Effect of Strain Hardening and Aging Processes on Microstructure Evolution, Tensile and Fatigue Properties of Cast Ti-6Al-2Sn-2Zr-2Mo-1.5Cr-2Nb-0.1Si Alloy

被引:11
|
作者
Elshaer, Ramadan N. [1 ]
El-Deeb, Mostafa S. S. [2 ]
Mohamed, S. S. [3 ]
Ibrahim, Khaled M. [4 ]
机构
[1] Tabbin Inst Met Studies, Cairo, Egypt
[2] Modern Acad Engn & Technol, Cairo, Egypt
[3] Benha Univ, Shoubra Fac Engn, Cairo, Egypt
[4] Cent Met R&D Inst, Cairo, Egypt
关键词
TC21; Ti-Alloy; Strain hardening; Microstructure; Aging; Hardness; Tensile; Fatigue; MECHANICAL-PROPERTIES; TITANIUM-ALLOY; HEAT-TREATMENT; TC21; DEFORMATION; PHASE;
D O I
10.1007/s40962-021-00622-7
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Abstract: The effect of strain hardening and aging processes on microstructure, tensile and fatigue properties was investigated on cast TC21 samples with a chemical composition of Ti-6.1Al-2.96Mo-2.11Nb-1.98Sn-2.05Zr-1.44Cr-0.1Si. Plastic deformation (strain hardening) was applied on swaged samples at room temperature with 2%, 3% and 4% strain. By applying aging process at 575°C for 4 hr, secondary α-platelets were precipitated in the transformed β-phase. Maximum hardness (HV440) was achieved for 4%def. + aged samples. However, minimum hardness (HV323) was recorded for aged samples. Maximum ultimate tensile strength (1311MPa) and elongation (14%) were obtained for 4% def. + aged samples due to presence of high amount of dislocation density as well as precipitation of secondary α-platelets in the residual β-phase. Minimum ultimate tensile strength (1020MPa) and elongation (3%) were reported for as-cast samples. Theoretical study using ANSYS software program was carried out for estimating fatigue limits for investigated samples. For validating the theoretical results, experimental test was done using rotating bending fatigue testing machine on three selected conditions of swaged, 2%def. + aged and 4%def. + aged. Maximum estimated fatigue strength of 775 MPa was obtained for 4%def. + aged samples, and the experimental one was 755 MPa. Hence, the difference between estimated and experimental fatigue limits for 4%def. + aged samples was less than of 3%. Graphical Abstract: [Figure not available: see fulltext.] © 2021, American Foundry Society.
引用
收藏
页码:723 / 737
页数:15
相关论文
共 50 条
  • [31] Effects of microstructure on short crack growth behavior of Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy
    Jin, O
    Mall, S
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 359 (1-2): : 356 - 367
  • [32] Effect of heat treatment and silicon addition on the microstructure development of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, XD
    Bonniwell, P
    Fraser, HL
    Baeslack, WA
    Evans, DJ
    Ginter, T
    Bayha, T
    Cornell, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 343 (1-2): : 210 - 226
  • [33] Effect of stretching on the strength (Bauschinger effect) of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, XD
    Ginter, TJ
    Cornell, B
    Evans, DJ
    Fraser, HL
    JOURNAL OF ADVANCED MATERIALS, 2000, 32 (01): : 34 - 38
  • [34] Effect of stretching on the strength (Bauschinger effect) of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, Xiao-Dong
    Ginter, Timothy J.
    Cornell, Brian
    Evans, Dan J.
    Fraser, Hamish L.
    1600, SAMPE, Covina, CA, United States (32):
  • [35] The fatigue limit of Ti-6Al-2Zr-2Sn-3Mo-1Cr-2Nb titanium alloy with different colony features
    Shi, Xiaohui
    Zeng, Weidong
    Zhao, Qinyang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 645 : 82 - 87
  • [36] Effect of Solution Treatment Temperature on Microstructure and Tensile Properties of Ti-4Al-6Mo-2V-5Cr-2Zr Alloy
    Wang, Shengyuan
    Zhang, Haoyu
    Zhou, Ge
    Chen, Xiaobo
    Chen, Lijia
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2022, 36 (12): : 893 - 899
  • [37] EFFECT OF HYDROGEN ON FLAW GROWTH IN TI-6AL-2SN-4ZR-2MO-0.1SI
    PAO, PS
    WILLE, GW
    JOURNAL OF NUCLEAR MATERIALS, 1982, 103 (1-3) : 931 - 935
  • [38] THE EFFECT OF SHEAR BANDS ON SERVICE PROPERTIES OF TI-6AL-2SN-4ZR-2MO-0.1SI FORGINGS
    SEMIATIN, SL
    LAHOTI, GD
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (04): : 743 - 750
  • [39] Effect of Boron on the Elevated-Temperature Tensile and Creep Behavior of Cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Weight Percent)
    Chen, W.
    Boehlert, C. J.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2009, 40A (07): : 1568 - 1578
  • [40] Effect of Boron on the Elevated-Temperature Tensile and Creep Behavior of Cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Weight Percent)
    W. Chen
    C.J. Boehlert
    Metallurgical and Materials Transactions A, 2009, 40 : 1568 - 1578