Long-term stability of PVDF-SiO2-HDTMS composite hollow fiber membrane for carbon dioxide absorption in gas-liquid contacting process

被引:3
|
作者
Pang, Honglei [1 ]
Qiu, Yayu [2 ]
Sheng, Weipeng [3 ]
机构
[1] Nanjing Vocat Univ Ind Technol, Nanjing 210023, Peoples R China
[2] Nanjing Vocat Coll Informat Technol, Nanjing 210023, Peoples R China
[3] Zhejiang Xinchai CO LTD, Shaoxing 312500, Peoples R China
关键词
CO2; ABSORPTION; POLY(VINYLIDENE FLUORIDE); PVDF MEMBRANE; SURFACE; NANOPARTICLES; PERFORMANCE; FABRICATION; SEPARATION; CAPTURE; LAYER;
D O I
10.1038/s41598-023-31428-8
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Hybrid polyvinylidene fluoride-silica-hexadecyltrimethoxysilane (PVDF-SiO2-HDTMS) membranes were fabricated via a non-solvent-induced phase-inversion method to create stable hollow-fiber membranes for use in the membrane contact absorption of carbon dioxide (CO2). The surface properties, performance characteristics, and long-term performance stability of the prepared membranes were compared and analyzed. The outer surfaces of the prepared membranes were superhydrophobic because of the formation of rough nanoscale microstructures on the surfaces and their low surface free energy. The addition of inorganic nanoparticles improved the mechanical strength of the PVDF-SiO2-HDTMS. Long-term stable operation experiments were carried out with a mixed inlet gas (CO2/N-2 = 19/81, v/v) at a flow rate of 20 mL/min. The absorbent liquid in these experiments was 1 mol/L diethanolamine (DEA) at a flow rate of 50 mL/min. The mass transfer flux of CO2 through the PVDF-SiO2-HDTMS membrane decreased from an initial value of 2.39 x 10(-3) mol/m(2)s to 2.31 x 10(-3) mol/m(2)s, a decrease of 3% after 20 days. The addition of highly stable and hydrophobic inorganic nanoparticles prevented pore wetting and structural damage to the membrane. The PVDF-SiO2-HDTMS membrane was found to have excellent long-term stable performance in absorbing CO2.
引用
收藏
页数:10
相关论文
共 45 条
  • [41] Experimental investigation of heat and moisture transfer performance of CaCl2/H2O-SiO2 nanofluid in a gas-liquid microporous hollow fiber membrane contactor
    Zheng, Yuanzhou
    Yang, Haoran
    Fazilati, Mohammad Ali
    Toghraie, Davood
    Rahimi, Hossein
    Afrand, Masoud
    INTERNATIONAL COMMUNICATIONS IN HEAT AND MASS TRANSFER, 2020, 113 (113)
  • [42] Hydrophobicity optimization of polypropylene hollow fiber membrane by sol–gel process for CO2 absorption in gas–liquid membrane contactor using response surface methodology
    Parya Amirabedi
    Reza Yegani
    Amir Hossein Hesaraki
    Iranian Polymer Journal, 2017, 26 : 431 - 443
  • [43] Effect of polymer extrusion temperature on poly(vinylidene fluoride) hollow fiber membranes: Properties and performance used as gas-liquid membrane contactor for CO2 absorption
    Ghasem, Nayef
    Al-Marzouqi, Mohamed
    Rahim, Nihmiya Abdul
    SEPARATION AND PURIFICATION TECHNOLOGY, 2012, 99 : 91 - 103
  • [44] Achieving long-term gas pressure stability in diffusion-cooled carbon dioxide (CO2) lasers by minimizing CO2 adsorption from 3Å molecular sieves with optimized cesium exchange rates
    T. Finke
    J. Serafińczuk
    R. Köhler
    W. Viöl
    Applied Physics A, 2025, 131 (4)
  • [45] Application of a water-energy-carbon coupling index to evaluate the long-term operational stability of the anaerobic-anoxic-oxic-membrane bioreactor (A2/O-MBR) process under the influence of rainstorms
    Yu, Lian
    Peng, Kaiming
    Huang, Yizhen
    Chen, Feng
    Chen, Shoubin
    Xia, Yulong
    Huang, Xiangfeng
    Ni, Xiaojing
    Guo, Ru
    Cai, Chen
    Liu, Jia
    WATER RESEARCH, 2024, 255