Effect of ball mill time and wet pre-milling on the fabrication of Ti powders by recycling Ti machining chips by planetary milling

被引:15
|
作者
Cuvalci, Oguzhan [1 ]
Varol, Temel [1 ,2 ]
Akcay, Serhatcan Berk [1 ]
Guler, Onur [1 ]
canakci, Aykut [1 ]
机构
[1] Karadeniz Tech Univ, Dept Met & Mat Engn, TR-61080 Trabzon, Turkiye
[2] Karadeniz Tech Univ, Med Device Design & Prod Applicat & Res Ctr, TR-61080 Trabzon, Turkiye
关键词
Mechanical milling; Wet pre-milling; Machining chips; Titanium; Ball to powder weight ratio; MATRIX COMPOSITES; MICROSTRUCTURE; NANOCOMPOSITES; RECOVERY; SIZE; PARAMETERS; DENSITY;
D O I
10.1016/j.powtec.2023.118637
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
In this study, Cp-Ti particles were fabricated from titanium turning chips by wet-pre milling assisted mechanical milling with different ball to powder ratio and milling time. The minimum particle size fabricated with a ball to powder weight ratio of 15:1 is approximately 15 times smaller than powders produced with 5:1. TiO2 (Anatase and Rutile) peaks were found in the structure of Cp-Ti particles fabricated after 4 h of milling at a ball-to-powder ratio of 15:1. However after the milling with low ball to powder ratios (5:1 and 10:1) the oxidation was not observed in results of XRD analysis. The lowest apparent density and hardness was measured as 2.45 g/cm3 and 126 HV for 0.5 h milled powders, respectively. The maximum apparent density and hardness was measured as 3.45 g/cm3 and 325 HV for 7 h milled powders, respectively.
引用
收藏
页数:16
相关论文
共 50 条
  • [21] Aqueous Dispersions of Latex Compounding Ingredients by Wet Ball Milling: Effect of Ball Size and Milling Time on Dispersion Quality
    K. Anand
    Siby Varghese
    Thomas Kurian
    Transactions of the Indian Institute of Metals, 2017, 70 : 1593 - 1600
  • [22] THERMAL-BEHAVIOR OF CU-TI AND CU-TI-H AMORPHOUS POWDERS PREPARED BY BALL MILLING
    BARICCO, M
    BATTEZZATI, L
    SOLETTA, I
    SCHIFFINI, L
    COWLAM, N
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 134 : 1398 - 1401
  • [23] Effect of ball milling time on Ti-Al and Ni-Al powder mixtures
    Benhaddad, S
    Bhan, S
    Rahmat, A
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1997, 16 (10) : 855 - 857
  • [24] Effect of ball size and powder loading on the milling efficiency of a laboratory-scale wet ball mill
    Shin, Hyunho
    Lee, Sangwook
    Jung, Hyun Suk
    Kim, Jong-Bong
    CERAMICS INTERNATIONAL, 2013, 39 (08) : 8963 - 8968
  • [25] Synthesis of ultrafine TiC1-X and Ti(CN) powders via planetary milling
    Jung, J
    Kang, S
    POWDER METALLURGY, 2004, 47 (01) : 93 - 98
  • [26] Effect of ball milling conditions on the microstructure and the transformation behavior of Ti-Ni and Ti-Ni-Cu shape memory alloy powders
    Nam, TH
    Kang, SH
    METALS AND MATERIALS INTERNATIONAL, 2002, 8 (02): : 145 - 150
  • [27] Fabrication of commercial pure Ti by selective laser melting using hydride-dehydride titanium powders treated by ball milling
    Wei Xu
    Shiqi Xiao
    Xin Lu
    Gang Chen
    Chengcheng Liu
    Xuanhui Qu
    JournalofMaterialsScience&Technology, 2019, 35 (02) : 322 - 327
  • [28] Fabrication of commercial pure Ti by selective laser melting using hydride-dehydride titanium powders treated by ball milling
    Xu, Wei
    Xiao, Shiqi
    Lu, Xin
    Chen, Gang
    Liu, Chengcheng
    Qu, Xuanhui
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 35 (02) : 322 - 327
  • [30] Synthesis of Fe3O4 nanoparticles by wet milling iron powder in a planetary ball mill
    Chen, Ding
    Ni, Song
    Chen, Zhenhua
    CHINA PARTICUOLOGY, 2007, 5 (05): : 357 - 358