Microstructure analysis of microwave and conventionally fired porcelain

被引:1
|
作者
Santos, Tiago A. C. [1 ,2 ,3 ,4 ]
Costa, Vitor A. F. [4 ]
Costa, Luis M. C. M. [1 ,2 ]
机构
[1] Univ Aveiro, I3N, P-3810193 Aveiro, Portugal
[2] Univ Aveiro, Dept Phys, P-3810193 Aveiro, Portugal
[3] Porcelanas Costa Verde SA, Vagos, Portugal
[4] Univ Aveiro, Ctr Mech Technol & Automat, Dept Mech Engn, Aveiro, Portugal
关键词
closed porosity; lower firing temperature; microwave fast-fired; porcelain; FIRING TEMPERATURE; MECHANICAL-PROPERTIES; BENDING STRENGTH; FUNDAMENTALS; BENEFICIATION; SUSCEPTOR; EVOLUTION; KAOLIN;
D O I
10.1002/fam.3103
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The evolution of porcelain closed porosity during microwave and electric fast-firing is investigated and compared with that of conventionally gas-fired porcelain (taken as reference). Samples were fired in less than 70 min and are considered to be fast-fired as their processing takes less than one-half of the conventional heating time (similar to 210 min). The closed porosity relationship with the porcelain functional properties explains some of the observed differences between microwave and electrically fired porcelain. Electrically-fired samples at 1100 degrees C present a microstructure like that of the biscuit reference, fired at similar to 1000 degrees C in 460 min, whereas microwave-fired samples already show some vitrification at this temperature. The samples microwave fired between 1300 degrees C and 1380 degrees C, in 70 min, present a microstructure similar to that of reference samples fired at 1380 degrees C in 210 min. Electric fast-firing requires similar to 80 degrees C higher firing temperatures (between 1350 degrees C and 1380 degrees C than microwave fast-firing to reach similar features. Both electrically and microwave fast-fired porcelain show similar microstructure evolutions and densifications (similar to 95% of the real density, equal to 2.57 g.cm(-3)), the microwave-fired samples presenting a more developed microstructure state for the same firing temperature.
引用
收藏
页码:375 / 385
页数:11
相关论文
共 50 条
  • [1] Impact of microwave processing on porcelain microstructure
    Lerdprom, Wirat
    Zapata-Solvas, Eugenio
    Jayaseelan, Doni D.
    Borrell, Amparo
    Salvador, Maria D.
    Lee, William E.
    CERAMICS INTERNATIONAL, 2017, 43 (16) : 13765 - 13771
  • [2] RECYCLING FIRED PORCELAIN
    SHASHIDHAR, N
    REED, JS
    AMERICAN CERAMIC SOCIETY BULLETIN, 1990, 69 (05): : 834 - 841
  • [3] Fired porcelain microstructures revisited
    Iqbal, Y
    Lee, WE
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (12) : 3584 - 3590
  • [4] PORCELAIN MICROSTRUCTURE
    HAFNER, A
    STUDII SI CERCETARI DE FIZICA, 1969, 21 (04): : 467 - +
  • [5] Chromatic behavior of porcelain fired on titanium
    Lakatos, Sorin
    Lakatos, Carmen
    Rominu, Mihai
    Florita, Zeno
    QUINTESSENCE INTERNATIONAL, 2007, 38 (07): : E368 - E373
  • [6] EVALUATION OF SOME PROPERTIES OF AN OPAQUE PORCELAIN FIRED SIMULTANEOUSLY WITH THE BODY PORCELAIN
    OBRIEN, WJ
    BOENKE, KM
    GROH, CL
    JOURNAL OF PROSTHETIC DENTISTRY, 1994, 72 (04): : 414 - 419
  • [7] Traditional and glass powder porcelain:: Technical and microstructure analysis
    Bragança, SR
    Bergmann, CP
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (08) : 2383 - 2388
  • [8] Microwave versus conventional porcelain firing: Colour analysis
    Santos, T.
    Hennetier, L.
    Costa, V. A. F.
    Costa, L. C.
    MATERIALS CHEMISTRY AND PHYSICS, 2022, 275
  • [9] STRUCTURE AND PROPERTIES OF RAPIDLY FIRED SANITARY PORCELAIN
    KUNAVIN, MM
    GRUMGRZHIMAILO, OS
    GLASS AND CERAMICS, 1983, 40 (1-2) : 91 - 92
  • [10] Effect of titania on fired characteristics of triaxial porcelain
    Bhattacharyya, S
    Das, SK
    Mitra, NK
    BULLETIN OF MATERIALS SCIENCE, 2005, 28 (05) : 445 - 452