Atmospheric pitting corrosion of 304L stainless steel: the role of highly concentrated chloride solutions

被引:39
|
作者
Street, Steven R. [1 ]
Mi, Na [1 ]
Cook, Angus J. M. C. [1 ]
Mohammed-Ali, Haval B. [1 ]
Guo, Liya [1 ]
Rayment, Trevor [2 ]
Davenport, Alison J. [1 ]
机构
[1] Univ Birmingham, Sch Met & Mat, Birmingham B15 2TT, W Midlands, England
[2] Diamond Light Source, Oxford OX11 0DE, England
基金
英国工程与自然科学研究理事会;
关键词
SALT AEROSOL PROXIES; IN-SITU; RELATIVE-HUMIDITY; PIT PROPAGATION; INITIAL-STAGE; DROPLETS; FILM; 304-STAINLESS-STEEL; ENVIRONMENTS; MECHANISM;
D O I
10.1039/c4fd00246f
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The morphology of atmospheric pitting corrosion in 304L stainless steel plate was analysed using MgCl2 droplets in relation to changes in relative humidity (RH) and chloride deposition density (CDD). It was found that highly reproducible morphologies occur that are distinct at different RH. Pitting at higher concentrations, i.e. lower RH, resulted in satellite pits forming around the perimeter of wide shallow dish regions. At higher RH, these satellite pits did not form and instead spiral attack into the shallow region was observed. Increasing CDD at saturation resulted in a very broad-mouthed pitting attack within the shallow dish region. Large data sets were used to find trends in pit size and morphology in what is essentially a heterogeneous alloy. Electrochemical experiments on 304 stainless steel wires in highly saturated solutions showed that the passive current density increased significantly above 3 M MgCl2 and the breakdown pitting potential dropped as the concentration increased. It is proposed that the shallow dish regions grow via enhanced dissolution of the passive film, whereas satellite pits and a spiral attack take place with active dissolution of bare metal surfaces.
引用
收藏
页码:251 / 265
页数:15
相关论文
共 50 条
  • [31] Influence of flow conditions on the corrosion of AISI 304L stainless steel
    Wharton, JA
    Wood, RJK
    WEAR, 2004, 256 (05) : 525 - 536
  • [32] Effect of texture on corrosion behavior of AISI 304L stainless steel
    Kumar, BR
    Singh, R
    Mahato, B
    De, PK
    Bandyopadhyay, NR
    Bhattacharya, DK
    MATERIALS CHARACTERIZATION, 2005, 54 (02) : 141 - 147
  • [33] An active corrosion mechanism for metal dusting on 304L stainless steel
    Szakalos, P
    Pettersson, R
    Hertzman, S
    CORROSION SCIENCE, 2002, 44 (10) : 2253 - 2270
  • [34] Effect of Laser Peening on the Corrosion Properties of 304L Stainless Steel
    Yoo, Young-Ran
    Choi, Seung-Heon
    Kim, Young-Sik
    MATERIALS, 2023, 16 (02)
  • [35] The effect of cysteine on the corrosion of 304L stainless steel in sulphuric acid
    Silva, A. B.
    Agostinho, S. M. L.
    Barcia, O. E.
    Cordeiro, G. G. O.
    D'Elia, E.
    CORROSION SCIENCE, 2006, 48 (11) : 3668 - 3674
  • [36] The Corrosion Susceptibility of 304L Stainless Steel Exposed to Crevice Environments
    Tsai, Kun-Chao
    Yeh, Chun-Ping
    MATERIALS, 2022, 15 (09)
  • [37] FINITE ELEMENT MODELLING OF TRANSGRANULAR CHLORIDE STRESS CORROSION CRACKING IN 304L AUSTENITIC STAINLESS STEEL
    Wenman, Mark
    Barton, James
    Trethewey, Kenneth
    Jarman, Sean
    Chard-Tuckey, Paul
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2008, VOL 6, PT A AND B, 2009, : 975 - 985
  • [38] Stress corrosion cracking of laser alloyed 304L stainless steel with Ru in hot chloride solution
    Tshilwane, N. N.
    van der Merwe, J. W.
    SURFACE & COATINGS TECHNOLOGY, 2018, 347 : 414 - 419
  • [39] The effect of salt loading on chloride-induced stress corrosion cracking of 304L austenitic stainless steel under atmospheric conditions
    Scatigno, G. G.
    Dong, P.
    Ryan, M. P.
    Wenman, M. R.
    MATERIALIA, 2019, 8
  • [40] Investigation on pitting corrosion behavior of ultrafine-grained 304L stainless steel in Cl- containing solution
    Piao, Nan
    Chen, Ji
    Yin, Chengjiang
    Sun, Cheng
    Zhang, Xinghang
    Wu, Zhanwen
    Jinshu Xuebao/Acta Metallurgica Sinica, 2015, 51 (09): : 1077 - 1084