Biomorphic SiC: porous SiC and ultrafine SiC powder formation through biomimicking route

被引:4
|
作者
Abdul Karim, Gulnar [1 ]
Ghosh, Abhijit [1 ]
Rao, Rekha [2 ]
Krishnan, Madangopal [1 ]
机构
[1] Bhabha Atom Res Ctr, Glass & Adv Mat Div, Mumbai 400085, Maharashtra, India
[2] BARC, Solid State Phys Div, Mumbai, Maharashtra, India
关键词
Silicon carbide; biomorphic; particle size; milling; CERAMICS;
D O I
10.1080/17436753.2020.1842106
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Natural wood is a ready-to-use template for making porous silicon carbide (SiC) body. Biomorphic beta-SiC was synthesised from wood of a mango (Mangifera Indica) tree. Carbon template was made by carbonising this wood at 1000 degrees C in argon gas atmosphere. Thus formed template was repeatedly infiltrated with a mixture of tetraethyl-orthosilicate (TEOS) (in alcohol) and oxalic acid solution (aqueous). Heat treatment at 1600 degrees C for 1 h in vacuum converted the infiltrated template to beta-SiC with a complex hierarchical cellular structure- a mimic of the plant structure. To produce phase pure SiC, unreacted carbon (C) and silica (SiO2) (if any) were removed by burning in air followed by treating with hydrofluoric acid. Mono dispersed SiC powder having particle size of similar to 225 nm has been obtained by crushing, grinding and milling of thus formed biomorphic SiC body. A grinding limit is reported for the first time in SiC system.
引用
收藏
页码:24 / 31
页数:8
相关论文
共 50 条
  • [1] Mechanical properties of porous biomorphic SiC
    Robledo, MJL
    Ferrer, RES
    León, AB
    Fernández, JM
    López, ARD
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2005, 44 (05): : 318 - 323
  • [2] Preparation of biomorphic SiC
    Istomina, E. I.
    Istomin, P. V.
    Nadutkin, A. V.
    INORGANIC MATERIALS, 2013, 49 (10) : 984 - 987
  • [3] Preparation of biomorphic SiC
    E. I. Istomina
    P. V. Istomin
    A. V. Nadutkin
    Inorganic Materials, 2013, 49 : 984 - 987
  • [4] Mechanical behavior of biomorphic Si/SiC porous composites
    Presas, M
    Pastor, JY
    Llorca, J
    de Arellano-López, AR
    Martínez-Fernández, J
    Sepúlveda, RE
    SCRIPTA MATERIALIA, 2005, 53 (10) : 1175 - 1180
  • [5] THERMAL CONDUCTIVITY OF BIOMORPHIC POROUS SIC BASED CERAMICS
    Popovska, Nadejda
    Alkhateeb, Emad
    Kugler, Tanja
    Froeba, Andreas P.
    Leipertz, Alfred
    PROCEEDINGS OF THE ASME INTERNATIONAL HEAT TRANSFER CONFERENCE - 2010 , VOL 3: COMBUSTION, CONDUCTION, ELECTRONIC COOLING, EVAPORATION,TWO-PHASE FLOW, 2010, : 313 - 316
  • [6] Sliding wear resistance of porous biomorphic sic ceramics
    Lopez-Robledo, M. J.
    Gomez-Martin, A.
    Ramirez-Rico, J.
    Martinez-Fernandez, J.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2016, 59 : 26 - 31
  • [7] Reaction–formation mechanisms and microstructure evolution of biomorphic SiC
    Francisco M. Varela-Feria
    Joaquín Ramírez-Rico
    Antonio R. de Arellano-López
    Julián Martínez-Fernández
    Mrityunjay Singh
    Journal of Materials Science, 2008, 43 : 933 - 941
  • [8] Synthesis of biomorphic SiC ceramics
    Institute of Nuclear Sciences Vinča, Materials Department, P. O. Box 522, 11001 Belgrade, Serbia
    J. Optoelectron. Adv. Mat., 2008, 12 (3447-3449):
  • [9] Indentation hardness of biomorphic SiC
    Gutierrez-Mora, F
    Goretta, KC
    Varela-Feria, FM
    López, ARA
    Fernández, JM
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2005, 23 (4-6): : 369 - 374
  • [10] Preparation of biomorphic SiC ceramics
    Egelja, A.
    Gulicovski, J.
    Devecerski, A.
    Ninic, M.
    Radosavljevic-Mihajlovic, A.
    Matovic, B.
    SCIENCE OF SINTERING, 2008, 40 (02) : 141 - 145