Fabrication and dielectric properties of phase-pure Ba2Ti9O20 microwave resonators

被引:0
|
作者
Lin, WY
Gerhardt, RA
Speyer, RF
Hackenberger, WS
Shrout, TR
机构
关键词
D O I
暂无
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
The thermal processing schedules necessary to form phase pure Ba2Ti9O20, with and without substitutional solid solution were investigated. Undoped compositions formed the compound most easily under rapid (500 degrees C/min) heating rates, where diffusional agglomeration of the TiO2 batch constituent was minimized. The compound formed most easily with minor (0.82%) substitutions of SnO2 and ZrO2 for TiO2. The solubility of Sn in Ba2Ti9O20 was higher than that of Zr. Extended heat treatment (16 vs. 6 h at 1390 degrees C) resulted in volitalization of grain boundary liquid phase, leading to a more porous and slightly degraded resonators. The effects of dopant concentrations and soak periods at 1390 degrees C on dielectric constants and temperature-dependent quality factors are reported.
引用
收藏
页码:501 / 506
页数:6
相关论文
共 50 条