Temperature gradient based annealing methodology for tungsten recrystallization kinetics assessment

被引:2
|
作者
Lemetais, Maxime [1 ,2 ,3 ]
Lenci, Matthieu [1 ]
Maurice, Claire [1 ]
Devictor, Timothee [1 ]
Durif, Alan [2 ]
Minissale, Marco [4 ]
Mondon, Marilyne [1 ]
Pintsuk, Gerald [5 ]
Piot, David [1 ]
Gallais, Laurent [3 ]
Richou, Marianne [2 ]
Kermouche, Guillaume [1 ]
机构
[1] Mines St Etienne, Ctr SMS, CNRS, LGF,UMR 5307, F-42023 St Etienne, France
[2] CEA, IRFM, F-13108 St Paul Les Durance, France
[3] Aix Marseille Univ, Inst Fresnel, CNRS, Cent Marseille, Marseille, France
[4] Aix Marseille Univ, CNRS, PIIM, Marseille, France
[5] Forschungszentrum Julich, Inst Energie & Klimaforsch, D-52425 Julich, Germany
关键词
Characterization; High -temperature annealing; Laser -based annealing; Recrystallization; Softening; Tungsten; Thermonuclear fusion; Hardness; WARM-ROLLED TUNGSTEN; IMPACT;
D O I
10.1016/j.fusengdes.2023.113785
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In future thermonuclear fusion reactors, like ITER and DEMO, plasma-facing components with tungsten armor material will have to sustain high thermal fluxes (10 MW/m2 in steady state and 20 MW/m2 in quasi-steadystate). For such extreme conditions, tungsten may reach temperatures higher than 1000 degrees C and, consequently can be prone to recrystallize, which can limit the lifetime of the divertor targets under cycling thermal loadings. Characterization of recrystallization kinetics involves the use of different methods and devices (furnace, laser heating) depending on the annealing temperature regime to be analyzed. For these methods, the heating and the subsequent characterization of around 10 samples (5 x 4 x 4 mm) per annealing temperature is needed. In this article, a method is proposed to quantify the recrystallization kinetics between 1300 degrees C and 1600 degrees C using a limited number of samples and heating conditions. The basic idea is to induce a steady-state temperature gradient in tungsten rods by heating one side of the rod using a laser heating system. Tungsten rods (50 x 4 x 5 mm) were annealed with this method. The resulting microstructures are characterized using optical microscopy and hardness measurements. The different stages of tungsten softening are clearly evidenced. These first results can be considered as a proof of concept for the use of such a methodology to assess tungsten recrystallization at high temperature.
引用
收藏
页数:6
相关论文
共 50 条
  • [21] Recrystallization behavior of hot-rolled pure tungsten and its alloy plates during high-temperature annealing
    Tsuchida, Kohei
    Miyazawa, Takeshi
    Hasegawa, Akira
    Nogami, Shuhei
    Fukuda, Makoto
    NUCLEAR MATERIALS AND ENERGY, 2018, 15 : 158 - 163
  • [22] High temperature annealing of ion irradiated tungsten
    Ferroni, Francesco
    Yi, Xiaoou
    Arakawa, Kazuto
    Fitzgerald, Steven P.
    Edmondson, Philip D.
    Roberts, Steve G.
    ACTA MATERIALIA, 2015, 90 : 380 - 393
  • [23] Dual-effects of carbon doping on the recrystallization kinetics of the Cantor alloy during mid-temperature annealing
    Chen, Wentian
    Wu, Yufan
    Guo, Lin
    Gu, Ji
    He, Junyang
    Song, Min
    INTERMETALLICS, 2023, 155
  • [24] INFLUENCE OF DEFORMATION TEMPERATURE ON KINETICS OF RECRYSTALLIZATION OF MAGNESIUM
    FROMAGEAU, R
    PASTOL, JL
    REVEL, G
    COMPTES RENDUS HEBDOMADAIRES DES SEANCES DE L ACADEMIE DES SCIENCES SERIE C, 1976, 282 (08): : 379 - 381
  • [25] REDUCTION OF DOPING IN ZONE RECRYSTALLIZATION WITH A TEMPERATURE-GRADIENT
    LOZOVSKII, VN
    KHULLA, VD
    INORGANIC MATERIALS, 1979, 15 (08) : 1094 - 1097
  • [26] Temperature and temperature gradient dependence of snow recrystallization in depth hoar snow
    Kamata, Y
    Sokratov, SA
    Sato, A
    ADVANCES IN COLD-REGION THERMAL ENGINEERING AND SCIENCES: TECHNOLOGICAL, ENVIRONMENTAL, AND CLIMATOLOGICAL IMPACT, 1999, 533 : 395 - 402
  • [27] EFFECT OF BUBBLE PARAMETERS ON SECONDARY RECRYSTALLIZATION TEMPERATURE OF DOPED TUNGSTEN
    SCHADE, P
    PLANSEEBERICHTE FUR PULVERMETALLURGIE, 1976, 24 (04): : 243 - 253
  • [28] ANNEALING AND RECRYSTALLIZATION KINETICS OF ULTRATHIN GOLD WIRES - MODULUS AND RESISTIVITY MEASUREMENTS
    BUSCH, K
    KUNZI, HU
    ILSCHNER, B
    SCRIPTA METALLURGICA, 1988, 22 (04): : 501 - 505
  • [29] Recovery and recrystallization kinetics of differently rolled, thin tungsten plates in the temperature range from 1325 °C to 1400 °C
    Ciucani, Umberto M.
    Thum, Angela
    Devos, Chloe
    Pantleon, Wolfgang
    NUCLEAR MATERIALS AND ENERGY, 2019, 20
  • [30] EFFECT OF A TEMPERATURE GRADIENT ON BUBBLE GROWTH IN TUNGSTEN
    DAWSON, CW
    METALLURGICAL TRANSACTIONS, 1972, 3 (12): : 3103 - 3107