A Comparative Study of Cyclic Oxidation and Sulfates-Induced Hot Corrosion Behavior of Arc-Sprayed Ni-Cr-Ti Coatings at Moderate Temperatures

被引:14
|
作者
Guo, Wenmin [1 ]
Wu, Yuping [1 ]
Zhang, Jianfeng [1 ]
Hong, Sheng [1 ]
Chen, Liyan [1 ]
Qin, Yujiao [1 ]
机构
[1] Hohai Univ, Coll Mech & Mat, Nanjing 210098, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
arc spray; coating; hot corrosion; oxidation; NA2SO4; DEPOSITS; ALLOYS; PERFORMANCE; SUPERALLOY; BOILER; RESISTANCE; MECHANISM; 900-DEGREES-C; OPTIMIZATION; METALS;
D O I
10.1007/s11666-015-0222-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The cyclic oxidation and sulfates-induced hot corrosion behaviors of a Ni-43Cr-0.3Ti arc-sprayed coating at 550-750 A degrees C were characterized and compared in this study. In general, all the oxidation and hot corrosion kinetic curves of the coating followed a parabolic law, i.e., the weight of the specimens showed a rapid growth initially and then reached the gradual state. However, the initial stage of the hot corrosion process was approximately two times longer than that of the oxidation process, indicating a longer preparation time required for the formation of a protective scale in the former process. At 650 A degrees C, the parabolic rate constant for the hot corrosion was 7.2 x 10(-12) g(2)/(cm(4)center dot s), approximately 1.7 times higher than that for the oxidation at the same temperature. The lower parabolic rate constant for the oxidation was mainly attributed to the formation of a protective oxide scale on the surface of corroded specimens, which was composed of a mixture of NiO, Cr2O3, and NiCr2O4. However, as the liquid molten salts emerged during the hot corrosion, these protective oxides would be dissolved and the coating was corrupted acceleratedly.
引用
收藏
页码:789 / 797
页数:9
相关论文
共 14 条
  • [11] Isothermal oxidation and hot corrosion behavior of HVOF sprayed 80Ni-20Cr coatings at 750?C
    Binal, Gulfem
    SURFACE & COATINGS TECHNOLOGY, 2023, 454
  • [12] Oxidation behavior of arc-sprayed FeMnCrAl/Cr3C2-Ni9Al coatings deposited on low-carbon steel substrates
    Luo, Laima
    Liu, Shaoguang
    Li, Jian
    Yucheng, Wu
    SURFACE & COATINGS TECHNOLOGY, 2011, 205 (11): : 3411 - 3415
  • [13] Effect of CeO2 on Cyclic Hot-Corrosion Behavior of Detonation-Gun Sprayed Cr3C2-NiCr Coatings on Ni-Based Superalloy
    Saladi, Sekar
    Menghani, Jyoti
    Prakash, Satya
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (03) : 1379 - 1389
  • [14] Effect of CeO2 on Cyclic Hot-Corrosion Behavior of Detonation-Gun Sprayed Cr3C2-NiCr Coatings on Ni-Based Superalloy
    Sekar Saladi
    Jyoti Menghani
    Satya Prakash
    Journal of Materials Engineering and Performance, 2015, 24 : 1379 - 1389