Optimization of local modified metakaolin-based geopolymer concrete by Taguchi method

被引:3
|
作者
Al Obeidy, Nazar F. [1 ]
Khalil, Wasan I. [1 ]
Ahmed, Hisham K. [2 ]
机构
[1] Univ Technol Baghdad, Civil Engn Dept, Baghdad, Iraq
[2] Al Esraa Univ Coll, Dept Comp Tech Engn, Bldg & Construct Technol Dept, Baghdad, Iraq
来源
OPEN ENGINEERING | 2024年 / 14卷 / 01期
关键词
geopolymer concrete; Taguchi method; sustainability; metakaolin; MICROSTRUCTURE;
D O I
10.1515/eng-2022-0561
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Geopolymer in recent concrete (GP) has gained significant attention due to its sustainability and environmental friendliness. Local metakaolin-based geopolymer is weaker than geopolymers made from other materials due to its low Si/Al ratio. A consistent mixture design is also lacking because geopolymers are affected by many variables. This study presents a method to find the optimal geopolymer mixture based on locally modified metakaolin as a source of aluminates and silicates using the Taguchi method. Metakaolin was modified using different contents of materials rich in silica, such as silica fume (SF), or materials rich in calcium, such as calcium oxide (CaO) of 5, 10, and 15%. The inclusion of 5% SF, 10% CaO, and a combination of 5% SF and 5% CaO as substitutes for metakaolin increases the compressive strength by 16.8, 6.9, and 22.8%, respectively, compared to the reference mixture without any modifications. In other words, adding 5% SF and CaO increased the molar ratio of SiO2/Al2O3 (R) from 1.782 to 1.914, resulting in the highest compressive strength of 53.3 MPa after 7 days of sun curing. To obtain the optimal mixture that achieves the highest compressive strength, the impact of three main variables, including the concentration of sodium hydroxide (SH), alkali solution-to-binder (Al/B) ratio, and sodium silicate-to-sodium hydroxide (SS/SH) ratio, must be considered using Taguchi method. A total of nine mixtures were investigated. It was found that 13 M of SH, 0.65 Al/B, and 2.5 SS/SH give a high compressive strength of 58.6 MPa at 7 days. Also, it was found that the concentration of SH plays a more important role in increasing the compressive strength than the alkali-to-binder ratio and SS/SH ratio. The scanning electron microscopy images show that the 5% weight replacement of metakaolin by silica and CaO could source fewer and smaller pores and reduce the microcracks' width.
引用
收藏
页数:17
相关论文
共 50 条
  • [21] Carbonation in the pore solution of metakaolin-based geopolymer
    Cyr, Martin
    Pouhet, Raphaelle
    CEMENT AND CONCRETE RESEARCH, 2016, 88 : 227 - 235
  • [22] Effect of Size of Coarse Aggregate on Mechanical Properties of Metakaolin-Based Geopolymer Concrete and Ordinary Concrete
    Fazli, Hamed
    Yan, Dongming
    Zhang, Yajun
    Zeng, Qiang
    MATERIALS, 2021, 14 (12)
  • [23] The use of machine learning techniques to investigate the properties of metakaolin-based geopolymer concrete
    Afzali, Seyed Ali Eftekhar
    Shayanfar, Mohsen Ali
    Ghanooni-Bagha, Mohammad
    Golafshani, Emad
    Ngo, Tuan
    JOURNAL OF CLEANER PRODUCTION, 2024, 446
  • [24] Metakaolin-Based Porous Geopolymer with Aluminium Powder
    Keawpapasson, Pimpawee
    Tippayasam, Chayanee
    Ruangjan, Silawat
    Thavorniti, Pajaree
    Panyathanmaporn, Thammarat
    Fontaine, Alexandre
    Leonelli, Cristina
    Chaysuwan, Duangrudee
    TRADITIONAL AND ADVANCED CERAMICS, 2014, 608 : 132 - +
  • [25] Taguchi-grey relational analysis for optimizing the compressive strength and porosity of metakaolin-based geopolymer
    Al-Sultani S.A.J.
    Disher Al-Hydary I.A.
    Ahmed Al-Dujaili M.A.
    International Journal of Engineering, Transactions B: Applications, 2021, 34 (11): : 2525 - 2533
  • [26] Investigating irradiation effects on metakaolin-based geopolymer
    Mahrous, Mahmoud A.
    Abdelghany, Muhammad A.
    Trindade, Ana Carolina Constancio
    Aboukhatwa, Mohamed
    Kriven, Waltraud M.
    Jasiuk, Iwona M.
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 437
  • [27] Experimental Study on the Mechanical Properties and Microstructure of Metakaolin-Based Geopolymer Modified Clay
    Shi, Xianzeng
    Zha, Qingkun
    Li, Shuqing
    Cai, Guojun
    Wu, Dun
    Zhai, Chaojiao
    MOLECULES, 2022, 27 (15):
  • [28] Optimization of Hybrid Microwave Curing Approach Based On the Performance of Metakaolin-Based Geopolymer Mortars
    Atalay, Yigit Alper
    Aydin, Tolga
    Bundur, Zeynep Basaran
    Mokhtari, Pozhhan
    Gulgun, Mehmet Ali
    Lafhaj, Zoubeir
    TURKISH JOURNAL OF CIVIL ENGINEERING, 2024, 35 (06):
  • [29] Effect of carbonation curing on the physical, mechanical, and microstructural properties of metakaolin-based geopolymer concrete
    Beltrame, Neusa Ap. Munhak
    Dias, Roberto Luiz
    Witzke, Franky Bruno
    Medeiros-Junior, Ronaldo A.
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 406
  • [30] Effect of GGBFS on the mechanical properties of metakaolin-based self-compacting geopolymer concrete
    Luo, Yiping
    Yang, Lianbi
    Wang, Defa
    Zhang, Qianzheng
    Wang, Zhiyang
    Xing, Meiguang
    Xue, Guobin
    Zhang, Jie
    Liu, Zhao
    JOURNAL OF BUILDING ENGINEERING, 2024, 96