Microstructure analysis of microwave and conventionally fired porcelain

被引:1
|
作者
Santos, Tiago A. C. [1 ,2 ,3 ,4 ]
Costa, Vitor A. F. [4 ]
Costa, Luis M. C. M. [1 ,2 ]
机构
[1] Univ Aveiro, I3N, P-3810193 Aveiro, Portugal
[2] Univ Aveiro, Dept Phys, P-3810193 Aveiro, Portugal
[3] Porcelanas Costa Verde SA, Vagos, Portugal
[4] Univ Aveiro, Ctr Mech Technol & Automat, Dept Mech Engn, Aveiro, Portugal
关键词
closed porosity; lower firing temperature; microwave fast-fired; porcelain; FIRING TEMPERATURE; MECHANICAL-PROPERTIES; BENDING STRENGTH; FUNDAMENTALS; BENEFICIATION; SUSCEPTOR; EVOLUTION; KAOLIN;
D O I
10.1002/fam.3103
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The evolution of porcelain closed porosity during microwave and electric fast-firing is investigated and compared with that of conventionally gas-fired porcelain (taken as reference). Samples were fired in less than 70 min and are considered to be fast-fired as their processing takes less than one-half of the conventional heating time (similar to 210 min). The closed porosity relationship with the porcelain functional properties explains some of the observed differences between microwave and electrically fired porcelain. Electrically-fired samples at 1100 degrees C present a microstructure like that of the biscuit reference, fired at similar to 1000 degrees C in 460 min, whereas microwave-fired samples already show some vitrification at this temperature. The samples microwave fired between 1300 degrees C and 1380 degrees C, in 70 min, present a microstructure similar to that of reference samples fired at 1380 degrees C in 210 min. Electric fast-firing requires similar to 80 degrees C higher firing temperatures (between 1350 degrees C and 1380 degrees C than microwave fast-firing to reach similar features. Both electrically and microwave fast-fired porcelain show similar microstructure evolutions and densifications (similar to 95% of the real density, equal to 2.57 g.cm(-3)), the microwave-fired samples presenting a more developed microstructure state for the same firing temperature.
引用
收藏
页码:375 / 385
页数:11
相关论文
共 50 条
  • [21] STRUCTURE AND PROPERTIES OF RAPIDLY FIRED SANITARY PORCELAIN.
    Kunavin, M.M.
    Grum-Grzhimailo, O.S.
    Glass and Ceramics (English translation of Steklo i Keramika), 1983, 40 (1-2): : 91 - 92
  • [22] Low-fired porcelain with diopside and marshalite additions
    Vereshchagin, V. I.
    Mogilevskaya, N. V.
    Gorbachev, D. V.
    GLASS AND CERAMICS, 2013, 69 (11-12) : 401 - 404
  • [23] Composition, Structure, and Properties of Low-Fired Porcelain
    A. M. Eminov
    Z. R. Kadyrova
    Af. A. Eminov
    Yu. K. Zhumanov
    I. R. Boizhanov
    Glass and Ceramics, 2022, 79 : 135 - 138
  • [24] Composition, Structure, and Properties of Low-Fired Porcelain
    Eminov, A. M.
    Kadyrova, Z. R.
    Eminov, Af A.
    Zhumanov, Yu K.
    Boizhanov, I. R.
    GLASS AND CERAMICS, 2022, 79 (3-4) : 135 - 138
  • [25] Low-Fired Electrotechnical Porcelain with Diopside Additives
    V. I. Vereshchagin
    D. V. Gorbachev
    N. V. Mogilevskaya
    Glass and Ceramics, 2021, 78 : 18 - 22
  • [26] Porcelain tile microstructure:: implications for polishability
    Hutchings, IM
    Xu, Y
    Sánchez, E
    Ibáñez, MJ
    Quereda, MF
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2006, 26 (06) : 1035 - 1042
  • [27] MICROSTRUCTURE DEVELOPMENT IN A VITRIFIED ANORTHITE PORCELAIN
    SLETSON, LC
    REED, JS
    AMERICAN CERAMIC SOCIETY BULLETIN, 1988, 67 (08): : 1403 - 1408
  • [29] Improvement of process of grinding fired porcelain ware on semiautomatic devices
    TUMANOV NS
    Glass and Ceramics (English translation of Steklo i Keramika), 1970, 27 (1-2): : 57 - 59
  • [30] The characterisation of paper composite porcelain in a fired state by XRD and SEM
    Jeoung-Ah, K
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (15-16) : 3823 - 3831