Obtention of Hard Coating Using Electrochemical Process in Aluminum-Silicon Alloys for Automotive Vehicles

被引:0
|
作者
Silva, P. R. C. [1 ]
Colosio, M. A. [1 ]
Orlando, M. T. D. [2 ]
Rossi, J. L. [1 ]
机构
[1] Ctr Ciencia & Tecnol Mat CNEN SP, Inst Pesquisas Energet & Nucl IPEN, Ave Prof Lineu Prestes 2242, BR-05508000 Sao Paulo, SP, Brazil
[2] Univ Fed Espirito Santo UFES, Ave Fernando Ferrari 514, Vitoria, ES, Brazil
关键词
anodization; aluminum; surface protection; thermal resistance;
D O I
10.1590/1980-5373-MR-2023-0017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Automotive industry is searching for new ways to improve vehicles' energy efficiency through mass reduction, using aluminum alloys. This change requires a surface protection to extend the life cycle of the components and aluminum anodization is the most used solution. This research is focused on the intake and exhaust ducts' surfaces of aluminum internal combustion engines cylinder head, which are subject to chemical agents and temperature variation. To extend the working life of this component it is necessary to obtain a covering protective layer. The process targeted the anodization of an internal surface of a much larger part of a cast aluminum-silicon alloy cylinder head. The anodization was obtained using a H2SO4 solution (184 g.L-1) and a DC voltage starting at 20 V. The Al2O3 layer obtained, inside the cylinder head & PRIME;s ducts, has an average thickness of 120 & mu;m in accordance with the proposal of providing a suitable surface protection.
引用
收藏
页数:7
相关论文
共 50 条
  • [31] Density and solidification shrinkage of hypoeutectic aluminum-silicon alloys
    Magnusson, T
    Arnberg, L
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (10): : 2605 - 2613
  • [32] Density and solidification shrinkage of hypoeutectic aluminum-silicon alloys
    T. Magnusson
    L. Arnberg
    [J]. Metallurgical and Materials Transactions A, 2001, 32 : 2605 - 2613
  • [33] THE DISSOLUTION OF STRONTIUM-CONTAINING MASTER ALLOYS IN ALUMINUM AND ALUMINUM-SILICON FOUNDRY ALLOYS
    PEKGULERYUZ, M
    CLOSSET, B
    GRUZLESKI, JE
    [J]. CIM BULLETIN, 1985, 78 (878): : 97 - 97
  • [34] ALLOYING ALUMINUM-SILICON ALLOYS TO IMPROVE THEIR PROPERTIES.
    Stepanov, Yu.N.
    Konovalov, Yu.I.
    Gulyaev, B.B.
    Petrov, S.M.
    Shemetev, G.F.
    [J]. Tsvetnye Metally, 1988, 1 : 66 - 68
  • [35] Surface porosity investigation of aluminum-silicon PM alloys
    Steedman, G.
    Bishop, D. P.
    Caley, W. F.
    Kipouros, G. J.
    [J]. POWDER TECHNOLOGY, 2012, 226 : 225 - 230
  • [36] STRUCTURAL MODIFICATION OF ALUMINUM-SILICON ALLOYS BY ANTIMONY TREATMENT
    NAGEL, G
    PORTALIER, R
    [J]. INTERNATIONAL CAST METALS JOURNAL, 1980, 5 (04): : 2 - 6
  • [37] HYPEREUTECTIC ALUMINUM-SILICON ALLOYS 390 AND A390
    JORSTAD, JL
    [J]. TRANSACTIONS OF THE METALLURGICAL SOCIETY OF AIME, 1968, 242 (07): : 1217 - &
  • [38] UNIDIRECTIONAL SLIDING WEAR OF ALUMINUM-SILICON ALLOYS.
    Sarkar, A.D.
    [J]. Light Metal Age, 1982, 40 (1-2): : 30 - 35
  • [39] TRIBOLOGICAL CHARACTERISTICS OF LEADED ALUMINUM-SILICON BEARING ALLOYS
    PATHAK, JP
    [J]. TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1993, 46 (06): : 377 - 385
  • [40] THE MECHANISM OF SILICON MODIFICATION IN ALUMINUM-SILICON ALLOYS - IMPURITY INDUCED TWINNING
    LU, SZ
    HELLAWELL, A
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1987, 18 (10): : 1721 - 1733