Dynamic analysis of liquid permeability in the dripping zone of blast furnace and reaction behavior at the slag-coke interface

被引:1
|
作者
Deng, Yong [1 ,2 ]
Liu, Ran [1 ,2 ]
Li, Tao [1 ,2 ]
Gao, Yanjia [1 ,2 ]
Yao, Kuo [1 ,2 ]
Wang, Laixin [3 ]
机构
[1] North China Univ Sci & Technol, Inst Met Engn & Technol, Tangshan 063210, Peoples R China
[2] North China Univ Sci & Technol, Coll Met & Energy, Minist Educ, Key Lab Modern Met Technol, Tangshan 063210, Peoples R China
[3] MCC Huatian Engn & Technol Co Ltd, Nanjing 210019, Peoples R China
关键词
blast furnace; dripping zone; liquid permeability; dynamic analysis; reaction behavior;
D O I
10.1051/metal/2024019
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The dripping zone connects the cohesive zone and the hearth, it is one of the key areas of the blast furnace (BF). This study aims to explore the mechanism of the dripping process in BF. The dripping experiments under different conditions were carried out. Dynamics of liquid permeability in the dripping zone was analyzed, the reaction behavior at the slag-coke interface was investigated, and the consumption of coke in the dripping zone was clarified. The results show that: The retention ratio increases with the increase of Al2O3 content. The increase in retention ratio is related to the viscosity of slag. Once the Al2O3 content in slag increases, Si4+ coordination polymer ions in tetrahedra will be replaced by Al3+ cations, forming a tetrahedral structure of [AlO4]5- tetrahedron. The retention ratio decreases with the increase of FeO content. The dissociation of free oxygen ions (O)2- from FeO increases the concentration of free oxygen ions (O)2- in slag, this reduces the viscosity of slag. The presence of FeO can compensate for the increase in retention ratio caused by Al2O3. The quantitative relationship between retention ratio and Al2O3 content and FeO content in slag is obtained. The reduction reaction of FeO occurs at the slag-coke interface, the molten iron takes on the shape of small iron beads, which is the result of multiple small droplets gathering. The reduction of TiO2 is carried out by a series of reactions, the Ti exhibits a granular embedding state in molten iron, its color is darker than that of molten iron and its particles have distinct edges and corners. In the slag-coke area of retained sample, the reduction reaction occurs between coke and oxides in slag. The carbon will be consumed, resulting in a decrease in particle size. In the iron-coke area of retained sample, the carburization reaction occurs in large quantities due to the carbon content of molten iron in hearth is undersaturated, coke is further consumed.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Numerical analysis on behavior of unburned char and fine coke in blast furnace
    Nogami, H
    Pintowantoro, S
    Yagi, JI
    ISIJ INTERNATIONAL, 2005, 45 (10) : 1489 - 1495
  • [32] Effect of Coke Reaction Index on Reduction and Permeability of Ore Layer in Blast Furnace Lumpy Zone Under Non-Isothermal Condition
    ZHAO Hong-bo
    BAI Yong-qiang
    CHENG Shu-sen
    JournalofIronandSteelResearch(International), 2013, 20 (04) : 6 - 10
  • [33] Effect of Coke Reaction Index on Reduction and Permeability of Ore Layer in Blast Furnace Lumpy Zone Under Non-Isothermal Condition
    Zhao Hong-bo
    Bai Yong-qiang
    Cheng Shu-sen
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2013, 20 (04) : 6 - 10
  • [34] Effect of Coke Reaction Index on Reduction and Permeability of Ore Layer in Blast Furnace Lumpy Zone Under Non-Isothermal Condition
    Hong-bo Zhao
    Yong-qiang Bai
    Shu-sen Cheng
    Journal of Iron and Steel Research International, 2013, 20 : 6 - 10
  • [35] Corrosion Behavior of Ceramic Cup of Blast Furnace Hearth by Liquid Iron and Slag
    Li, Yanglong
    Cheng, Shusen
    Wang, Zhifeng
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2016, 35 (09) : 941 - 948
  • [36] Gas Permeability Improvement Mechanism at the Blast Furnace Cohesive Zone by Mixed Coke Charging in Ore Layer and Effect of Coke Mixing for Different Cohesive Zone Condition on Gas Permeability
    Yakeya, Masahiro
    Kasai, Akito
    Tadai, Rikizo
    Nozawa, Kentaro
    ISIJ INTERNATIONAL, 2020, 60 (07) : 1438 - 1444
  • [37] Influence of Gasification Reaction of Coke on Sliding and Dynamic Contact Angles of Droplets in a Blast Furnace
    Ogyu, Shinsuke
    Zheng, Lichun
    Gao, Xu
    Ueda, Shigeru
    Sukenaga, Sohei
    Kitamura, Shin-ya
    ISIJ INTERNATIONAL, 2020, 60 (07) : 1401 - 1408
  • [38] Deadman Behavior and Slag-Iron-Coke Interaction of Low Carbon and Safety Blast Furnace: A Review
    Zong, Yanbing
    Guo, Ziyu
    Zhang, Jianliang
    Liu, Yanxiang
    Meng, Sai
    Ning, Xiaojun
    Jiao, Kexin
    STEEL RESEARCH INTERNATIONAL, 2024, 95 (10)
  • [39] INFLUENCE OF LOW PERMEABILITY ZONE IN BLAST-FURNACE HEARTH ON TEMPERATURE DISTRIBUTION IN FURNACE BOTTOM AND ON IRON AND SLAG TAPPING INDEXES
    SAWA, Y
    TAKEDA, K
    TAGUCHI, S
    MATSUMOTO, T
    WATANABE, Y
    KAMANO, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1992, 78 (07): : 1171 - 1178
  • [40] Interface wetting behavior between iron and coke during the carbon dissolution process in a blast furnace
    Zhan W.-L.
    Zhu H.-B.
    He Z.-J.
    Sun C.
    Yu Y.-C.
    Pang Q.-H.
    Zhang J.-H.
    He, Zhi-Jun (hzhj2002@126.com), 2020, Science Press (42): : 595 - 601