Comparison of the Translucency Parameters and Bond Strength of 5Y-ZP Zirconia, 3-YTZP Zirconia, and Lithium Disilicate

被引:0
|
作者
Adak, I. Ozkan [1 ]
Aguloglu, S. [1 ]
Adak, B. M. [2 ]
Sari, I [1 ,3 ]
机构
[1] Izmir Katip Celebi Univ, Dept Prosthet Dent, Izmir, Turkiye
[2] Izmir Katip Celebi Univ, Dept Oral & Maxillofacial Surg, Izmir, Turkiye
[3] Katip Celebi Univ, Atasehir Mahallesi Nazim Hikmet, Ran Bulvari 60-13, TR-35620 Izmir, Turkiye
关键词
Lithium disilicate; micro-shear bond strength; zirconia; LUTING CEMENTS; TRANSMISSION; ADHESIVES; CERAMICS;
D O I
10.4103/njcp.njcp_91_23
中图分类号
R5 [内科学];
学科分类号
1002 ; 100201 ;
摘要
Background: E-max is a more aesthetic material than traditional zirconia. In addition, the bond strength of traditional zirconia with adhesive cements is lower. There are not enough studies on how the aesthetic values and bond strength of 5-YZP, the new generation zirconia, compare to e-max and traditional zirconia. Can 5-YZP be an alternative to e-max in terms of aesthetics and bond strength? Aim: The aim of the study is to compare the translucency property and bonding ability of 5y-zp zirconias with previous generation zirconias and lithium disilicate. Materials and Methods: Two types of zirconia Katana UT and Katana HT for measuring translucency values; and using a type of lithium disilicate IPS e.max CAD LT, three groups were formed (n = 10). Translucency specimens were fabricated (n = 10). Their L*a*b* values were measured against a black-and-white background with a spectrophotometer, and DE00 was calculated. To perform micro-shear tests, a cylinder design was made from zirconia and IPS e.max CAD blocks (n = 20). After the samples were aged by thermal cycle, the micro-shear test was applied to specimens cemented to teeth extracted with two different adhesive cement systems. Results: According to the results of one-way analysis of variance, a statistically significant difference was found between the translucency parameter (TP) values of the groups. According to Tukey's honestly significant difference (HSD) multiple comparisons, the values of the three groups are statistically different from each other. Although IPS e.max CAD group has the highest TP values, the Katana HT group has the lowest values. Conclusion: 5Y-PZ has a TP intermediate to those of 3Y-TZP and lithium disilicate. Long-term bond strength of 3Y-TZP and 5Y-ZP were similar to those of lithium disilicate. To be an alternative to glass ceramics in the anterior region, translucency and bond strength values need to be improved.
引用
收藏
页码:1491 / 1497
页数:7
相关论文
共 33 条
  • [21] Does the bond strength of highly translucent zirconia show a different dependence on the airborne-particle abrasion parameters in comparison to conventional zirconia?
    Zhao, Peng
    Yu, Ping
    Xiong, Yuhuan
    Yue, Li
    Arola, Dwayne
    Gao, Shanshan
    JOURNAL OF PROSTHODONTIC RESEARCH, 2020, 64 (01) : 60 - 70
  • [22] An in vitro comparison of the marginal and internal adaptation of ultrathin occlusal veneers made of 3D-printed zirconia, milled zirconia, and heat-pressed lithium disilicate
    Ioannidis, Alexis
    Park, Ji-Man
    Huesler, Juerg
    Bomze, Daniel
    Muehlemann, Sven
    Oezcan, Mutlu
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 128 (04): : 709 - 715
  • [23] Fatigue behavior and reliability of pressed lithium disilicate ceramics compared to 5Y-TZP zirconia under different loading protocols
    Buser, Ramona
    Dönmez, Mustafa Borga
    Hoffmann, Moritz
    Hampe, Rüdiger
    Stawarczyk, Bogna
    Dental Materials, 2025, 41 (02) : 134 - 140
  • [24] Comparative evaluation of shear bond strength of newer resin cement (RelyX ultimate and RelyX U200) to lithium disilicate and zirconia ceramics as influenced by thermocycling
    Kansal, Rinki
    Rani, Sapna
    Kumar, Manoj
    Kumar, Shalabh
    Issar, Gaurav
    CONTEMPORARY CLINICAL DENTISTRY, 2018, 9 (04) : 601 - 606
  • [25] Comparison of the Effect of Surface Conditioning Methods on the Bond Strength of Different Zirconia Reinforced Lithium Silicate and Hybrid Ceramics to Resin Cement
    Sevmez, Hatice
    Yilmaz, Handan
    CLINICAL AND EXPERIMENTAL HEALTH SCIENCES, 2021, 11 (03): : 554 - 563
  • [26] Impact of liner treatment on the translucency of CAD/CAM multi-colored lithium disilicate and multi-layered zirconia implant-supported crowns, and evaluation of fracture strength of ceramic crowns
    Ji-Hyun Kim
    Seon-Mi Byeon
    Tae-Sung Bae
    Yong-Seok Jang
    Min-Ho Lee
    Seung-Geun Ahn
    Odontology, 2025, 113 (2) : 645 - 654
  • [27] Effect of air abrasion, acid etching, and aging on the shear bond strength with resin cement to 3Y-TZP zirconia
    Seo, Song-Hee
    Kim, Jong-Eun
    Nam, Na-Eun
    Moon, Hong-Seok
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 134
  • [28] Effect of air abrasion, acid etching, and aging on the shear bond strength with resin cement to 3Y-TZP zirconia
    Seo, Song-Hee
    Kim, Jong-Eun
    Nam, Na-Eun
    Moon, Hong-Seok
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 134
  • [29] Effect of air abrasion, acid etching, and aging on the shear bond strength with resin cement to 3Y-TZP zirconia
    Seo, Song-Hee
    Kim, Jong-Eun
    Nam, Na-Eun
    Moon, Hong-Seok
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 134
  • [30] Impact of high-speed sintering on translucency, phase content, grain sizes, and flexural strength of 3Y-TZP and 4Y-TZP zirconia materials
    Jansen, Jan Ulrich
    Luemkemann, Nina
    Letz, Inge
    Pfefferle, Regina
    Sener, Beatrice
    Stawarczyk, Bogna
    JOURNAL OF PROSTHETIC DENTISTRY, 2019, 122 (04): : 396 - 403