State of Deadman in Blast Furnace Hearth and Its Internal Phase Distribution Characteristics

被引:1
|
作者
Deng, Yong [1 ,2 ]
Liu, Ran [1 ,2 ]
Wang, Dequan [3 ]
Jiao, Kexin [4 ]
Liu, Yanjun [3 ]
Guo, Ziyu [4 ]
Meng, Sai [4 ]
Song, Mingbo [4 ]
Xiao, Zhixin [5 ]
机构
[1] North China Univ Sci & Technol, Inst Met Engn & Technol, Tangshan 063210, Peoples R China
[2] North China Univ Sci & Technol, Coll Met & Energy, Minist Educ, Key Lab Modern Met Technol, Tangshan 063210, Peoples R China
[3] Delong Steel Co Ltd, Xingtai 054009, Peoples R China
[4] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[5] Baosteel Cent Res Inst Qingshan, Wuhan 430080, Peoples R China
关键词
blast furnace; deadman; sidewall erosion; phase distribution; interfacial reaction; COLD-MODEL; SIDEWALL EROSION; HOT METAL; BEHAVIOR; ACTIVATION; MECHANISM; RENEWAL; MOTION; COKE;
D O I
10.2355/isijinternational.ISIJINT-2022-363
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The state of deadman in hearth is important for the long campaign life of blast furnace (BF). In order to clarify the influence of deadman on sidewall erosion, the corresponding relationship between the shape of deadman and sidewall erosion was studied, the fundamental reason for the difference of sidewall erosion was analyzed, the influence mechanism of slag-coke interface and iron-coke interface on the coke in deadman was explored based on the phase distribution in deadman. The results show that: The shape of circumferential bulge at the root of deadman is a common feature of BFs, this feature is the main reason for the serious erosion of sidewall, and the serious erosion area of sidewall corresponds to the root position of deadman. The deadman shows a dynamic evolution law of sinking and floating under the action of force in the smelting process of BF, the depth of slag and iron level in hearth has the greatest influence on the deadman. The difference of central voidage of deadman is the fundamental reason for the difference of sidewall erosion for BFs in which the deadman is in the same floating state. Slag-coke interface and iron-coke interface commonly exist in hearth. The dissolution reaction at iron-coke interface makes carbon in coke continuously migrate into molten iron, which makes the graphitization degree of coke increase, the coke is easy to pulverize, this is the main mechanism of coke deterioration and renewal in deadman. The enrichment of harmful element K at slag-coke interface makes the coke expand and crack, the coke matrix is easier to peel off, which accelerates the deterioration process of coke.
引用
收藏
页码:828 / 834
页数:7
相关论文
共 50 条
  • [21] CHECKING STATE OF HEARTH LINING ON AN OPERATING BLAST FURNACE
    GORSKOV, VK
    MYSLIVTS.IV
    USHKOV, IA
    ZHIKLIN, NK
    STAL IN ENGLISH-USSR, 1965, (04): : 267 - &
  • [22] Numerical Estimation of Hearth Internal Geometry of an Industrial Blast Furnace
    Zhang, Chengbo
    Zhao, Chenxi
    Shao, Lei
    Saxen, Henrik
    Qu, Yingxia
    Zou, Zongshu
    STEEL RESEARCH INTERNATIONAL, 2022, 93 (02)
  • [23] Prediction of blast furnace hearth condition: part II - a transient state simulation of hearth condition during blast furnace shutdown
    Dong, X. F.
    Zulli, P.
    Biasutti, M.
    IRONMAKING & STEELMAKING, 2020, 47 (05) : 561 - 566
  • [24] Improvement of the Uniformity of Blast Distribution over the Circumference of Blast-Furnace Hearth
    Lyalyuk, V. P.
    Tarakanov, A. K.
    Kassim, D. A.
    Riznitskii, I. G.
    METALLURGIST, 2018, 62 (1-2) : 119 - 124
  • [25] TEMPERATURE DISTRIBUTION IN HEARTH OF A BLAST FURNACE WITH AIR-COOLED HEARTH BOTTOM FACE
    WARTMANN, R
    MERTES, H
    STEINECK.V
    STAHL UND EISEN, 1967, 87 (07): : 357 - &
  • [26] Modeling of the distribution of the liquid iron level in the blast furnace hearth
    Podlubny, I
    Kostial, I
    Kacenák, M
    Terpák, J
    METALURGIJA, 2001, 40 (02): : 107 - 109
  • [27] Flow induced stress distribution on wall of blast furnace hearth
    Vats, AK
    Dash, SK
    IRONMAKING & STEELMAKING, 2000, 27 (02) : 123 - 128
  • [28] Asymptotic Model of Refractory and Buildup State of the Blast Furnace Hearth
    Weiqiang Liu
    Lei Shao
    Zongshu Zou
    Henrik Saxén
    Metallurgical and Materials Transactions B, 2022, 53 : 320 - 333
  • [29] Activation of deadman state in the blast furnace using serpentine injection through tuyere
    Ichida, M
    Orimoto, T
    Sakatani, M
    Nakamura, K
    Kumaoka, H
    Ueno, H
    ISIJ INTERNATIONAL, 2004, 44 (12) : 2134 - 2143
  • [30] Asymptotic Model of Refractory and Buildup State of the Blast Furnace Hearth
    Liu, Weiqiang
    Shao, Lei
    Zou, Zongshu
    Saxen, Henrik
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2022, 53 (01): : 320 - 333