Enhanced temperature stability and quality factor with Hf substitution for Sn and MnO2 doping of (Ba0.97Ca0.03)(Ti0.96Sn0.04)O3 lead-free piezoelectric ceramics with high Curie temperature

被引:11
|
作者
Tsai, Cheng-Che [1 ]
Chao, Wei-Hsiang [2 ]
Chu, Sheng-Yuan [2 ,3 ]
Hong, Cheng-Shong [4 ]
Weng, Chung-Ming [2 ]
Su, Hsiu-Hsien [2 ]
机构
[1] Tung Fang Design Inst, Dept Digital Game & Animat Design, Kaohsiung 829, Taiwan
[2] Natl Cheng Kung Univ, Dept Elect Engn, Tainan 701, Taiwan
[3] Natl Cheng Kung Univ, Ctr Micro Nano Sci & Technol, Tainan 701, Taiwan
[4] Natl Kaohsiung Normal Univ, Dept Elect Engn, Kaohsiung 802, Taiwan
来源
AIP ADVANCES | 2016年 / 6卷 / 12期
关键词
MORPHOTROPIC PHASE-BOUNDARY; ELECTRICAL-PROPERTIES;
D O I
10.1063/1.4972201
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, the process of two-stage modifications for (Ba0.97Ca0.03)(Ti0.96Sn0.04-xHfx)O-3 (BCTS4-100xH100x) ceramics was studied. The trade-off composition was obtained by Hf substitution for Sn and MnO2 doping (two-stage modification) which improves the temperature stability and piezoelectric properties. The phase structure ratio, microstructure, and dielectric, piezoelectric, ferroelectric, and temperature stability properties were systematically investigated. Results showed that BCTS4-100xH100x piezoelectric ceramics with x =0.035 had a relatively high Curie temperature (T-C) of about 112 degrees C, a piezoelectric charge constant (d(33)) of 313 pC/N, an electromechanical coupling factor (k(p)) of 0.49, a mechanical quality factor (Q(m)) of 122, and a remnant polarization (P-r) of 19 mu C/cm(2). In addition, the temperature stability of the resonant frequency (f(r)), k(p), and aging d(33) could be tuned via Hf content. Good piezoelectric temperature stability (up to 110 degrees C) was found with x =0.035. BCTS0.5H3.5 + a mol% Mn (BCTSH + a Mn) piezoelectric ceramics with a = 2 had a high TC of about 123 degrees C, k(p) similar to 0.39, d(33) similar to 230 pC/N, Q(m) similar to 341, and high temperature stability due to the produced oxygen vacancies. This mechanism can be depicted using the complex impedance analysis associated with a valence compensation model on electric properties. Two-stage modification for lead-free (Ba0.97Ca0.03)(Ti0.96Sn0.04)O-3 ceramics suitably adjusts the compositions for applications in piezoelectric motors and actuators. (C) 2016 Author(s). All article content, except where otherwise noted, is licensed under a Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Temperature Stability in Dy-Doped (Ba0.99Ca0.01)(Ti0.98Zr0.02)O3 Lead-Free Ceramics with High Piezoelectric Coefficient
    Li, Wei
    Xu, Zhijun
    Chu, Ruiqing
    Fu, Peng
    Zang, Guozhong
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2011, 94 (10) : 3181 - 3183
  • [42] Enhanced electrical properties of lead-free (Ba1−xCax)(Ti0.94Zr0.01Sn0.05)O3 piezoelectric ceramics by optimizing phase ratio and sintering temperature
    Ning Wang
    Yucheng Tang
    Wenyuan Pan
    Boping Zhang
    Journal of Materials Science: Materials in Electronics, 2020, 31 : 21682 - 21692
  • [43] Enhanced electrical properties of lead-free (Ba1-xCax)(Ti0.94Zr0.01Sn0.05)O3 piezoelectric ceramics by optimizing phase ratio and sintering temperature
    Wang, Ning
    Tang, Yucheng
    Pan, Wenyuan
    Zhang, Boping
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (23) : 21682 - 21692
  • [44] Piezoelectric properties of [Li0.03(K0.48Na0.52)0.97](Nb0.97Sb0.03)O3-(Ba0.85Ca0.15)(Ti0.90Zr0.10)O3 lead-free piezoelectric ceramics
    Chen, Xiaoyu
    Wu, Jiagang
    Cheng, Xiaojing
    Wu, Bo
    Wu, Wenjuan
    Xiao, Dingquan
    Zhu, Jianguo
    CURRENT APPLIED PHYSICS, 2012, 12 (03) : 752 - 754
  • [45] High piezoelectric coefficient and temperature stability of Ga2O3-doped (Ba0.99Ca0.01)(Zr0.02Ti0.98)O3 lead-free ceramics by low-temperature sintering
    Ma, Jiafeng
    Liu, Xinyu
    Li, Wenhua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 581 : 642 - 645
  • [46] Low temperature sintering of (Ba0.85Ca0.15) (Ti0.90Zr0.10)O3 lead-free piezoceramic with the additive of MnO2
    Mekonnen, Mulualem Abebe
    Tadesse, Mesfin Zewdu
    JOURNAL OF ELECTROCERAMICS, 2021, 46 (03) : 115 - 123
  • [47] Low temperature sintering of (Ba0.85Ca0.15) (Ti0.90Zr0.10)O3 lead-free piezoceramic with the additive of MnO2
    Mulualem Abebe Mekonnen
    Mesfin Zewdu Tadesse
    Journal of Electroceramics, 2021, 46 : 115 - 123
  • [48] Enhanced piezoelectric properties of (Ba0.85Ca0.15)(Ti0.9Zr0.1)O3 lead-free ceramics by optimizing calcination and sintering temperature
    Wang, Pan
    Li, Yongxiang
    Lu, Yiqing
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (11) : 2005 - 2012
  • [49] Enhanced electrocaloric strengths at room temperature in (SrxBa1-x) (Sn0.05Ti0.95)O3 lead-free ceramics
    Lu, Sheng-Guo
    Lin, Xiongwei
    Li, Jiang
    Li, Dandan
    Yao, Yingbang
    Tao, Tao
    Liang, Bo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 871
  • [50] High piezoelectric d33 coefficient in (Ba1-xCax)(Ti0.98Zr0.02)O3 lead-free ceramics with relative high Curie temperature
    Li, Wei
    Xu, Zhijun
    Chu, Ruiqing
    Fu, Peng
    Zang, Guozhong
    MATERIALS LETTERS, 2010, 64 (21) : 2325 - 2327