Corrosion Behaviour of 316L Stainless Steel in Hot Dilute Sulphuric Acid Solution with Sulphate and NaCl

被引:8
|
作者
Zhang, Jian [1 ]
Ju, Pengfei [2 ]
Wang, Chaoli [1 ]
Dun, Yuchao [1 ]
Zhao, Xuhui [1 ]
Zuo, Yu [1 ]
Tang, Yuming [1 ]
机构
[1] Beijing Univ Chem Technol, Key Lab Electrochem Proc & Technol Mat, Beijing 100029, Peoples R China
[2] Shanghai Aerosp Equipment Manufacture Co Ltd, Shanghai 200245, Peoples R China
基金
中国国家自然科学基金;
关键词
316L SS; hot dilute sulphuric acid; corrosion; sodium chloride; sodium sulphate; corrosion products; PITTING CORROSION; SINGLE PIT; CHLORIDE; TEMPERATURE; INITIATION; GROWTH; IONS; DISSOLUTION; CHROMIUM; AISI-304;
D O I
10.1134/S207020511901026X
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The corrosion behaviour of 316L stainless steel (316L SS) in 10% H2SO4 solution (94 degrees C) with various concentrations of NaCl (0-0.085 mol/L) was studied by immersion corrosion test and polarization methods, combined with SEM/EDS, XPS and XRD tests. The influence of NaCl on the corrosion of 316L SS was investigated. The results showed that at lower NaCl contents (0-0.0085 mol/L), the steel presented a general corrosion characteristic with a higher corrosion speed and the corrosion rate increased with the NaCl content. At higher NaCl contents (0.017 mol/L), the corrosion rate decreased remarkably due to the protective corrosion products precipitation which contained metallic sulphates and NaHSO4. However, the higher concentration of chloride ions caused micron pitting-like local dissolution on the surface. The addition of Na2SO4 effectively inhibited general corrosion of the steel because of a dense and continuous products layer enriched with more NaHSO4 and metallic sulphates formed.
引用
收藏
页码:148 / 156
页数:9
相关论文
共 50 条
  • [1] Corrosion Behaviour of 316L Stainless Steel in Hot Dilute Sulphuric Acid Solution with Sulphate and NaCl
    Pengfei Jian Zhang
    Chaoli Ju
    Yuchao Wang
    Xuhui Dun
    Yu Zhao
    Yuming Zuo
    Protection of Metals and Physical Chemistry of Surfaces, 2019, 55 : 148 - 156
  • [2] Investigation in the corrosion behaviour of bulk nanocrystalline 316L austenitic stainless steel in NaCl solution
    Eskandari, M.
    Yeganeh, M.
    Motamedi, M.
    MICRO & NANO LETTERS, 2012, 7 (04) : 380 - 383
  • [3] Corrosion Behaviour of 316L Stainless Steel in Boric Acid Solutions
    Zhang, Shenghan
    Lu, Quan
    Xu, Yunfei
    He, Kuan
    Bang, Kexin
    Tan, Yu
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2018, 13 (04): : 3246 - 3256
  • [4] Corrosion and electrochemical behaviour of 316L stainless steel in acetic acid solutions
    Turnbull, A
    Ryan, M
    Willetts, A
    Zhou, SQ
    CORROSION SCIENCE, 2003, 45 (05) : 1051 - 1072
  • [5] Corrosion Behaviour of Type 316L Stainless Steel in Hot Caustic Aqueous Environments
    Raul Davalos Monteiro
    Jan van de Wetering
    Benjamin Krawczyk
    Dirk L. Engelberg
    Metals and Materials International, 2020, 26 : 630 - 640
  • [6] Corrosion Behaviour of Type 316L Stainless Steel in Hot Caustic Aqueous Environments
    Monteiro, Raul Davalos
    van de Wetering, Jan
    Krawczyk, Benjamin
    Engelberg, Dirk L.
    METALS AND MATERIALS INTERNATIONAL, 2020, 26 (05) : 630 - 640
  • [7] CORROSION-FATIGUE OF 316L STAINLESS-STEEL IN HOT LIOH SOLUTION
    ZHENG, JH
    DUQUETTE, DJ
    BOGAERTS, WF
    CORROSION, 1993, 49 (05) : 372 - 376
  • [8] Corrosion behaviour of 316L stainless steel in PTA slurry
    Ju, P. F.
    Zuo, Y.
    Tang, J. L.
    Tang, Y. M.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2013, 48 (03) : 207 - 210
  • [9] FRETTING CORROSION BEHAVIOR OF 316L STAINLESS STEEL HEAT EXCHANGER TUBE IN NACL SOLUTION
    Ma, Xu
    Zhang, Shengzan
    Tan, Wei
    Zhu, Guorui
    PROCEEDINGS OF ASME 2022 PRESSURE VESSELS AND PIPING CONFERENCE, PVP2022, VOL 4B, 2022,
  • [10] Electrochemical and corrosion behaviour of stainless steels 316L and 317L in chloridised ammonium sulphate solution
    Ghahremaninezhad, A.
    Wang, W.
    Asselin, E.
    Budac, J.
    Alfantazi, A.
    CANADIAN METALLURGICAL QUARTERLY, 2012, 51 (04) : 471 - 484