Influence of bulk pre-straining on the size effect in nickel compression pillars

被引:62
|
作者
Schneider, A. S. [1 ]
Kiener, D. [2 ]
Yakacki, C. M. [3 ]
Maier, H. J. [4 ]
Gruber, P. A. [5 ]
Tamura, N. [6 ]
Kunz, M. [6 ]
Minor, A. M. [7 ,8 ]
Frick, C. P. [9 ]
机构
[1] INM Leibniz Inst New Mat, D-66123 Saarbrucken, Germany
[2] Univ Leoben, Dept Mat Phys, A-8700 Leoben, Austria
[3] Univ Colorado, Dept Mech Engn, Denver, CO 80217 USA
[4] Univ Paderborn, Lehrstuhl Werkstoffkunde Mat Sci, D-33098 Paderborn, Germany
[5] Karlsruhe Inst Technol, Inst Appl Mat, D-76131 Karlsruhe, Germany
[6] Univ Calif Berkeley, Lawrence Berkeley Natl Lab, Adv Light Source, Berkeley, CA 94720 USA
[7] Univ Calif Berkeley, Dept Mat Sci & Engn, Berkeley, CA 94720 USA
[8] Univ Calif Berkeley, Lawrence Berkeley Natl Lab, Natl Ctr Electron Microscopy, Berkeley, CA 94720 USA
[9] Univ Wyoming, Dept Mech Engn, Laramie, WY 82071 USA
基金
奥地利科学基金会;
关键词
Nickel; Plasticity; Dislocations; Size effect; Micropillar compression; Electron microscopy; MECHANICAL-PROPERTIES; DISLOCATION NUCLEATION; YIELD STRENGTH; SMALL-SCALE; SINGLE; DEFORMATION; PLASTICITY; FCC; MICROPILLARS; CU;
D O I
10.1016/j.msea.2012.08.055
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Micro-compression tests were performed on pre-strained nickel (Ni) single crystals in order to investigate the influence of the initial dislocation arrangement on the size dependence of small-scale metal structures. A bulk Ni sample was grown using the Czochralski method and sectioned into four compression samples, which were then pre-strained to nominal strains of 5, 10, 15 and 20%. Bulk samples were then characterized using transmission electron microscopy (TEM), micro-Laue diffraction, and electron backscatter diffraction. TEM results show that a dislocation cell structure was present for all deformed samples, and Laue diffraction demonstrated that the internal strain increased with increased amount of pre-straining. Small-scale pillars with diameters from 200 nm to 5 pm were focused ion beam (FIB) machined from each of the four deformed bulk samples and further compressed via a nanoindenter equipped with a flat diamond punch. Results demonstrate that bulk pre-straining inhibits the sample size effect. For heavily pre-strained bulk samples, the deformation history does not affect the stress-strain behavior, as the pillars demonstrated elevated strength and rather low strain hardening over the whole investigated size range. In situ TEM and micro-Laue diffraction measurements of pillars confirmed little change in dislocation density during pillar compression. Thus, the dislocation cell walls created by heavy bulk pre-straining become the relevant internal material structure controlling the mechanical properties, dominating the sample size effect observed in the low dislocation density regime. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:147 / 158
页数:12
相关论文
共 50 条
  • [41] EFFECT OF TENSILE PRE-STRAINING ON NUCLEATION OF MARTENSITE IN AN FE-NI-C ALLOY - REPLY
    GUIMARAES, JRC
    SCRIPTA METALLURGICA, 1976, 10 (11): : 1051 - 1051
  • [42] Influence of uniaxial and biaxial pre-straining on the high cycle fatigue performance of DP590 steel
    Ghosal, Puja
    Paul, Surajit Kumar
    Raj, Abhishek
    International Journal of Fatigue, 2021, 151
  • [43] Influence of Pre-straining and Pre-ageing on the Age-hardening Response of Al-Mg-Si Alloys
    Yan, Yong
    Liang, Zeqin
    Banhart, John
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 903 - 908
  • [44] Deviations in yield and ultimate tensile strength estimation with the Small Punch Test: Numerical analysis of pre-straining and Bauschinger effect influence
    Calaf-Chica, Jose
    Palomar, Mario Sanchez
    Diez, Pedro Miguel Bravo
    Calzada, Monica Preciado
    MECHANICS OF MATERIALS, 2021, 153
  • [45] Effect of pre-straining and pre-ageing on bake hardening response of Al-Mg-Si alloy
    Xu, Huan-Huan
    Zhang, Zhi-Qing
    Wu, Sai-Nan
    Huang, Guang-Jie
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2013, 23 (03): : 623 - 627
  • [46] Influence of test temperature on the size effect in molybdenum small-scale compression pillars
    Schneider, A. S.
    Frick, C. P.
    Arzt, E.
    Clegg, W. J.
    Korte, S.
    PHILOSOPHICAL MAGAZINE LETTERS, 2013, 93 (06) : 331 - 338
  • [47] On the effect of pre-straining on the fatigue behaviour of a particulate-reinforced metal-matrix composite
    Beyer, G
    Biermann, H
    Mughrabi, H
    SCRIPTA MATERIALIA, 1997, 36 (08) : 935 - 941
  • [48] The effect of pre-straining on the mechanical behaviour of self-piercing riveted aluminium alloy sheets
    Han, L.
    Young, K. W.
    Hewitt, R.
    Chrysanthou, A.
    O'Sullivan, J. M.
    Sheet Metal 2005, 2005, 6-8 : 157 - 162
  • [49] Influence of uniaxial and biaxial pre-straining on the high cycle fatigue performance of DP590 steel
    Ghosal, Puja
    Paul, Surajit Kumar
    Raj, Abhishek
    INTERNATIONAL JOURNAL OF FATIGUE, 2021, 151
  • [50] Low-cycle fatigue of a metal-matrix composite: Influence of pre-straining on the fatigue life
    Biermann, H
    Beyer, G
    Mughrabi, H
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 234 : 198 - 201