High temperature oxidation behavior of Fe-3.0%Si steel with non-equilibrium reaction

被引:3
|
作者
Ma, E. [1 ]
Yang, Xingrui [2 ]
Su, Yingtao [2 ]
Bi, Zimo [2 ]
Sun, Huilan [2 ]
Wang, Bo [2 ]
Ma, Cheng [1 ]
Zhang, Di [2 ]
机构
[1] HBIS Grp, Mat Res Inst, Hebei 050023, Peoples R China
[2] Hebei Univ Sci & Technol, Sch Mat Sci & Engn, Hebei Key Lab Mat Near Net Forming Technol, Shijiazhuang 050000, Peoples R China
基金
中国国家自然科学基金;
关键词
Oxidation mechanism; Fe-3; 0%Si steel; Microstructure evolution; Phase formation; Oxide layer morphology; OXIDE SCALE; IRON; MICROSTRUCTURE; OXYGEN;
D O I
10.1016/j.jmrt.2023.01.163
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The phase formation-transition process and microstructure evolution of Fe-3%Si steel oxide layers were systematically studied during the high-temperature oxidation process with oxidizing atmosphere when annealed at 1000-1240 degrees C for 200 min. The micromor-phology, oxidation mechanism and crystal structure stability were characterized and discussed combining with the XRD, FESEM and XPS technology. The oxidized scale shows more and more complex multiple layers structure including single layer, double layers and three layers with the increasing of annealing temperature, which attributes to the diffusion effect and oxidation reaction oxygen anions and metal cations. The formation of SiO2, FeO and Fe2SiO4 layer also could inhibit the oxidation reaction of matrix. The oxidized scale mainly shows a single layer structure of Fe2O3 when annealed at 1000-1080 degrees C, which is easy to peel off from matrix. It shows a double oxide layers structure when annealed at 1080-1120 degrees C, the loose outer layer contains Fe2O3 , and the grid inner layer contain SiO2, FeO and Fe2SiO4 compounds. It shows an outermost, intermediate and inner three layers structure when annealed at 1160-1240 degrees C. The outermost layer is Fe2O3 , the main phases of intermediate layer are FeO and Fe2SiO4 compounds as well as some SiO2 particles, and the inner layer (joint layer) is SiO2. (c) 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:2587 / 2600
页数:14
相关论文
共 50 条
  • [31] A High-Temperature, Thermal Non-equilibrium Thermochemical Model for Polytetrafluoroethylene
    Sonoda, Shiho
    Henrikson, Erik
    Mikellides, Pavlos
    [J]. INTERNATIONAL JOURNAL OF THERMOPHYSICS, 2011, 32 (09) : 1918 - 1941
  • [32] A High-Temperature, Thermal Non-equilibrium Equation of State for Ammonia
    D. L. Allison
    P. G. Mikellides
    [J]. International Journal of Thermophysics, 2006, 27 : 794 - 819
  • [33] VLWIR high operating temperature non-equilibrium photovoltaic HgCdTe devices
    Velicu, S.
    Grein, C. H.
    Itsuno, A.
    Phillips, J. D.
    [J]. QUANTUM SENSING AND NANOPHOTONIC DEVICES VIII, 2011, 7945
  • [34] Ground test and numerical simulation on high temperature non-equilibrium flow
    Li, Junhong
    Miao, Wenbo
    Shen, Junmou
    Cheng, Xiaoli
    [J]. Hangkong Dongli Xuebao/Journal of Aerospace Power, 2023, 38 (11): : 2574 - 2582
  • [35] A high-temperature, thermal non-equilibrium equation of state for ammonia
    Allison, D. L.
    Mikellides, P. G.
    [J]. INTERNATIONAL JOURNAL OF THERMOPHYSICS, 2006, 27 (03) : 794 - 819
  • [36] Forming mechanism of equilibrium and non-equilibrium metallurgical phases in dissimilar aluminum/steel (Al-Fe) joints
    Shang, Shun-Li
    Sun, Hui
    Pan, Bo
    Wang, Yi
    Krajewski, Adam M.
    Banu, Mihaela
    Li, Jingjing
    Liu, Zi-Kui
    [J]. SCIENTIFIC REPORTS, 2021, 11 (01)
  • [37] Study on the non-equilibrium temperature behavior of normal shock waves and the bulk viscosity
    Ohr, Young Gie
    [J]. PHYSICS OF FLUIDS, 2020, 32 (06)
  • [38] Gram growth and texture evolutions in non-equilibrium microcrystalline high silicon steel
    Anisimova, MV
    Poliak, EI
    [J]. GRAIN GROWTH IN POLYCRYSTALLINE MATERIALS III, 1998, : 573 - 578
  • [39] NON-EQUILIBRIUM SOLIDIFICATION AND MICROSEGREGATION IN CENTRIFUGALLY CAST HIGH SPEED STEEL FOR ROLLS
    Klancnik, U.
    Kosec, B.
    Mrvar, P.
    Medved, J.
    [J]. JOURNAL OF MINING AND METALLURGY SECTION B-METALLURGY, 2018, 54 (01) : 59 - 66
  • [40] High temperature oxidation of Fe-3Si alloy
    Amano, T
    Yamada, K
    Okazaki, M
    Takeda, M
    Onishi, T
    [J]. HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 169 - 173