Microstructures and bio-corrosion resistances of as-extruded Mg-Ca alloys with ultra-fine grain size

被引:9
|
作者
Xie, Zi-Ren [1 ]
Zhang, Cheng [1 ]
Pan, Hu-Cheng [1 ]
Wang, Yu-Xin [1 ]
Ren, Yu-Ping [1 ]
Qin, Gao-Wu [1 ]
机构
[1] Northeastern Univ, Key Lab Anisotropy & Texture Mat, Minist Educ, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
Magnesium alloys; Corrosion; Defects; Grain size; MAGNESIUM ALLOY; MECHANICAL-PROPERTIES; BEHAVIOR; SR; BIOCORROSION; DISSOLUTION; REFINEMENT; ADDITIONS; AZ31; ZR;
D O I
10.1007/s12598-017-0945-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Electrochemical and immersion tests were conducted to characterize the bio-corrosion resistance of as-extruded Mg-Ca binary alloys with submicron grain size. The microstructures were further characterized by optical microscopy (OM), scanning electronic microscopy and transmission electron microscope (TEM). The grain size was estimated from OM and TEM images. Three samples and at least 20 images were used to evaluate the average grain size. Macro-textures of the as-extruded samples were measured via X-ray diffraction. The Mg-2Ca alloy extruded at 300 degrees C (2Ca-300) exhibits the lowest current density of 1.683 mA center dot cm(-2) and corrosion rate of 22.14 g center dot m(-2)center dot day(-1) in simulated body fluid, which is comparable with that of pure Mg. The Ca addition can reduce grain size of as-extruded Mg alloy and decrease the corrosion rate. The formed Mg2Ca phases would accelerate the local galvanic corrosion and protect the alpha-Mg matrix simultaneously due to the lower electrode potential. The lower defect density, finer grain size and weaker basal texture intensity contribute to the excellent bi-corrosion resistance of the 2Ca-300 alloy.
引用
收藏
页码:680 / 687
页数:8
相关论文
共 45 条
  • [41] Thermal stability, grain growth kinetics, mechanical properties, and bio-corrosion resistance of pure Mg, ZK30, and ZEK300 alloys: A comparative study
    Savaedi, Zeinab
    Mirzadeh, Hamed
    Aghdam, Rouhollah Mehdinavaz
    Mahmudi, Reza
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [42] The formation mechanism and bio-corrosion properties of Ag/HA composite conversion coating on the extruded Mg-2Zn-1Mn-0.5Ca alloy for bone implant application
    Hu, Guangwu
    Zeng, Liangcai
    Du, Hui
    Fu, Xiande
    Jin, Xixi
    Deng, Meng
    Zhao, Yujin
    Liu, Xinwang
    SURFACE & COATINGS TECHNOLOGY, 2017, 325 : 127 - 135
  • [43] Effect of a duplex grain size on the tensile ductility of an ultra-fine grained Al-Mg alloy, AA5754, produced by asymmetric rolling and annealing
    Jin, H
    Lloyd, DJ
    SCRIPTA MATERIALIA, 2004, 50 (10) : 1319 - 1323
  • [44] The role of Al2Ca and Al2(Sm,Ca,La) particles in the microstructures and electrochemical discharge performance of as-extruded Mg-3wt.%Al-1wt.%Zn-based alloys for primary Mg-air batteries
    Liu, Xuan
    Guo, Zhichao
    Xue, Jilai
    Zhang, Pengju
    INTERNATIONAL JOURNAL OF ENERGY RESEARCH, 2019, 43 (09) : 4569 - 4579
  • [45] Effect of grain size on the corrosion behavior of fully recrystallized ultra-fine grained 316L stainless steel fabricated by high-energy ball milling and hot isostatic pressing sintering
    Tian, Lixi
    Zheng, Ruixiao
    Yuan, Cuiqi
    Yang, Guang
    Shi, Chao
    Zhang, Bangyan
    Zhang, Zhe
    MATERIALS CHARACTERIZATION, 2021, 174