HYDRATION AND EARLY MECHANICAL PERFORMANCE OF BELITE SULFOALUMINATE CEMENT CONTAINING MgAl2O4 FROM SOLID WASTE

被引:0
|
作者
Wang, Zengyao [1 ]
Liu, Hao [2 ]
Yu, Liang [1 ]
Yan, Jinghua [1 ]
Wu, Fengnian [1 ]
Wang, Shoude [1 ]
Zhao, Piqi [1 ]
Cheng, Xin [1 ]
机构
[1] Univ Jinan, Shandong Prov Key Lab Preparat & Measurement Bldg, Jinan 250022, Peoples R China
[2] China Railway Construct Grp Co Ltd, Shandong Branch, Jinan 266109, Peoples R China
关键词
Belite sulfoaluminate cement; Calcination; Setting time; Hydration; Compressive strength; FLY-ASH;
D O I
10.13168/cs.2023.0014
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study dealt with the use of gold tailings, red mud, bauxite, desulfurised gypsum and high magnesium limestone as the raw materials in the production of a belite sulfoaluminate cement clinker containing MgAl2O4. The hydration and early mechanical properties of this cement were characterised by isothermal calorimetry, a mechanical test, X-ray diffraction and a thermal analysis. The results showed that the optimal calcination temperature to obtain a satisfactory clinker strength was 1350 celcius and the corresponding 1, 3 and 7-day strengths were 27.7, 45.8 and 54.3 MPa, respectively. The initial and final setting times of the cements range between 20 and 31 minutes. The cements had the characteristics of rapid hardening and the main hydration products were AFt, AFm and AH3. The total hydration heat release of this cement within the first 50 hours was only 158 J center dot g-1, which could effectively avoid the generation of internal cracks in the cement and has the potential to be applied to large concrete projects. Furthermore, the MgAl2O4 mineral phase was inert in the belite sulfoaluminate cement and did not participate in the hydration reaction, which eliminates the disadvantage of MgO in the cement systems and potentially increases the use of high magnesium limestone in cement production.
引用
收藏
页码:167 / 173
页数:7
相关论文
共 50 条
  • [31] Hydration and mechanical properties of Portland cement containing eloxal waste from aluminium industry
    Erdem, E
    Günay, ME
    Donat, R
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2003, 136 (1-3) : 35 - 38
  • [32] Cyclic performance of cathode material LiMn2O4 with MgAl2O4 spinel doping
    Xiao, J
    Zhu, HL
    Chen, ZY
    Peng, ZD
    Hu, GR
    CHINESE JOURNAL OF INORGANIC CHEMISTRY, 2005, 21 (11) : 1719 - 1722
  • [33] Research on sintering performance and corrosion mechanism of whisker enhanced MgAl2O4 2 O 4 saggar
    Zhang, Hao
    Zhang, Han
    Xiao, Zixiu
    Li, Youqi
    Zhao, Huizhong
    CERAMICS INTERNATIONAL, 2024, 50 (22) : 47017 - 47023
  • [34] Effect of pretreated microstructure on subsequent sintering performance of MgAl2O4 ceramics
    Guo, Shengqiang
    Wang, Hao
    Xu, Pengyu
    Wang, Bin
    Xiong, Yan
    Tu, Bingtian
    Wang, Weimin
    Fu, Zhengyi
    CERAMICS INTERNATIONAL, 2019, 45 (06) : 7544 - 7551
  • [35] Exploring the hydration and shrinking behavior regulated by the superabsorbent polymers in superlight foamed cement made from solid waste-based sulfoaluminate cement
    Pang, Fangjie
    Zhang, Zuoyou
    Wang, Wenlong
    Wang, Zengmei
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 457
  • [36] The deposition of coke from methane on a Ni/MgAl2O4 catalyst
    Guo, Jianjun
    Lou, Hui
    Zheng, Xiaoming
    CARBON, 2007, 45 (06) : 1314 - 1321
  • [37] The effect of Pr substitution on the spectrum and photocatalytic performance of MgAl2O4 nanoparticles
    Yu, Z. J.
    Zhou, J. B.
    Xu, M. H.
    Yang, Y. F.
    Wang, Y. Y.
    DIGEST JOURNAL OF NANOMATERIALS AND BIOSTRUCTURES, 2024, 19 (04) : 1719 - 1735
  • [38] High-performance flash joining of MgAl2O4 transparent ceramics
    Li, Tianyu
    Liu, Yan
    Li, Gui
    Zhou, Hao
    Zhang, Keying
    Yang, Jinjing
    Liu, Xuejian
    Huang, Zhengren
    CERAMICS INTERNATIONAL, 2022, 48 (21) : 32561 - 32565
  • [39] Peculiar site preferences of B and Ga in MgAl2O4 spinet solid solutions
    Yoshiasa, Akira
    Sakai, Syunsuke
    Maekawa, Hideki
    Sugiyama, Kazumasa
    Nakatsuka, Akihiko
    Ito, Eiji
    ACTA CRYSTALLOGRAPHICA A-FOUNDATION AND ADVANCES, 2008, 64 : C500 - C501
  • [40] Study of the Synthesis of MgAl2O4 Spinel Refractory from Waste Chromium Slag of a Chrome Plant in China
    Meng, Jinxia
    Chen, Weiqing
    Zhao, Jizeng
    Liu, Li
    ENERGY TECHNOLOGY 2018: CARBON DIOXIDE MANAGEMENT AND OTHER TECHNOLOGIES, 2018, : 341 - 355