Effect of cryogenic conditions on the critical crack tip opening displacement for the laminated material AA2519-AA1050-Ti6Al4V-T62

被引:1
|
作者
Kotyk, Maciej [1 ]
机构
[1] Bydgoszcz Univ Sci & Technol, Al Prof S Kaliskiego 7, PL-85796 Bydgoszcz, Poland
关键词
Uniaxial loading; Fracture life; Fracture toughness; Explosive welding; Cryogenic conditions; CTOD FRACTURE-TOUGHNESS; AL/TI LAYERED MATERIAL; GROWTH ANALYSIS; AMBIENT; ALLOY;
D O I
10.1016/j.jmrt.2023.12.211
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the case of operating technical objects in conditions that accelerate material wear, it is necessary to adequately protect the object from the aggressive working environment. There are several possibilities, ranging from applying surface coatings (paint, varnish, galvanic layers) to the use of composites. An example of such a material is a composite formed by explosively welded AA2519, AA1050, and Ti6Al4V alloys. Since the described material is relatively new, its mechanical properties are still being determined. Therefore, in this article, the results of research and their analysis regarding the fracture toughness of the described composite in comparison to the fracture toughness of the base materials in the selected range are presented. The main objective of study was to determine the crack tip opening displacement (CTOD) values for the AA2519-AA1050-Ti6Al4V laminated material explosively welded under ambient and cryogenic conditions. The tests were carried out to determine the effect of the aforementioned temperature conditions on selected properties of the tested laminated material. This paper presents the theoretical basis and the adopted testing methodology. The experimental results obtained and their analysis are also presented. Thanks to the analysis, the effect of cryogenic conditions on the value of the crack tip opening displacement was observed. Moreover, the state of knowledge presented in earlier publications on crack tip opening displacement determination for base materials, i.e. AA2519 and Ti6Al4V, has been extended. The paper also presents a CTOD determination procedure for laminated material based on the knowledge on the mechanical properties of the base materials.
引用
收藏
页码:3319 / 3332
页数:14
相关论文
共 50 条
  • [1] Crack initiation and growth analysis in explosively welded AA2519-AA1050-Ti6Al4V layered material in ambient and cryogenic conditions
    Boronski, Dariusz
    Kotyk, Maciej
    Mackowiak, Pawel
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2018, 232 (08) : 1470 - 1480
  • [2] Mechanical properties of explosively welded AA2519-AA1050-Ti6Al4V layered material at ambient and cryogenic conditions
    Boronski, Dariusz
    Kotyk, Maciej
    Mackowiak, Pawel
    Sniezek, Lucjan
    MATERIALS & DESIGN, 2017, 133 : 390 - 403
  • [3] The Effect of Heat Treatment (T62) on the Tensile Shearing Test of Explosively Welded Layered Material AA2519-AA1050-Ti6Al4V
    Kotyk, Maciej
    Brych, Lukasz
    INTERNATIONAL JOURNAL OF HEAT AND TECHNOLOGY, 2024, 42 (06) : 1870 - 1878
  • [4] Local mechanical properties of explosively welded AA2519-AA1050-Ti6Al4V layered material
    Boronski, Dariusz
    WELDING IN THE WORLD, 2020, 64 (12) : 2083 - 2099
  • [5] Investigation of the Fracture Process of Explosively Welded AA2519-AA1050-Ti6Al4V Layered Material
    Boronski, Dariusz
    Dzioba, Ihor
    Kotyk, Maciej
    Krampikowska, Aleksandra
    Pala, Robert
    MATERIALS, 2020, 13 (10)
  • [6] Local mechanical properties of explosively welded AA2519-AA1050-Ti6Al4V layered material
    Dariusz Boroński
    Welding in the World, 2020, 64 : 2083 - 2099
  • [7] Mechanical and microstructural characteristics of Ti6Al4V/AA2519 and Ti6Al4V/AA1050/AA2519 laminates manufactured by explosive welding
    Bazarnik, P.
    Adamczyk-Cieslak, B.
    Galka, A.
    Plonka, B.
    Sniezek, L.
    Cantoni, M.
    Lewandowska, M.
    MATERIALS & DESIGN, 2016, 111 : 146 - 157
  • [8] Mechanical Properties Analysis of the AA2519-AA1050-Ti6Al4V Explosive Welded Laminate
    Szachogluchowicz, Ireneusz
    Sniezek, Lucjan
    Slezak, Tomasz
    Kluczynski, Janusz
    Grzelak, Krzysztof
    Torzewski, Janusz
    Fras, Teresa
    MATERIALS, 2020, 13 (19) : 1 - 16
  • [9] Ti6Al4V-AA1050-AA2519 explosively-cladded plates under impact loading
    Fras, T.
    Szachogluchowicz, I.
    Sniezek, L.
    EUROPEAN PHYSICAL JOURNAL-SPECIAL TOPICS, 2018, 227 (1-2): : 17 - 27
  • [10] Ti6Al4V-AA1050-AA2519 explosively-cladded plates under impact loading
    T. Fras
    I. Szachogluchowicz
    L. Sniezek
    The European Physical Journal Special Topics, 2018, 227 : 17 - 27