Damping properties of Sn58Bi and Sn3.0Ag0.5Cu solders with different thicknesses and preparation directions

被引:2
|
作者
Li, Wangyun [1 ]
Liu, Linyiang [1 ]
Li, Xingmin [1 ]
机构
[1] Guilin Univ Elect Technol, Sch Mech & Elect Engn, Guilin, Peoples R China
基金
中国国家自然科学基金;
关键词
Sn58Bi; Sn3; 0Ag0; 5Cu; Solder thickness; Preparation direction; Damping; MECHANICAL-PROPERTIES; TEMPERATURE; DISLOCATION; CREEP;
D O I
10.1108/SSMT-05-2022-0043
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Purpose This study aims to experimentally assess the effect of thickness and preparation direction on the damping properties of Sn58Bi and Sn3.0Ag0.5Cu solders. Design/methodology/approach Sn58Bi and Sn3.0Ag0.5Cu solder strips with different thicknesses were prepared from the bulk in longitudinal and horizontal directions, and the ratio of loss modulus and storage modulus of the samples was measured by the dynamic mechanical analysis method as the index of damping properties. Findings Sn58Bi and Sn3.0Ag0.5Cu solders exhibited viscoelastic relaxation, and their damping properties decreased with decreasing thickness. The damping properties of both solders had no obvious difference in longitudinal and horizontal directions. Sn58Bi has a more obvious high-temperature damping background than Sn3.0Ag0.5Cu solder. In addition, compared with Sn58Bi solder, Sn3.0Ag0.5Cu solder had an obvious internal friction peak, which moved toward high temperature with increasing frequency. The activation energies of Sn58Bi solder with a thickness of 0.5 mm at the longitudinal and horizontal directions were 0.84 and 0.67 eV, respectively, which were 0.39 and 0.53 eV, respectively, for the Sn3.0Ag0.5Cu solder. Originality/value The damping properties of Sn58Bi and Sn3.0Ag0.5Cu solder decreased with decreasing thickness, while their damping properties changed insignificantly when they were prepared from different directions. The internal friction peak of Sn3.0Ag0.5Cu solder moved to higher temperatures with increasing frequency.
引用
收藏
页码:86 / 94
页数:9
相关论文
共 50 条
  • [31] Aging resistance and mechanical properties of Sn3.0Ag0.5Cu solder bump joints with different bump shapes
    Chen, Ping
    Zhao, Xiu-Chen
    Liu, Ying
    Li, Hong
    Wang, Yong
    RARE METALS, 2021, 40 (01) : 225 - 230
  • [32] The Evolution of IMCs in Single Crystal Sn3.0Ag0.5Cu and Sn3.0Ag3.0Bi3.0In BGA Solder Joints with Au/Ni/Cu Pads Under Current Stressing
    Tian, Yu
    Wang, Yishu
    Guo, Fu
    Ma, Limin
    Han, Jing
    JOURNAL OF ELECTRONIC MATERIALS, 2019, 48 (05) : 2770 - 2779
  • [33] The Evolution of IMCs in Single Crystal Sn3.0Ag0.5Cu and Sn3.0Ag3.0Bi3.0In BGA Solder Joints with Au/Ni/Cu Pads Under Current Stressing
    Yu Tian
    Yishu Wang
    Fu Guo
    Limin Ma
    Jing Han
    Journal of Electronic Materials, 2019, 48 : 2770 - 2779
  • [34] Effect of deep cryogenic treatment on mechanical properties and microstructure of Sn3.0Ag0.5Cu solder
    Yao Yao
    Xiao Li
    Xu He
    Journal of Materials Science: Materials in Electronics, 2018, 29 : 4517 - 4525
  • [35] Microstructure growth and tensile strength of Cu/Sn3.0Ag0.5Cu/Cu solder joints
    Yang, Linmei
    Quan, Shanyu
    Shi, Guimei
    MATERIALS RESEARCH EXPRESS, 2019, 6 (01)
  • [36] Improvement on interfacial structure and properties of Sn–58Bi/Cu joint using Sn–3.0Ag–0.5Cu solder as barrier
    Fengjiang Wang
    Dongyang Li
    Zhijie Zhang
    Mingfang Wu
    Chao Yan
    Journal of Materials Science: Materials in Electronics, 2017, 28 : 19051 - 19060
  • [37] Effect of deep cryogenic treatment on mechanical properties and microstructure of Sn3.0Ag0.5Cu solder
    Yao, Yao
    Li, Xiao
    He, Xu
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2018, 29 (06) : 4517 - 4525
  • [38] Shear Fracture Behavior of Sn3.0Ag0.5Cu Solder joints on Cu Pads with Different Solder Volumes
    Tian, Yanhong
    Wang, Chunqing
    Yang, Shihua
    Lin, Penrong
    Liang, Le
    2008 INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING, VOLS 1 AND 2, 2008, : 684 - +
  • [39] Sn-3.0Ag-0.5Cu nanocomposite solders reinforced by graphene nanosheets
    Huang, Yilong
    Xiu, Ziyang
    Wu, Gaohui
    Tian, Yanhong
    He, Peng
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2016, 27 (07) : 6809 - 6815
  • [40] Sn3.0Ag0.5Cu倒装焊点中的电迁移
    陆裕东
    何小琦
    恩云飞
    王歆
    庄志强
    物理学报, 2009, 58 (03) : 1942 - 1947