Industrial-scale fabrication of FeSiCr magnetic powder cores with high magnetic permeability and low loss

被引:10
|
作者
Wang, Pu [1 ]
Zhu, Zhengqu [1 ]
Liu, Jiaqi [1 ]
Wang, Chengfei [1 ]
Pang, Jing [2 ]
Zhang, Jiaquan [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Qingdao Yunlu Adv Mat Technol Co Ltd, Qingdao 266232, Shandong, Peoples R China
关键词
Soft magnetic powder cores; Industrial-scale process; Insulating layer; Soft magnetic properties; Corrosion resistance; PHOSPHATE COATINGS; COMPOSITES; FE; EVOLUTION; MICROSTRUCTURE;
D O I
10.1016/j.jallcom.2023.171095
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
FeSiCr magnetic powders is the key raw material for inductive components such as molding choke and power factor correction (PFC) inductors. In this paper, the industrial-scale insulation coating process of high-performance FeSiCr soft magnetic powder cores (SMPCs) were studied by using mature and environmentally friendly silica sol (SiO2), aluminum dihydrogen phosphate solution (AHP), glass powders (GP), and phosphoric acid (PA) as insulators and water-soluble sodium silicate (NSO) as an inorganic binder, respectively. A comprehensive analysis of the SEM, EDS, and XPS results showed that the surface insulation layer uniformity of the four coating powders is poor due to the irregular morphology of the FeSiCr powder, with the glass powder having the worst coating uniformity due to partial agglomeration occurring in mechanical mixing. The four coated powders all had high saturation magnetization (173.1-176.5 emu.g(-1)), in which the chemical reaction of FeSiCr in the phosphoric acid coating process consumed Fe atoms, resulting in the lowest M-s of the powders in the several coating processes. At the corresponding optimum heat treatment temperature, the FeSiCr@SiO2 @NSO SMPCs had the highest permeability of 96.1, while the FeSiCr@PA@NSO SMPCs had the lowest at 75.5, due to the phosphoric acid consuming part of the ferromagnetic material and the loose porous structure of the phosphate layer further reducing the density of SMPCs. The total losses of the four powder cores are low (228.9-259.2 mW.cm(-3), 100 Gs, 1000 kHz), while loss separation and experiments with different pressing tonnages showed that the eddy current losses of SMPCs was higher than the hysteresis losses, which was caused by the irregular morphology of FeSiCr powders. The FeSiCr@SiO2 @NSO SMPCs exhibit optimum corrosion resistance due to the uniform coating of the SiO2 nano-insulating layer on the powders surface as a result of the strong bonding of the silica sol with FeSiCr. As can be seen, FeSiCr@SiO2 @NSO SMPCs prepared using silica sols have very high saturation magnetization, very high permeability, low core loss, and good corrosion resistance compared to the other three insulation processes and can be industrially produced on a large scale, offering great application prospects in the field of high current and high frequency.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Fe-based amorphous powder cores with low core loss and high permeability fabricated using the core-shell structured magnetic flaky powders
    Sun, Haibo
    Wang, Ce
    Wang, Jinghui
    Yu, Mingguang
    Guo, Zhili
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2020, 502
  • [22] Effect of phosphoric acid concentration on performance of FeSiCr@phosphate/sodium silicate soft magnetic powder cores
    Wang, Pu
    Liu, Jiaqi
    Wang, Chengfei
    Zhu, Zhengqu
    Pang, Jing
    Zhang, Jiaquan
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2024, 55 (08): : 2879 - 2886
  • [23] MEDIUM ALLOYED MAGNETIC STEEL WITH LOW CORE LOSS AND HIGH PERMEABILITY
    HUNEUS, H
    KOCHMANN, T
    SCHOPPA, A
    WICH, H
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1992, 112 (1-3) : 159 - 161
  • [24] Improved permeability of Fe based amorphous magnetic powder cores by adding Permalloy
    Li, B.
    Zheng, Z. G.
    Yu, H. Y.
    Zeng, D. C.
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2017, 438 : 138 - 143
  • [25] Effects of hydrophilic and hydrophobic SiO2 composite organic resin coating on properties of FeSiCr magnetic powder cores
    Lai Xiaoxiang
    Yu Hongya
    Feng Yue
    Zhong Xichun
    Liu Zhongwu
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2022, 50 (02): : 135 - 143
  • [26] Fabrication of FeSiBPNb amorphous powder cores with high DC-bias and excellent soft magnetic properties
    Guo, Junjiang
    Dong, Yaqiang
    Man, Qikui
    Li, Qiang
    Chang, Chuntao
    Wang, Xin-Min
    Li, Run-Wei
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2016, 401 : 432 - 435
  • [27] Fabrication and magnetic properties of novel Fe-based amorphous powder and corresponding powder cores
    Liu, Min
    Huang, Keyu
    Liu, Lei
    Li, Tong
    Cai, Pingping
    Dong, Yaqiang
    Wang, Xin-Min
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2018, 29 (07) : 6092 - 6097
  • [28] Fabrication and magnetic properties of novel Fe-based amorphous powder and corresponding powder cores
    Min Liu
    Keyu Huang
    Lei Liu
    Tong Li
    Pingping Cai
    Yaqiang Dong
    Xin-Min Wang
    Journal of Materials Science: Materials in Electronics, 2018, 29 : 6092 - 6097
  • [29] Effects of Coils on Precision of Magnetic Measurements for Low Permeability Toroidal Cores in High Frequency Region
    Yamamoto K.-I.
    Narita Y.
    Ishiyama K.
    IEEJ Transactions on Fundamentals and Materials, 2023, 143 (06) : 216 - 221
  • [30] Nanostructured soft magnetic material with low loss and low permeability
    Fukunaga, H
    Furukawa, N
    Tanaka, H
    Nakano, M
    JOURNAL OF APPLIED PHYSICS, 2000, 87 (09) : 7103 - 7105