Influence of Diffusion Bonding Pressure on Microstructural Features and Strength Performance of Dissimilar Ti-6Al-4V Alloy and AISI 304 Steel Joints Developed Using Copper Interlayer

被引:9
|
作者
Negemiya, A. Arun [1 ]
Rajakumar, Selvarajan [2 ]
Sonar, Tushar [3 ]
Ivanov, Mikhail [3 ]
机构
[1] Sri Shakthi Inst Engn & Technol, Dept Mech Engn, Coimbatore 641062, Tamil Nadu, India
[2] Annamalai Univ, Ctr Mat Joining & Res CEMAJOR, Dept Mfg Engn, Annamalainagar 608002, Tamil Nadu, India
[3] South Ural State Univ, Natl Res Univ, Inst Engn & Technol, Dept Welding Engn, Chelyabinsk 454080, Russia
关键词
diffusion bonding; Ti6Al4V titanium alloy; AISI 304 austenitic stainless steel; microstructure; mechanical properties; MICRODUPLEX STAINLESS-STEEL; TITANIUM-ALLOY; MECHANICAL-PROPERTIES; INTERFACE MICROSTRUCTURE; PHASE-TRANSFORMATION; BONDED JOINTS; 304-STAINLESS-STEEL; TEMPERATURE; SILVER; NICKEL;
D O I
10.1115/1.4062443
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The joining of Ti-6Al-4V (Ti64) alloy and AISI 304 austenitic stainless steel (ASS 304) carries significant importance in aeroengines for turbine blade applications. However, it is difficult to join using fusion welding. The fusion welding of Ti64 alloy and ASS 304 steel promotes the evolution of various Fe-Cr-Ti and Fe-Ti intermetallics in weld zone owing to limited solid solubility of Fe, Cr, Ti, and Ni with each other. The evolution of these intermetallics deteriorates the strength performance of joints. Hence for joining Ti64 alloy and ASS 304 steel, vacuum diffusion bonding (VDB) method is employed with thin copper (Cu) foil as an interlayer. The DB pressure extends significant influence on microstructural evolution and strength of joints. So, for the feasibility of joining Ti64 alloy and ASS 304 steel, the effect of DB pressure on microstructure and strength of joints is investigated. Results showed that the dissimilar joints of Ti64 alloy and ASS 304 steel developed using the DB pressure of 14 MPa exhibited greater lap shear strength (LSS) and bonding strength (BS) of 180 MPa and 268 MPa, respectively. It is attributed to the improved coalescence of joining interface and the development of ideal bonding width with the least amount of embrittlement consequences. An increase in DB pressure increases the width of the diffusion region which promotes the development of detrimental intermetallics of Ti-Fe and deteriorates the strength of dissimilar joints.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Influence of bonding time during diffusion bonding of Ti-6Al-4V to AISI 321 stainless steel on metallurgical and mechanical properties
    Wang, Hongliang
    Paidar, Moslem
    Kumar, N. Keerthi
    Eldin, Hany M. Seif
    Kannan, Sathish
    Abdullaev, Sherzod
    Mehrez, Sadok
    VACUUM, 2024, 222
  • [22] Microstructural features of thermochemical processing in a Ti-6Al-4V alloy
    Fang, TY
    Wang, WH
    MATERIALS CHEMISTRY AND PHYSICS, 1998, 56 (01) : 35 - 47
  • [23] Diffusion Bonding of Ti6Al4V and SS 304 with Nb Interlayer
    Thirunavukarasu, Gopinath
    Patel, Vivek V.
    Kundu, Sukumar
    Alankar, Alankar
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2019, 8 (05) : 1008 - 1031
  • [24] Microstructure and interface characterization of dissimilar friction stir welded lap joints between Ti-6Al-4V and AISI 304
    Campo, Kaio Niitsu
    Campanelli, Leonardo Contri
    Bergmann, Luciano
    dos Santos, Jorge Fernandez
    Bolfarini, Claudemiro
    MATERIALS & DESIGN, 2014, 56 : 139 - 145
  • [25] Superplastic characteristics and diffusion bonding of Ti-6Al-4V alloy
    Lee, Ho-Sung
    Yoon, Jong-Hoon
    Yi, Yeong-Moo
    Shin, Dong Hyuk
    MECHANICAL BEHAVIOR OF MATERIALS X, PTS 1AND 2, 2007, 345-346 : 549 - +
  • [26] Diffusion bonding of a microduplex stainless steel to Ti-6Al-4V
    Orhan, N
    Khan, TI
    Eroglu, M
    SCRIPTA MATERIALIA, 2001, 45 (04) : 441 - 446
  • [27] Interfacial reaction products formation in the diffusion bonded joints made between Ti-6Al-4V and AISI 304L with brass interlayer
    Vigraman, T.
    Babu, R., V
    Kumar, R. Narendra
    MATERIALS TODAY-PROCEEDINGS, 2021, 43 : 1071 - 1080
  • [28] Experimental investigation of Ti-6Al-4V titanium alloy and 304L stainless steel friction welded with copper interlayer
    Kumar, R.
    Balasubramanian, M.
    DEFENCE TECHNOLOGY, 2015, 11 (01): : 65 - 75
  • [29] Development of processing windows for diffusion bonding of Ti-6Al-4V titanium alloy and 304 stainless steel with silver as intermediate layer
    Balasubramanian, M.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (09) : 2932 - 2938
  • [30] Diffusion brazing of Ti-6Al-4V and AISI 304: an EBSD study and mechanical properties
    Norouzi, Ehsan
    Shamanian, Morteza
    Atapour, Masoud
    Khosravi, Babak
    JOURNAL OF MATERIALS SCIENCE, 2017, 52 (20) : 12467 - 12475