Microstructure and dielectric properties of 0.99 (0.94Bi0.47Na0.47Ba0.06TiO3-0.06BiAlO3)-0.01NaNbO3 lead-free ceramics via different methods

被引:2
|
作者
Lian, Han-li [1 ]
He, Ya-ru [1 ]
Liu, Li-na [2 ]
Chen, Xiao-ming [2 ]
Liang, Xin-juan [1 ]
Wu, Wen-wen [2 ]
Guo, Wei-ming [3 ]
机构
[1] Xian Univ Posts & Telecommun, Sch Sci, Xian 710121, Peoples R China
[2] Shaanxi Normal Univ, Sch Phys & Informat Technol, Xian 710119, Peoples R China
[3] Guangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Peoples R China
基金
中国国家自然科学基金;
关键词
Microstructure; Dielectric properties; Lead-free ceramics; BNT; ENERGY-STORAGE PROPERTIES; FERROELECTRIC PROPERTIES; ELECTRICAL-PROPERTIES; PIEZOELECTRIC PROPERTIES; PERMITTIVITY; FIELD;
D O I
10.1016/j.matchemphys.2023.127457
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, 0.99(0.94Bi0.47Na0.47Ba0.06TiO3-0.06BiAlO3)-0.01NaNbO3 lead-free ceramics were synthesized by means of different methods including conventional solid state sintering (SSS), cold-sintering-assisted sintering (CSS), and spark plasma sintering (SPS) methods. Their microstructure and dielectric properties were studied comparatively. The ceramics via SPS and SSS exhibit pure structure, while a secondary phase exists in the ce-ramics via CSS. Compared to SSS, CSS and SPS can obviously reduce the processing temperatures for obtaining dense ceramics. The ceramics via SPS have the smallest mean grain size of 80 nm, while those via CSS and SSS exhibit increased grain sizes. The dielectric measurement demonstrates that temperature stability in dielectric constant at high temperatures is affected by sintering methods. The SPS sample shows the poorest temperature stability of permittivity. The ceramics post-annealed at 1050 degrees C via CSS exhibits the widest temperature range between 49 degrees C and 412 degrees C for temperature coefficient of capacitance <=+/- 15%, which can be expected to be used in the field of high-temperature capacitors.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Piezoelectric, ferroelectric and dielectric properties of Nd2O3-doped (Bi0.5Na0.5)0.94Ba0.06TiO3 lead-free ceramics
    Fu, Peng
    Xu, Zhijun
    Chu, Ruiqing
    Li, Wei
    Zang, Guozhong
    Hao, Jigong
    MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2010, 167 (03): : 161 - 166
  • [42] Electrical and photoluminescence properties of (Bi0.5-x/0.94Erx/0.94Na0.5)0.94Ba0.06TiO3 lead-free ceramics
    Liu, Li-na
    Chen, Xiao-ming
    Jing, Rui-yi
    Lian, Han-li
    Wu, Wen-wen
    Mou, Yan-ping
    Liu, Peng
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (05) : 5233 - 5239
  • [43] Electrical and photoluminescence properties of (Bi0.5−x/0.94Erx/0.94Na0.5)0.94Ba0.06TiO3 lead-free ceramics
    Li-na Liu
    Xiao-ming Chen
    Rui-yi Jing
    Han-li Lian
    Wen-wen Wu
    Yan-ping Mou
    Peng Liu
    Journal of Materials Science: Materials in Electronics, 2019, 30 : 5233 - 5239
  • [44] Effect of HfO2 content on the microstructure and piezoelectric properties of (Bi0.5Na0.5)0.94Ba0.06TiO3 lead-free ceramics
    Chen, Tao
    Wang, Hongli
    Zhang, Ting
    Wang, Guangchang
    Zhou, Jifang
    Zhang, Jianwei
    Liu, Yuhong
    CERAMICS INTERNATIONAL, 2014, 40 (02) : 2959 - 2963
  • [45] Enhancement of pyroelectric properties of lead-free 0.94Na0.5Bi0.5TiO3-0.06BaTiO3 ceramics by La doping
    Balakt, A. M.
    Shaw, C. P.
    Zhang, Qi
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (04) : 1459 - 1466
  • [46] Effects of Li on electrical properties of (K0.47Na0.53)1-xLixNb0.94Sb0.06O3 lead-free ceramics
    Zhang, Cheng
    Xiao, Dingquan
    Wu, Wenjuan
    Liang, Wenfeng
    Zhu, Jianguo
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2011, 208 (09): : 2211 - 2214
  • [47] Effect of substitution of (NiNb)4+ into B-sites on the phase formation, microstructure and electrical properties of Bi0.47Na0.47Ba0.06TiO3 ceramics
    Luangpangai, Anupong
    Bhupaijit, Pamornnarumol
    Charoenthai, Nipaphat
    Vittayakorn, Naratip
    Thountom, Sarawut
    Bongkarn, Theerachai
    FERROELECTRICS, 2022, 601 (01) : 96 - 107
  • [48] Dielectric and ferroelectric properties of (Bi0.5Na0.5)0.94Ba0.06Ti1-xAlxO3-δ lead-free ferroelectric ceramics
    Lian, Han-li
    Cheng, Rui-xue
    Qiu, Yan-zi
    Shi, Jin-yan
    Chen, Xiao-ming
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (10) : 7927 - 7936
  • [49] Effect of Eu doping on structure and electrical properties of lead-free (Bi0.5Na0.5)0.94Ba0.06TiO3 ceramics
    Ma, Xiao
    Yin, Jiatian
    Zhou, Qilai
    Xue, Lihong
    Yan, Youwei
    CERAMICS INTERNATIONAL, 2014, 40 (05) : 7007 - 7013
  • [50] Dielectric and ferroelectric properties of (Bi0.5Na0.5)0.94-δBa0.06Ti1-xNbxO3 lead-free ceramics
    Lian, Han-li
    Shi, Jin-yan
    Qiu, Yan-zi
    Chen, Xiao-ming
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (23) : 21467 - 21477