Fatigue and fracture toughness of Fe3Al alloys with additions of Zr and C

被引:0
|
作者
Karlik, M. [1 ]
Kubosova, A. [1 ]
Hausild, P. [1 ]
Prahl, J. [1 ]
机构
[1] Czech Tech Univ, Fac Nucl Sci & Phys Engn, Dept Mat, Prague 12000 2, Czech Republic
来源
KOVOVE MATERIALY-METALLIC MATERIALS | 2008年 / 46卷 / 02期
关键词
iron aluminides; Fe3Al; tensile test; fatigue crack growth; fracture toughness; fractographic analysis;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fracture behaviour of two intermetallic alloys based on Fe3Al with different Zr content was studied. On the alloy Fe-29.5Al-2.3Cr-0.63Zr-0.2C (at.%) (FA06Z), basic characterization of the microstructure by light and electron metallography was carried out. Tensile tests and fracture toughness tests were performed at 20, 200, 400, and 600 degrees C. The values of fracture toughness vary from 26 MPa m(1/2) (at 20 degrees C) to 42 MPa m(1/2) (at 400 degrees C). The fractographic analysis showed that the samples fractured at 20, 200 and 400 degrees C in the tensile or fracture toughness tests exhibit transgranular cleavage fracture, while the ductile dimple fracture predominates at 600 degrees C. Previous fatigue experiments on the alloy Fe-31.5Al-3.5Cr-0.25Zr-0.2C (at.%) (FA02Z) were completed by fatigue tests at 150 and 600 degrees C. The highest fatigue life and the lowest fatigue crack growth rates were found at 150 degrees C. The fatigue samples tested at all temperatures (20 to 600 degrees C) failed by transgranular cleavage fracture.
引用
收藏
页码:77 / 85
页数:9
相关论文
共 50 条
  • [41] Enhanced ductility in coarse grained Fe3Al alloys
    Huang, XX
    Yang, WY
    Sun, ZQ
    INTERMETALLICS, 2004, 12 (7-9) : 1019 - 1023
  • [42] VACANCY CONCENTRATION AND ORDERING KINETICS IN FE3AL ALLOYS
    HASAKA, M
    OKI, K
    EGUCHI, T
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1977, 18 (11): : 750 - 758
  • [43] HALL-KIKOIN EFFECT IN FE3AL ALLOYS
    PUZEI, IM
    ATAEV, A
    POGOSOV, VZ
    FIZIKA METALLOV I METALLOVEDENIE, 1975, 40 (04): : 871 - 874
  • [44] PLASTIC DEFORMATION OF ORDERED FECO + FE3AL ALLOYS
    STOLOFF, NS
    DAVIES, RG
    ACTA METALLURGICA, 1964, 12 (05): : 473 - &
  • [45] ORDER-DISORDER TRANSFORMATION IN FE3AL ALLOYS
    LESOILLE, MR
    GIELEN, PM
    PHYSICA STATUS SOLIDI, 1970, 37 (01): : 127 - &
  • [46] Wet abrasive wear of ordered Fe3Al alloys
    Tu, JP
    Liu, MS
    WEAR, 1997, 209 (1-2) : 31 - 36
  • [47] The Charpy impact behavior of Fe3Al and Fe3Al-20at%Mn alloys
    Liu, JN
    Yan, W
    Ma, JL
    Wu, KH
    HIGH-TEMPERATURE ORDERED INTERMETALLIC ALLOYS VII, 1997, 460 : 343 - 348
  • [48] The Role of Zr in the High-temperature Oxidation of Fe3Al
    Przybylski, K.
    Chevalier, S.
    Juzon, P.
    Galerie, A.
    Borchardt, G.
    Heintz, O.
    Larpin, J. P.
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 7, PTS 1 AND 2, 2008, 595-598 : 1103 - 1110
  • [49] The effect of Zr on the oxidation properties of Fe3Al intermetallic compound
    Przybylski, Kazimierz
    OCHRONA PRZED KOROZJA, 2009, 52 (11): : 576 - 576
  • [50] The Effect of Niobium and Carbon on the Oxidation Resistance of Alloys Based on Fe3Al at 900°C
    Hotar, A.
    Hotar, V
    Svec, M.
    Danis, S.
    OXIDATION OF METALS, 2022, 98 (1-2): : 77 - 107