Creep Rupture Strength for Weld Joint of 23Cr-45Ni-7W Alloy

被引:7
|
作者
Nomura, Kyohei [1 ]
Kubushiro, Keiji [1 ]
Nakagawa, Hirokatsu [2 ]
Murata, Yoshinori [3 ]
机构
[1] IHI Corp, Res Lab, Yokohama, Kanagawa 2358501, Japan
[2] IHI Corp, Dept Mat Engn, Energy & Plant Operat, Toyosu, Tokyo 1358710, Japan
[3] Nagoya Univ, Grad Sch Engn, Dept Mat Phys & Energy Engn, Nagoya, Aichi 4648603, Japan
关键词
advanced-ultra super critical (A-USC); HR6W; weld joints; creep strength; microstructure; heat-affected zone; precipitation strengthening; carbides; Laves-phase; HIGH-TEMPERATURE CREEP; AUSTENITIC STAINLESS-STEEL; PHASE;
D O I
10.2320/jinstmet.J2015015
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The creep rupture strength and the degradation mechanism of 23Cr-43Ni-7W alloy weld joints were investigated by creep rupture tests and microstructure observation of the ruptured specimens. The creep rupture tests were conducted at 973, 1023, and 1073 K at stresses from 80 to 180 MPa. The creep strength of the weld joints was higher than that of the base metal. The ruptured area of every specimen was over 10 mm away from the bond line. The microcracks increased gradually up to 10 mm from the bond line, above which they increased suddenly. In the grains, traces of M23C6 were observed near the bond line, and the sizes of the M23C6 deposits increased further away from the bond line. But the size of the Laves phase was constant in every observed area. On the grain boundary, the grain boundary shielding ratio by precipitates was constant until 10 mm from the bond line, above which it decreased. These observations show that the creep strength near the bond line is higher than that of the base metal because of both precipitation strengthening in the grain and grain boundary.
引用
收藏
页码:348 / 355
页数:8
相关论文
共 50 条
  • [21] Creep rupture properties of a Ni-Cr-W superalloy in air environment
    Kurata, Y
    Tsuji, H
    Shindo, M
    Nakajima, H
    JOURNAL OF NUCLEAR MATERIALS, 1997, 246 (2-3) : 196 - 205
  • [22] Creep rupture properties of a Ni-Cr-W superalloy in air environment
    Japan Atomic Energy Research Inst, Ibaraki, Japan
    J Nucl Mater, 2-3 (196-205):
  • [23] Creep-fatigue damage for boiler header stub mock-up specimen of 47Ni-23Cr-23Fe-7W alloy
    Yamazaki N.
    Nomura K.
    Kubushiro K.
    Zairyo/Journal of the Society of Materials Science, Japan, 2019, 68 (02) : 136 - 141
  • [24] Creep-Fatigue Damage for Boiler Header Stub Mock-Up Specimen of 47Ni-23-Cr-23Fe-7W Alloy
    Yamazaki, Naoki
    Nomura, Kyohei
    Kubushiro, Keiji
    MATERIALS TRANSACTIONS, 2020, 61 (06) : 1109 - 1114
  • [25] Prediction of creep deformation and rupture behaviour of 2.25Cr-1Mo weld joint
    Laha, K
    Chandravathi, KS
    Rao, KBS
    Mannan, SL
    Sastry, DH
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2000, 77 (12) : 761 - 769
  • [26] IMPROVEMENT OF CREEP-RUPTURE STRENGTH OF HIGH CR FERRITIC STEEL BY ADDITION OF W
    TSUCHIDA, Y
    OKAMOTO, K
    TOKUNAGA, Y
    ISIJ INTERNATIONAL, 1995, 35 (03) : 317 - 323
  • [27] Creep rupture behavior of 9Cr-1.8W-0.5Mo-VNb (ASME grade 92) ferritic steel weld joint
    Sakthivel, T.
    Vasudevan, M.
    Laha, K.
    Parameswaran, P.
    Chandravathi, K. S.
    Selvi, S. Panneer
    Maduraimuthu, V.
    Mathew, M. D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 591 : 111 - 120
  • [28] Effects of vacuum carburizing treatment on high-temperature creep rupture life of Cr35Ni45Nb alloy
    Peng, Yi-Chao
    Zhang, Mai-Cang
    Xiao, Jiang-Chu
    Du, Chen-Yang
    Dong, Jian-Xin
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2015, 36 (07): : 174 - 181
  • [29] DEGRADATION MECHANISM OF LONG-TERM CREEP RUPTURE STRENGTH IN GR. 23 (2.25CR-1.6W) STEEL
    Komai, Nobuyoshi
    Lmazato, Toshiyuki
    Tominaga, Kimihiko
    Fujita, Masaaki
    JOINT EPRI - 123HIMAT INTERNATIONAL CONFERENCE ON ADVANCES IN HIGH-TEMPERATURE MATERIALS, 2019, 2019, : 185 - 196
  • [30] CREEP-RUPTURE PROPERTIES OF NI-26CR-17W ALLOYS IN AIR
    TANABE, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1984, 70 (13): : 1242 - 1242