摘要
To understand the effect of refractories in the ladle lining system on the evolution of inclusions in the secondary refining process, refractory samples were taken from different locations in the ladle system (Slag lining bricks, Sidewall bricks, Refractory mortar, and Bottom bricks). Laboratory experiments were carried out using heavy-rail steel slab samples (Si-Mn-killed steel) and different refractory bricks. The four kinds of refractory bricks can be roughly divided into 3 categories: (1) MgO-Al2O3-C system (MAC, high MgO>55%); (2) Al2O3-MgO-C system (AMC, low MgO<13%); (3) Al2O3-SiO2 system (AS). The results show that after the reaction between molten steel and refractory materials, both AMC (slag lining bricks and sidewall bricks) and MAC (bottom bricks) will dissolve their component Al2O3, increasing [%Al] content in molten steel, forming MgO-Al2O3 type inclusions, and the dissolution of its component MgO depends on the content of MgO. When MgO>55%, MgO will dissolve. When MgO<13%, due to the low activity of MgO, MgO will not dissolve. MgO inclusions were found in the steel when the MgO content in the refractory was higher than 55%. MgO inclusions may originate from the refractory itself. The reduction of TiO2 in the AS (refractory mortar) by [%Al] and [%Si] in the steel increases the [%Ti] content of the steel, forming Ti-containing inclusions.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] A Coupling Model Predicting the Precipitation and Growth of MnS Inclusions in U75V High-Carbon Heavy Rail Steel
    Xue, Zhengliang
    Li, Ning
    Wang, Lu
    Song, Shengqiang
    Liu, Dongming
    Huang, Ao
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2021, 52 (06): : 3860 - 3874
  • [22] Super Long Life Fatigue Properties Of Rail Steel U71Mn And U75V
    Luo Zefu
    Cui Shiming
    Wu Yanzeng
    Wang Qingyuan
    MATERIAL DESIGN, PROCESSING AND APPLICATIONS, PARTS 1-4, 2013, 690-693 : 1753 - 1756
  • [23] Comparative Study on the Cyclic Corrosion Test of Rail Steel U68CuCr and U75V
    Ren An-chao
    Zhou Huan
    Zhu Min
    Yuan Ze-xi
    SUSTAINABLE DEVELOPMENT OF NATURAL RESOURCES, PTS 1-3, 2013, 616-618 : 1059 - +
  • [24] Straightness of U75V 100m Heavy Rail under Deferent Straightening Processes
    Kang, Hao
    Wu, Di
    Zhao, Xian-ming
    NUMBERS, INTELLIGENCE, MANUFACTURING TECHNOLOGY AND MACHINERY AUTOMATION, 2012, 127 : 105 - +
  • [25] The Deformation Rule of the Cooled U75V Heavy Rail Caused by the Different Heat Transfer Coefficient
    Gao Mingxin
    Wang Peilong
    Jia Hao
    Tong Shanhu
    Song Hua
    Yuan Siyu
    Wang Zhongqiang
    MATERIALS AND MANUFACTURING, PTS 1 AND 2, 2011, 299-300 : 1005 - +
  • [26] Microstructure and properties of U75V 60 kg/m heavy rail after slack cooling
    Kang, H. (kanghao@cnitdc.com), 2012, Northeast University (33):
  • [27] Analysis of the evolution law of oxide inclusions in U75V heavy rail steel during the LF-RH refining process
    Liu, Hongbo
    Xie, Rongyuan
    Li, Min
    Zhang, Caidong
    Yao, Hongyong
    Tian, Zhiqiang
    Yang, Haibin
    Liu, Zhanli
    Wang, Qiang
    Kang, Ju
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2023, 42 (01)
  • [28] Effects of Quenching Temperature and Cooling Rate on the Microstructure and Mechanical Properties of U75V Rail Steel
    Yuzhe Lan
    Gang Zhao
    Yaowen Xu
    Chuanlong Ye
    Shaocheng Zhang
    Metallography, Microstructure, and Analysis, 2019, 8 : 249 - 255
  • [29] Effects of Quenching Temperature and Cooling Rate on the Microstructure and Mechanical Properties of U75V Rail Steel
    Lan, Yuzhe
    Zhao, Gang
    Xu, Yaowen
    Ye, Chuanlong
    Zhang, Shaocheng
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2019, 8 (02) : 249 - 255
  • [30] Effect of cooling time on hardened layer of U75V 60 kg/m heavy rail after heat treatment
    Kang, Hao
    Zhao, Xian-Ming
    Wu, Di
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2012, 43 (11): : 4242 - 4247