Wu, Peidong
    Jiang, Yanyao
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2024, 55 (08): : 2790 - 2810
  • [22] Asymmetry in the hot deformation behavior of AZ31B magnesium sheets
    Liu, Kai
    Dong, Xianghuai
    Xie, Huanyang
    Wu, Yunjian
    Peng, Fang
    Chen, Fei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 659 : 198 - 206
  • [23] Effects of melt temperature on as-cast structure and mechanical properties of AZ31B magnesium alloy
    Chen, Shu-ying
    Chang, Guo-wei
    Huang, Yu-duo
    Liu, Sheng-yang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2013, 23 (06) : 1602 - 1609
  • [24] Research on formability of AZ31B magnesium alloy at room temperature
    Yu, Zujian
    Li, Jianhui
    Yang, Yan
    ADVANCED RESEARCH ON MATERIAL SCIENCE, ENVIROMENT SCIENCE AND COMPUTER SCIENCE III, 2014, 886 : 3 - 6
  • [25] Warm Deformation Behavior and Flow Stress Modeling of AZ31B Magnesium Alloy under Tensile Deformation
    Murugesan, Mohanraj
    Yu, Jae-Hyeong
    Chung, Wanjin
    Lee, Chang-Whan
    MATERIALS, 2023, 16 (14)
  • [26] EFFECT OF ROLLING TEMPERATURE ON THE AZ31B MAGNESIUM ALLOY MICROSTRUCTURE
    Choquechambi Catorceno, Litzy L.
    Padillha, Angelo F.
    MAGNESIUM TECHNOLOGY 2012, 2012, : 283 - 287
  • [27] Superplastic Behavior and Constitutive Equation of AZ31B Magnesium Alloy
    Chen, Fuxiao
    Chen, Xiangzhen
    Sun, Futao
    MATERIALS AND COMPUTATIONAL MECHANICS, PTS 1-3, 2012, 117-119 : 1689 - +
  • [28] Study of the Microstructure of AZ31B Magnesium Alloy Under High Strain Rate Deformation
    Mao Pingli
    Liu Zheng
    Wang Changyi
    Wang Zhi
    ADVANCED STRUCTURAL MATERIALS, 2011, 686 : 325 - 331
  • [29] Flow stress and softening behavior of wrought magnesium alloy AZ31B at elevated temperature
    Wang, L.-Y. (cqulywang@yahoo.com.cn), 1600, Allerton Press Inc. (13):
  • [30] Flow stress and softening behavior of wrought magnesium alloy AZ31B at elevated temperature
    汪凌云
    范永革
    黄光杰
    黄光胜
    Transactions of Nonferrous Metals Society of China, 2003, (02) : 335 - 338