nanocrystalline diamond;
nanostructured carbon;
inductively coupled plasma;
electron energy loss spectroscopy;
sp(2)/sp(3) bonding;
D O I:
暂无
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
A 13.56 MHz low pressure inductively coupled CH4/CO/H-2 plasma has been applied to prepare nanocrystalline diamond particles of 200-700 nm diameter. The minimum diameter of the particles was found to be 5 nm. Two-dimensional platelet-like graphite and carbon nanotubes also were deposited with different conditions. The characterizations were performed with transmission electron microscopy (TEM) and electron energy loss spectroscopy (EELS). The TEM observations have revealed that the two-dimensional platelet-like deposits consist of disordered microcrystalline graphite, whereas the particles are composed of only diamond nanocrystallites. The high-resolution TEM images clearly show that each particle is composed of small particles of about several ten nm in diameter. The mapping of sp(2) bonding by the pi* image reveals that sp(2)-bonded carbons are localized in the grain boundaries of 20-50 nm sub-grains of nanocrystalline diamond particles at approximately 1 nm width.
机构:
Natl Nucl Secur Adm Kansas City Plant, Kansas City, MO USA
Univ Calif Los Angeles, Dept Chem & Biomol Engn, Los Angeles, CA USANatl Nucl Secur Adm Kansas City Plant, Kansas City, MO USA
Ladwig, Angela M.
Koch, Ronald D.
论文数: 0引用数: 0
h-index: 0
机构:
Natl Nucl Secur Adm Kansas City Plant, Kansas City, MO USANatl Nucl Secur Adm Kansas City Plant, Kansas City, MO USA
Koch, Ronald D.
Wenski, Edward G.
论文数: 0引用数: 0
h-index: 0
机构:
Natl Nucl Secur Adm Kansas City Plant, Kansas City, MO USANatl Nucl Secur Adm Kansas City Plant, Kansas City, MO USA
Wenski, Edward G.
Hicks, Robert F.
论文数: 0引用数: 0
h-index: 0
机构:
Univ Calif Los Angeles, Dept Chem & Biomol Engn, Los Angeles, CA USANatl Nucl Secur Adm Kansas City Plant, Kansas City, MO USA