Effect of interlayer coating La2O3 particles on arc behavior and microstructure of wire arc additive manufacturing Al-Si alloy deposition

被引:10
|
作者
Fan, Yufeng [1 ]
Chen, Furong [1 ]
Cao, Silong [1 ,2 ]
Hu, Yanan [1 ]
Xie, Ruijun [1 ]
Yang, Yihang [1 ]
机构
[1] Inner Mongolia Univ Technol, Sch Mat Sci & Engn, Hohhot 010051, Peoples R China
[2] Minist Educ, Engn Res Ctr Dev & Proc Protect Adv Light Met, Hohhot 010051, Peoples R China
基金
中国国家自然科学基金;
关键词
Additive manufacturing; La; 2; O; 3; powder; Al-Si alloy; Arc behavior; Microstructure evolution; MECHANICAL-PROPERTIES;
D O I
10.1016/j.jmapro.2023.06.032
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, three kinds of ER4043 aluminum alloy depositions with the interlayer coating La2O3 particles were successfully fabricated by cold metal transfer (CMT) wire arc additive manufacturing (WAAM) technology, and the evolution of various La2O3 particles size on arc behavior, forming defects, microstructure and mechanical properties was described. The results indicated that arc length and horizontal diameter of the CMT-WAAM specimens were directly related to the size of coating La2O3 particles. When the interlayer was coated ordinary and micron-sized La2O3 particles, the violent arc fluctuations and welding spatter were generated and deteriorated forming quality. When the interlayer was coated nano-sized La2O3 particles, the proper arc deflection could improve the fluidity of the molten pool and promote the stomas escape to obtain excellent forming quality. The tensile strength in both horizontal and vertical directions increased to 209.17 MPa and 165.34 MPa, which were 22.55 % and 15.82 % higher than that of the additive specimen without coated powder, respectively. A majority of La2O3 particles were existed in grain boundaries in a form of like-eutectic. Additionally, some of dissociated La2O3 particles became heterogeneous nucleation sites and were included in the Al matrix. This process of interlayer coating nano-sized La2O3 provided more nucleation masses and further refined microstructure of the WAAM specimens during the solidification. The results from this study provided an essential reference to introduce rare earth oxides into deposited interlayer and improve the mechanical properties of CMT-WAAM depositions.
引用
收藏
页码:943 / 958
页数:16
相关论文
共 50 条
  • [31] Microstructure evolution and mechanical properties of the wire plus arc additive manufacturing Al-Cu alloy
    Wang, Zhennan
    Lin, Xin
    Wang, Lilin
    Cao, Yang
    Zhou, Yinghui
    Huang, Weidong
    ADDITIVE MANUFACTURING, 2021, 47
  • [32] Microstructure and Mechanical Properties of Cu-6.5%Al Alloy Deposited by Wire Arc Additive Manufacturing
    Yanhu Wang
    Chuanchu Su
    Sergey Konovalov
    Metallography, Microstructure, and Analysis, 2021, 10 : 634 - 641
  • [33] Effect of Deposition Strategies on the Microstructure and Tensile Properties of Wire Arc Additive Manufactured Al-5Si Alloys
    Chuanchu Su
    Xizhang Chen
    Sergey Konovalov
    R. Arvind Singh
    S. Jayalakshmi
    Lei Huang
    Journal of Materials Engineering and Performance, 2021, 30 : 2136 - 2146
  • [34] Effect of Deposition Strategies on the Microstructure and Tensile Properties of Wire Arc Additive Manufactured Al-5Si Alloys
    Su, Chuanchu
    Chen, Xizhang
    Konovalov, Sergey
    Arvind Singh, R.
    Jayalakshmi, S.
    Huang, Lei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (03) : 2136 - 2146
  • [35] Microstructure, Mechanical, and Tribological Behavior of Al-5%Si Thin Wall Fabricated through Wire Arc Additive Manufacturing
    Kishor, Gaurav
    Mugada, Krishna Kishore
    Mahto, Raju Prasad
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [36] Research on hot deformation behavior and microstructure characterization of the NiTi alloy fabricated by wire arc additive manufacturing
    Chen, Xiaochun
    Chen, Hongsheng
    Nie, Huihui
    Wang, Wenxian
    Zheng, Liuwei
    Zhou, Jun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 9180 - 9194
  • [37] Development of Wire Arc Additive Manufactured Cu-Si Alloy: Study of Microstructure and Wear Behavior
    Kashif Hasan Kazmi
    Sumit K. Sharma
    Alok Kumar Das
    Amitava Mandal
    Amarish Shukla
    Journal of Materials Engineering and Performance, 2024, 33 : 110 - 119
  • [38] Development of Wire Arc Additive Manufactured Cu-Si Alloy: Study of Microstructure and Wear Behavior
    Kazmi, Kashif Hasan
    Sharma, Sumit K.
    Das, Alok Kumar
    Mandal, Amitava
    Shukla, Amarish
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (01) : 110 - 119
  • [39] Effects of Fe Content on Microstructure and Properties of Al-7Si-0.6Mg Alloy Fabricated by Wire Arc Additive Manufacturing
    Li, Chengde
    Gu, Huimin
    Wang, Wei
    Wang, Shuai
    Ren, Lingling
    Zhai, Yu-Chun
    Wang, Zhenbiao
    Ming, Zhu
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2020, 49 (06): : 1860 - 1866
  • [40] Effects of Fe Content on Microstructure and Properties of Al-7Si-0.6Mg Alloy Fabricated by Wire Arc Additive Manufacturing
    Li Chengde
    Gu Huimin
    Wang Wei
    Wang Shuai
    Ren Lingling
    Zhai Yu-chun
    Wang Zhenbiao
    Ming Zhu
    RARE METAL MATERIALS AND ENGINEERING, 2020, 49 (06) : 1860 - 1866