Hot deformation behavior and microstructural evolution of the Al-Cu-Li alloy: A study with processing map

被引:29
|
作者
Tang, Jiaguo [1 ,2 ]
Yi, Youping [1 ,2 ,3 ]
He, Hailin [2 ,3 ]
Huang, Shiquan [2 ,3 ]
Zhang, Jingjing [1 ,2 ]
Dong, Fei [2 ,3 ]
机构
[1] Cent South Univ, Sch Mech & Elect Engn, Changsha 410083, Peoples R China
[2] State Key Lab High Performance Complex Mfg, Changsha 410083, Peoples R China
[3] Cent South Univ, Res Inst Light Alloy, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Cu-Li alloy; Hot deformation; Processing map; Microstructure; MECHANICAL-PROPERTIES; DYNAMIC RECRYSTALLIZATION; CONSTITUTIVE EQUATION; STRAIN-RATE; FLOW; QUANTIFICATION; EXTRUSION; PROPERTY; STRENGTH; MODEL;
D O I
10.1016/j.jallcom.2022.167755
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The 2195 Al-Cu-Li alloy is widely utilized for the fabrication of key aerospace vehicle components; hence, an in-depth understanding of its hot deformation behavior is essential for consistently achieving high-per-formance products. In this study, isothermal compression tests were performed on 2195 Al-Cu-Li alloy ingots in the temperature and strain rate ranges of 250-500 degrees C and 10-3-1 s-1, respectively. A processing map was established to predict the workability under different conditions. The corresponding micro-structures were examined to reveal their hot deformation mechanism. Results demonstrated that the processing map was divided into four distinct domains. The unstable zone was located in the 250-375 degrees C/ 10-1.5-1 s-1 and 250-275 degrees C/10-2.5-10-1.5 s-1, temperature/strain rate regimes, in which deformation bands and flow localization were observed. The deformation bands blocked dislocations and compromised the dynamic recrystallization (DRX) behavior, hence damaging the microstructure. Further, large coarse T1 phases precipitated in the 325-410 degrees C/10-2.5-10-3 s-1 regime, which led to the formation of heterogeneities in the microstructure, corresponding to a minimum workability in the processing map. The optimal hot -working domain for the 2195 alloy was determined to be 460-500 degrees C/10-3-10-2 s-1, and the dominating hot deformation mechanisms were DRX and dynamic recovery (DRV). Specifically, continuous and dis-continuous DRX behaviors dominated in the 300-400 degrees C/10-3 s-1 and 450-500 degrees C/10-3 s-1 regimes, re-spectively. DRX gradually weakened as the strain rate increased at 500 degrees C. Further, the weakening of DRX was only minimally affected by temperature at 400-500 degrees C during high-speed deformation (1 s-1). The results reported herein can provide valuable insights into the hot working of Al-Cu-Li alloys. (c) 2022 Elsevier B.V. All rights reserved.
引用
收藏
页数:16
相关论文
共 50 条
  • [31] Characterization of Hot Deformation Behavior of a Novel Al–Cu–Li Alloy Using Processing Maps
    Xin-Xiang Yu
    Yi-Ran Zhang
    Deng-Feng Yin
    Zhi-Ming Yu
    Shu-Fei Li
    Acta Metallurgica Sinica (English Letters), 2015, 28 : 817 - 825
  • [32] Characterization of Hot Deformation Behavior of a Novel Al–Cu–Li Alloy Using Processing Maps
    Xin-Xiang Yu
    Yi-Ran Zhang
    Deng-Feng Yin
    Zhi-Ming Yu
    Shu-Fei Li
    Acta Metallurgica Sinica(English Letters), 2015, 28 (07) : 817 - 825
  • [33] Microstructural Evolution and Dynamic Recrystallization Behavior of the Homogenized 2195 Al–Li Alloy During Hot Deformation
    Rong Fu
    Yuanchun Huang
    Yu Liu
    Hui Li
    Metals and Materials International, 2023, 29 : 2605 - 2622
  • [34] Hot tensile deformation behavior, fracture mechanism and microstructural evolution of 2195 Al-Li alloy
    Huang, Xiaomin
    Guan, Ben
    Wang, Baoyu
    Zang, Yong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 946
  • [35] Superplastic behavior of Al-Cu-Li based alloy
    杜予晅
    张新明
    叶凌英
    罗智辉
    Transactions of Nonferrous Metals Society of China, 2006, (S3) : 1379 - 1382
  • [36] Superplastic behavior of Al-Cu-Li based alloy
    Du Yu-xuan
    Zhang Xin-ming
    Ye Ling-ying
    Luo Zhi-hui
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1379 - S1382
  • [37] The hot deformation characteristics and the associated microstructural evolution of an Al-Cu-Li-Zn alloy studied by constitutive equations and processing maps
    Wang, Hua
    Yin, Dengfeng
    Zhao, Ming-Chun
    Tian, Yan
    Atrens, Andrej
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 401 - 418
  • [38] Microstructural evolution and mechanical performance of Al-Cu-Li alloy joined by friction stir welding
    Naumov, Anton
    Isupov, Fedor
    Rylkov, Evgenii
    Polyakov, Pavel
    Panteleev, Mikhail
    Skupov, Aleksey
    Amancio-Filho, Sergio T.
    Panchenko, Oleg
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (06): : 14454 - 14466
  • [39] Study of deformation-aging of Al-Cu-Li alloy containing Sc
    Zhou, Chang-Rong
    Pan, Qing-Lin
    Wang, Xin-Yu
    Liang, Wen-Jie
    Yin, Zhi-Min
    Jinshu Rechuli/Heat Treatment of Metals, 2004, 29 (10):
  • [40] Microstructural evolution and mechanical behaviors of Al-Cu-Li alloy processed by laser shock peening
    Wang, Jian
    Yang, Ke
    Bai, Zhi-hao
    Lu, Ya-lin
    Zhu, Xiu-rong
    Wang, Jun
    Pang, Song
    MATERIALS CHARACTERIZATION, 2022, 191