Biomorphic SiC: porous SiC and ultrafine SiC powder formation through biomimicking route

被引:4
|
作者
Abdul Karim, Gulnar [1 ]
Ghosh, Abhijit [1 ]
Rao, Rekha [2 ]
Krishnan, Madangopal [1 ]
机构
[1] Bhabha Atom Res Ctr, Glass & Adv Mat Div, Mumbai 400085, Maharashtra, India
[2] BARC, Solid State Phys Div, Mumbai, Maharashtra, India
关键词
Silicon carbide; biomorphic; particle size; milling; CERAMICS;
D O I
10.1080/17436753.2020.1842106
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Natural wood is a ready-to-use template for making porous silicon carbide (SiC) body. Biomorphic beta-SiC was synthesised from wood of a mango (Mangifera Indica) tree. Carbon template was made by carbonising this wood at 1000 degrees C in argon gas atmosphere. Thus formed template was repeatedly infiltrated with a mixture of tetraethyl-orthosilicate (TEOS) (in alcohol) and oxalic acid solution (aqueous). Heat treatment at 1600 degrees C for 1 h in vacuum converted the infiltrated template to beta-SiC with a complex hierarchical cellular structure- a mimic of the plant structure. To produce phase pure SiC, unreacted carbon (C) and silica (SiO2) (if any) were removed by burning in air followed by treating with hydrofluoric acid. Mono dispersed SiC powder having particle size of similar to 225 nm has been obtained by crushing, grinding and milling of thus formed biomorphic SiC body. A grinding limit is reported for the first time in SiC system.
引用
收藏
页码:24 / 31
页数:8
相关论文
共 50 条
  • [21] Biomorphic SiC from lotus root
    Wang, Qing
    Wang, Donghua
    Jin, Guoqiang
    Wang, Yingyong
    Guo, Xiangyun
    PARTICUOLOGY, 2009, 7 (03) : 199 - 203
  • [22] Biomorphic SiC from peas and beans
    Kiselov, V. S.
    Yukhymchyk, V. A.
    Poludin, V. I.
    Tryus, M. P.
    Belyaev, A. E.
    SEMICONDUCTOR PHYSICS QUANTUM ELECTRONICS & OPTOELECTRONICS, 2012, 15 (04) : 305 - 309
  • [23] Biomorphic Hierarchical Porous SIC Prepared from Carbonized Broomcorn Millet
    Wang Qing
    Zhang Yahui
    Guo Yuwei
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 : 662 - 664
  • [24] Erosion and strength degradation of biomorphic SiC
    de Arellano-López, AR
    Martínez-Fernández, J
    Varela-Feria, FM
    Orlova, TS
    Goretta, KC
    Gutierrez-Mora, F
    Chen, N
    Routbort, JL
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (05) : 861 - 870
  • [25] Thermal conductivity of porous biomorphic SiC derived from wood precursors
    Gomez-Martin, A.
    Orihuela, M. P.
    Ramirez-Rico, J.
    Chacartegui, R.
    Martinez-Fernandez, J.
    CERAMICS INTERNATIONAL, 2016, 42 (14) : 16220 - 16229
  • [26] Preparation and characterization of porous, biomorphic SiC ceramic with hybrid pore structure
    Qian, JM
    Jin, ZH
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2006, 26 (08) : 1311 - 1316
  • [27] Microstructure and fracture properties of biomorphic SiC
    Presas, M
    Pastor, JY
    Llorca, J
    López, ARA
    Fernández, JM
    Sepúlveda, R
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2006, 24 (1-2): : 49 - 54
  • [28] SiC/SiC composites through transient eutectic-phase route for fusion applications
    Katoh, Y
    Kohyama, A
    Nozawa, T
    Sato, M
    JOURNAL OF NUCLEAR MATERIALS, 2004, 329 : 587 - 591
  • [29] PREPARATION AND HIGH-PRESSURE SINTERING OF ULTRAFINE SIC POWDER
    TAKAHASHI, S
    KATO, M
    HIRAYAMA, T
    UYEDA, R
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1988, 96 (05): : 603 - 607
  • [30] Electrical properties of bio-SiC and Si components of the SiC/Si biomorphic composite
    Orlova, T. S.
    Il'in, D. V.
    Smirnov, B. I.
    Smirnov, I. A.
    Sepulveda, R.
    Martinez-Fernandez, J.
    de Arellano-Lopez, A. R.
    PHYSICS OF THE SOLID STATE, 2007, 49 (02) : 205 - 210