Effect of cryogenic conditions on the critical crack tip opening displacement for the laminated material AA2519-AA1050-Ti6Al4V-T62

被引:1
|
作者
Kotyk, Maciej [1 ]
机构
[1] Bydgoszcz Univ Sci & Technol, Al Prof S Kaliskiego 7, PL-85796 Bydgoszcz, Poland
关键词
Uniaxial loading; Fracture life; Fracture toughness; Explosive welding; Cryogenic conditions; CTOD FRACTURE-TOUGHNESS; AL/TI LAYERED MATERIAL; GROWTH ANALYSIS; AMBIENT; ALLOY;
D O I
10.1016/j.jmrt.2023.12.211
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the case of operating technical objects in conditions that accelerate material wear, it is necessary to adequately protect the object from the aggressive working environment. There are several possibilities, ranging from applying surface coatings (paint, varnish, galvanic layers) to the use of composites. An example of such a material is a composite formed by explosively welded AA2519, AA1050, and Ti6Al4V alloys. Since the described material is relatively new, its mechanical properties are still being determined. Therefore, in this article, the results of research and their analysis regarding the fracture toughness of the described composite in comparison to the fracture toughness of the base materials in the selected range are presented. The main objective of study was to determine the crack tip opening displacement (CTOD) values for the AA2519-AA1050-Ti6Al4V laminated material explosively welded under ambient and cryogenic conditions. The tests were carried out to determine the effect of the aforementioned temperature conditions on selected properties of the tested laminated material. This paper presents the theoretical basis and the adopted testing methodology. The experimental results obtained and their analysis are also presented. Thanks to the analysis, the effect of cryogenic conditions on the value of the crack tip opening displacement was observed. Moreover, the state of knowledge presented in earlier publications on crack tip opening displacement determination for base materials, i.e. AA2519 and Ti6Al4V, has been extended. The paper also presents a CTOD determination procedure for laminated material based on the knowledge on the mechanical properties of the base materials.
引用
收藏
页码:3319 / 3332
页数:14
相关论文
共 50 条
  • [31] The optimization of friction spot welding process parameters in AA6181-T4 and Ti6Al4V dissimilar joints
    Plaine, A. H.
    Gonzalez, A. R.
    Suhuddin, U. F. H.
    dos Santos, J. F.
    Alcantara, N. G.
    MATERIALS & DESIGN, 2015, 83 : 36 - 41
  • [32] Microstructure and mechanical behavior of friction spot welded AA6181-T4/Ti6Al4V dissimilar joints
    A. H. Plaine
    U. F. H. Suhuddin
    N. G. Alcântara
    J. F. dos Santos
    The International Journal of Advanced Manufacturing Technology, 2017, 92 : 3703 - 3714
  • [33] Effect of ultrasound-assisted vibration on Ti-6Al-4V/Al2024-T351 laminated material processing with geometric tools
    Lei Wei
    Dazhong Wang
    The International Journal of Advanced Manufacturing Technology, 2020, 106 : 219 - 232
  • [34] Effect of ultrasound-assisted vibration on Ti-6Al-4V/Al2024-T351 laminated material processing with geometric tools
    Wei, Lei
    Wang, Dazhong
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 106 (1-2): : 219 - 232
  • [35] Effect of test frequency on fatigue crack growth rates of Ti-6Al-4V ELI alloy at cryogenic temperature
    Yuri, T.
    Ono, Y.
    Ogata, T.
    ADVANCES IN CRYOGENIC ENGINEERING, VOL 52A & 52B, 2006, 824 : 153 - +
  • [36] On the Effect of Testing Frequency on High and Very High Cycle Fatigue Behavior of AA2024-T3, Ti-6Al-4V, and Inconel 718
    Kuliiev, Ruslan
    Riekehr, Stefan
    Ventzke, Volker
    Keller, Soeren
    Kashaev, Nikolai
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (23) : 10843 - 10856
  • [37] On the Effect of Testing Frequency on High and Very High Cycle Fatigue Behavior of AA2024-T3, Ti-6Al-4V, and Inconel 718
    Ruslan Kuliiev
    Stefan Riekehr
    Volker Ventzke
    Sören Keller
    Nikolai Kashaev
    Journal of Materials Engineering and Performance, 2023, 32 : 10843 - 10856
  • [38] Experimental Verification of the Crack Opening Displacement Using Finite Element Method for CT Specimens Made of Ti6Al4V Titanium Alloy
    Soltysiak, Robert
    Boronski, Dariusz
    Kotyk, Maciej
    FATIGUE FAILURE AND FRACTURE MECHANICS XXVI, 2016, 1780
  • [39] Highlighting the effect of the aluminium alloy self-corrosion on the AA2024-T3/Ti6Al4V galvanic coupling in NaCl media
    Coelho, L. B.
    Hacha, M.
    Paint, Y.
    Olivier, M-G
    SURFACES AND INTERFACES, 2019, 16 : 15 - 21
  • [40] Effect of Ag interlayer on the microstructural properties and nanocreep behavior of Ti6Al4V/AA7075 dissimilar laser weldments
    Iltaf, Asim
    Barka, Noureddine
    Dehghan, Shayan
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2024, 238 (11) : 2259 - 2272