The influence of porosity and precipitates on the corrosion behavior of A356 aluminum alloy

被引:7
|
作者
Zhang, Hao [1 ,2 ]
Yu, Shuqin [1 ,2 ]
Yang, Zixuan [1 ,2 ]
Zhang, Chaoqun [1 ,2 ]
机构
[1] Ningbo Univ, Zhejiang Prov Engn Res Ctr Safety Pressure Vessel, Ningbo 315211, Peoples R China
[2] Ningbo Univ, Coll Mech Engn & Mech, Ningbo 315211, Peoples R China
基金
中国国家自然科学基金;
关键词
A356 aluminum alloy; Electrochemistry; Salt spray test; CT; SKPFM; Corrosion behavior; MECHANICAL-PROPERTIES; PITTING CORROSION; MG; NACL; GRAIN; MICROSTRUCTURE; ND;
D O I
10.1016/j.jelechem.2023.117796
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
In this article, the pore and precipitation phases of A356 aluminum alloy were regulated by adding element Cu, and the corrosion kinetic behavior was investigated by electrochemical experiments and salt spray test (SST), while the corrosion mechanism of A356 aluminum alloy was studied by scanning electron microscopy (SEM), 3D laser confocal microscopy (LSCM) and atomic force microscopy (SKPFM). The results of both electrochemical and salt spray experiments showed that the corrosion rate increased with increasing Cu content, and the average corrosion rate increased from 0.040 mm y-1 to 0.329 mm y-1 when the Cu content increased from 0 wt% to 7 wt %, and the Cu free alloy exhibited a greater charge transfer resistance. This is mainly due to the addition of Cu on the one hand to increase the number of precipitation phase, Al2Cu become the main precipitation phase, SKPFM test results show that the precipitation phase relative to the Al matrix potential difference in order: Al2Cu (350 380 mV), Si (250 - 275 mV), Mg2Si (80 - 110 mV), the increase in potential difference between the two phases to promote the corrosion of occurrence. On the other hand, CT results showed that the average diameter of pores increased from 89.95 mu m to 281.00 mu m, and the volume fraction increased from 0.05 % to 0.18 %, and the larger and more porous pores help promote corrosion. Therefore, how to control the porosity and precipitation phase is an important factor in regulating the corrosion behavior of A356 aluminum alloy.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Porosity distribution in AlSi7MgO3 (A356) aluminum alloy castings
    Chiesa, F.
    Regimbal, R.
    Fonderie-Fondeur d'Aujourd'hui, 2000, (194): : 17 - 25
  • [22] Fretting Wear Behavior of Microarc Oxidation Film on A356 Aluminum Alloy
    Sun Lu
    Li Yuandong
    Ma Ying
    Cao Chi
    Luo Xiaomei
    Qiu Jin
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (03) : 796 - 806
  • [23] Influence of Surface Finish and Porosity on the Fatigue behaviour of A356 Aluminium Casting Alloy
    Hidalgo, Raquel
    Ander Esnaola, Jon
    Larranaga, Miren
    Llavori, Inigo
    Herrero-Dorca, Nuria
    Hurtado, Inaki
    Otxoa, Edurne
    Rodriguez, Patxi
    Kortabarria, Aitor
    12TH INTERNATIONAL FATIGUE CONGRESS (FATIGUE 2018), 2018, 165
  • [24] The rheological behavior for thixocasting of semi-solid aluminum alloy (A356)
    Yang, XJ
    Jing, YH
    Liu, J
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2002, 130 : 569 - 573
  • [25] Crack propagation behavior of A356 aluminum alloy under resonant vibration
    Jiang, DS
    Lui, TS
    Chen, LH
    SCRIPTA MATERIALIA, 1997, 36 (01) : 15 - 20
  • [26] Effect of Strontium Modification on Porosity Formation in A356 Alloy
    Qian Wang
    Qitang Hao
    Wentao Yu
    International Journal of Metalcasting, 2019, 13 : 944 - 952
  • [27] An analysis on porosity formation in A356 aluminium alloy castings
    Li, KD
    Chang, E
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2002, 15 (01) : 25 - 30
  • [28] Effect of Strontium Modification on Porosity Formation in A356 Alloy
    Wang, Qian
    Hao, Qitang
    Yu, Wentao
    INTERNATIONAL JOURNAL OF METALCASTING, 2019, 13 (04) : 944 - 952
  • [29] Study on Defects of A356 Aluminum Alloy Wheel
    Zhao, Weimin
    Zhang, Liang
    Wang, Zhifeng
    Yan, Hongji
    MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 3862 - +
  • [30] Effects of hydrogen, solidification rate, and Ca on porosity formation in as-cast aluminum alloy A356
    Anyalebechi, PN
    LIGHT METALS 2003, 2003, : 971 - 981