Influence of Surface Treatment and Accelerated Ageing on Biaxial Flexural Strength and Hardness of Zirconia

被引:1
|
作者
Rohr, Nadja [1 ]
Schonenberger, Angela Jacqueline [1 ]
Fischer, Jens [1 ]
机构
[1] Univ Basel, Univ Ctr Dent Med Basel UZB, Dept Reconstruct Dent, Biomat & Technol, CH-4058 Basel, Switzerland
关键词
zirconia implants; accelerated ageing; surface treatment; mechanical properties; OSTEOBLAST-LIKE CELLS; Y-TZP; MARTENS HARDNESS; TITANIUM; IMPLANTS; ROUGHNESS; CERAMICS;
D O I
10.3390/ma16030910
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The aim was to investigate how the surface treatment and the process of accelerated ageing of zirconia for dental implants affect the biaxial flexural strength and hardness. Zirconia discs with a diameter of 12.6 mm were subjected to either one of the following treatments: polishing (Zp); polishing and heat treatment at 1250 degrees C for 1 h (Zpt); machining (Zm); machining and heat treatment (Zmt); or sandblasting, acid-etching, and heat treatment (Z14) (n = 45 per group). Biaxial flexural strength and Martens hardness (HM) were measured without further treatment and after accelerated ageing for 5 h or 5 x 5 h according to ISO 13356 (n = 15 per group). Two-way ANOVA was applied to test the effect of surface treatment and ageing (alpha = 0.05). The reliability of the specimens was described with Weibull two-parameter distribution of biaxial flexural strength data. Overall, the surface treatment (p < 0.001) and ageing (p = 0.012) revealed a significant effect on biaxial flexural strength values, while HM was only affected by the surface treatment (p < 0.001) but not ageing (p = 0.160). Surface treatment significantly affected HM (p < 0.001) but not ageing (p = 0.160). The applied surface treatments affected the biaxial flexural strength and HM of zirconia. For accelerated ageing, a duration of both 5 h and 5 x 5 h is recommended to evaluate the effect of surface treatments. Zm was the most reliable surface as it was least affected by ageing and provided low standard deviations of biaxial flexural strength values.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] The effects of mechanical and hydrothermal aging on microstructure and biaxial flexural strength of an anterior and a posterior monolithic zirconia
    Munoz, Eduardo Mariscal
    Longhini, Diogo
    Antonio, Selma Gutierres
    Adabo, Gelson Luis
    JOURNAL OF DENTISTRY, 2017, 63 : 94 - 102
  • [42] The effect of surface treatment and low-temperature degradation on flexural strength of additive manufactured zirconia
    Kim, So-Hyun
    Oh, Nam -Sik
    Pang, Nan-Sim
    Jung, Bock-Young
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 148
  • [43] Effect of metal chloride solutions on coloration and biaxial flexural strength of yttria-stabilized zirconia
    Gye-Jeong Oh
    Kwangmin Lee
    Doh-Jae Lee
    Hyun-Pil Lim
    Kwi-Dug Yun
    Jae-Sam Ban
    Kyung-Ku Lee
    John G. Fisher
    Sang-Won Park
    Metals and Materials International, 2012, 18 : 805 - 812
  • [44] The effect of melt infiltration of borosilicate glass on biaxial flexural strength of porcelain-veneered zirconia
    Joo, Kyu Ji
    Song, Kyung Woo
    Jung, Jong Hyun
    Ahn, Hyo Jin
    Park, Il Song
    Lee, Min Ho
    Bae, Tae Sung
    METALS AND MATERIALS INTERNATIONAL, 2011, 17 (04) : 557 - 562
  • [45] The number of specimens in a furnace affects the biaxial flexural strength of veneered zirconia specimens after sintering
    Rippe, Marilia Pivetta
    de Melo, Renata Marques
    Duarte Moura, Dayanne Monielle
    Machado, Pablo Soares
    Assuncao Souza, Rodrigo Othavio
    Valandro, Luiz Felipe
    Bottino, Marco Antonio
    Oezcan, Mutlu
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2021, 35 (06) : 663 - 672
  • [46] Effect of metal chloride solutions on coloration and biaxial flexural strength of yttria-stabilized zirconia
    Oh, Gye-Jeong
    Lee, Kwangmin
    Lee, Doh-Jae
    Lim, Hyun-Pil
    Yun, Kwi-Dug
    Ban, Jae-Sam
    Lee, Kyung-Ku
    Fisher, John G.
    Park, Sang-Won
    METALS AND MATERIALS INTERNATIONAL, 2012, 18 (05) : 805 - 812
  • [47] Effect of Zirconia Core Thickness and Veneer Firing Cycle on the Biaxial Flexural Strength of Veneering Ceramic
    Alayad, Abdullah Saeed
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2020, 29 (01): : 26 - 33
  • [48] The influence of core-build up materials on biaxial flexural strength of strength-gradient zirconia and lithium disilicate ceramics: an in-vitro study
    Ereifej, Nadia S.
    Musa, Dina B.
    Oweis, Yara G.
    Abu-Awwad, Motasum
    Tabnjh, Abedelmalek K.
    SCIENTIFIC REPORTS, 2024, 14 (01):
  • [49] Influence of yttria content and surface treatment on the strength of translucent zirconia materials
    McLaren, Edward A.
    Maharishi, Anvita
    White, Shane N.
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 129 (04): : 638 - 643
  • [50] Influence of Surface Treatment on the Band Strength of Resin Cements to Monolithic Zirconia
    Elsaka, Shaymaa E.
    JOURNAL OF ADHESIVE DENTISTRY, 2016, 18 (05): : 387 - 395