Thermal cycle test performances of environmental barrier coatings of HfO2-SiO2/Yb2Si2O7 in the steam environment at 1475 °C

被引:13
|
作者
Zhang, Zhenya [1 ,3 ]
Park, Youngjin [1 ]
Park, Hunkwan [1 ]
Kang, Yongjin [1 ]
Xue, Zhaolu [3 ]
Zhang, Shihong [3 ]
Byon, Eungsun [1 ]
Koo, Bon Heun [2 ]
机构
[1] Korea Inst Mat Sci, Dept Extreme Environm Coatings, Chang Won 51508, South Korea
[2] Changwon Natl Univ, Dept Mat Convergence & Syst Engn, Chang Won 51140, Gyeongnam, South Korea
[3] Anhui Univ Technol, Res Ctr Modern Surface & Interface Engn, Maanshan 243002, Peoples R China
基金
新加坡国家研究基金会;
关键词
Environmental barrier coatings; Thermally grown oxide; Failure; Separate; HfO2-SiO2; Yb2Si2O7; CORROSION BEHAVIOR; OXIDATION BEHAVIOR; SILICON-CARBIDE; YB2SI2O7; DEGRADATION; COMPOSITES; KINETICS; HFO2;
D O I
10.1016/j.jeurceramsoc.2023.04.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The novel bi-layer environmental barrier coatings (EBCs) with HfO2-SiO2/Yb2Si2O7 structure (70HfO2-30SiO2/ Yb2Si2O7: 70HS/YbDS, 50HfO2-50SiO2/Yb2Si2O7: 50HS/YbDS, molar ratios) was tested in 90%H2O-10%O2 conditions between room temperature and 1475 degrees C in an Al2O3 tube furnace, then its performance was evaluated. The YbDS layer was contaminated by alumina impurities under steam conditions. After 22 cycles, the 70HS/YbDS completely separated from the SiC substrate, while the 50HS/YbDS and SiC did not separate, even though cracks formed at the 50HS/SiC interface and the TGO layer. Furthermore, the thermally grown oxide (TGO) layer formed at the HfO2-SiO2/SiC interface. Formation and growth of the TGO led to the formation and propagation of cracks at the HfO2-SiO2/TGO interface and TGO interior, which was the culprit leading to the failure of EBCs. These results demonstrated that the 50HS/YbDS EBCs have the potential to protect SiC in steam conditions at 1475 degrees C.
引用
收藏
页码:5004 / 5013
页数:10
相关论文
共 50 条
  • [41] Crystal growth behavior and sintering-resistance property of nano-sized β-Yb2Si2O7 for environmental barrier coatings
    Wang, Chunjie
    Wang, Yue
    CERAMICS INTERNATIONAL, 2020, 46 (11) : 19514 - 19518
  • [42] Microstructure and Resistance to Molten Salt Corrosion of Si-Yb2O3/Yb2Si2O7/Yb2SiO5 EBC
    Wang D.-W.
    Li Q.-L.
    Zhang L.
    Li S.-Q.
    Yang W.-H.
    Surface Technology, 2023, 52 (05): : 131 - 139and162
  • [43] High-Temperature thermochemical interactions of molten silicates with Yb2Si2O7 and Y2Si2O7 environmental barrier coating materials
    Stokes, Jamesa L.
    Harder, Bryan J.
    Wiesner, Valerie L.
    Wolfe, Douglas E.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (15) : 5059 - 5067
  • [44] Corrosion behaviors and failure mechanism of plasma sprayed Yb2Si2O7/Si environmental barrier coatings exposed to CMAS+NaVO3
    Hu, Xunxun
    Chen, Yongguo
    Guo, Hongbo
    Xu, Huibin
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (03)
  • [45] Comparative study on high-temperature performance and thermal shock behavior of plasma-sprayed Yb2SiO5 and Yb2Si2O7 coatings
    Zhong, Xin
    Niu, Yaran
    Li, Hong
    Zhu, Tao
    Song, Xuemei
    Zeng, Yi
    Zheng, Xuebin
    Ding, Chuanxian
    Sun, Jinliang
    SURFACE & COATINGS TECHNOLOGY, 2018, 349 : 636 - 646
  • [46] The effect of porosity, mixed molecular/Knudsen diffusion, and a surface barrier layer on steam corrosion of Yb2Si2O7
    McCormack, Simon
    Cao, Huatang
    Martins, Joao P.
    Withers, Philip J.
    Xiao, Ping
    CORROSION SCIENCE, 2023, 219
  • [47] Failure mechanisms of (Gd0.9Yb0.1)2Zr2O7/Yb2SiO5/Si thermal/environmental barrier coatings during thermal exposure at 1300 °C/1400 °C
    Chen, Wenbo
    He, Wenting
    He, Jian
    Guo, Qian
    Li, Shan
    Guo, Hongbo
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (07) : 3297 - 3304
  • [48] Thermal shock behavior of LaMgAl11O19/Yb2Si2O7/Si thermal/environmental barrier coatings with LaMgAl11O19-LiAlSiO4 transition layer
    Lue, Kaiyue
    Dong, Shujuan
    Huang, Yan
    Mao, Chuanyong
    Jiang, Jianing
    Deng, Longhui
    Cao, Xueqiang
    SURFACE & COATINGS TECHNOLOGY, 2022, 443
  • [49] High-temperature oxidation performance of novel environmental barrier coating 50HfO2-50SiO2/YxYb(2_x)Si2O7 at 1475 °C
    Zhang, Zhenya
    Park, Youngjin
    Kim, Do Hyun
    Xue, Zhaolu
    Ji, Xiaojuan
    Park, Hunkwan
    Zhang, Shihong
    Byon, Eungsun
    Koo, Bon Heun
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (03) : 1127 - 1140
  • [50] Corrosion behavior of PS-PVD spray Yb2Si2O7 environmental barrier coatings during continuous water vapor exposure
    Wu, Jian
    Yang, Wenchao
    Zhang, Xiaofeng
    Wang, Chao
    Zhuo, Xueshi
    Zhan, Yongzhong
    Liu, Min
    Zhou, Kesong
    CORROSION SCIENCE, 2023, 210