Reducing the cyclic tension-compression asymmetry and cyclic hardening of ZK61 magnesium alloy via the compression-extrusion process

被引:4
|
作者
Wang, Haixuan [1 ]
Chen, Wenzhen [1 ,2 ,4 ]
Wang, Wenke [1 ,2 ]
Fu, Zhichao [1 ]
Zhang, Wencong [1 ,3 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Weihai Lightweight Mat & Forming Engn Res Ctr, Weihai 264209, Peoples R China
[3] Harbin Inst Technol, Weihai Innovat Pk, Weihai 264209, Peoples R China
[4] Harbin Inst Technol, Sch Mat Sci & Engn, Room A301, Weihai 264209, Peoples R China
基金
中国国家自然科学基金;
关键词
Magnesium alloy; Cyclic tension-compression asymmetry; Cyclic hardening; Compression-extrusion process; Texture weakening; Grain refining; MECHANICAL-PROPERTIES; TEXTURE DEPENDENCE; DEFORMATION; FATIGUE; BEHAVIOR;
D O I
10.1016/j.msea.2023.145324
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to reduce the cyclic tension-compression asymmetry and cyclic hardening that exists widely in magnesium alloys, ZK61magnesium alloys with different texture intensities and grain sizes were fabricated by conventional extrusion and compression-extrusion process. It was found that the compression-extrusion process had a remarkable effect on the texture weakening and grain refining, which significantly improved monotonic tension-compression asymmetry and cyclic tension-compression asymmetry. Under their combined effects, the {10-12} twinning-detwinning behavior of ZK61 magnesium alloy during cyclic tension-compression deformation was effectively suppressed, resulting in a remarkable reduction of the difference of peak stresses in tension and compression. In the meantime, shape asymmetry embodied in a concave-up characteristic of the cyclic hysteresis loops was almost eliminated as the weakening of the detwinning-prismatic slip transition. Twinningpromoted dislocation pile-up and twinning-induced grain segmentation were significantly attenuated with texture weakening and grain refining, leading to a substantial weakening of cyclic hardening. Eventually, ZK61 magnesium alloy with low cyclic tension-compression.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Tension-Compression Asymmetry and Microstructure of Extruded AZ31 Magnesium Alloy
    Su, Hui
    Chu, Zhibing
    Xue, Chun
    Li, Yugui
    Ma, Lifeng
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (10): : 3446 - 3453
  • [22] Tension-compression asymmetry of the AZ91 magnesium alloy with multiheterogenous microstructure
    Sun, Jiapeng
    Yang, Zhenquan
    Liu, Huan
    Han, Jing
    Wu, Yuna
    Zhuo, Xiaoru
    Song, Dan
    Jiang, Jinghua
    Ma, Aibin
    Wu, Guosong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 759 : 703 - 707
  • [23] Tension-Compression Asymmetry and Microstructure of Extruded AZ31 Magnesium Alloy
    Su Hui
    Chu Zhibing
    Xue Chun
    Li Yugui
    Ma Lifeng
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (10) : 3446 - 3453
  • [24] Mechanical properties in cyclic tension-compression loading process on sheet metal
    Yu, Gaochao
    Ma, Rui
    Zhai, Ruixue
    Zhao, Jun
    PROCEEDINGS OF THE 17TH INTERNATIONAL CONFERENCE ON METAL FORMING METAL FORMING 2018, 2018, 15 : 1769 - 1776
  • [25] Observations of tension/compression asymmetry in the cyclic deformation of aluminum alloy 7075
    Meininger, JM
    Dickerson, SL
    Gibeling, JC
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1996, 19 (01) : 85 - 97
  • [26] RESEARCH ON THE TENSION-COMPRESSION ASYMMETRY OF AS-EXTRUDED ZK60 MAGNESIUM ALLOYS AT ROOM TEMPERATURE
    Lin Jinbao
    Ren Weijie
    Wang Xinyi
    ACTA METALLURGICA SINICA, 2016, 52 (03) : 264 - 270
  • [27] Microstructure of NiTi shape memory alloy due to tension-compression cyclic deformation
    Xie, ZL
    Liu, Y
    Van Humbeeck, J
    ACTA MATERIALIA, 1998, 46 (06) : 1989 - 2000
  • [28] Influence of cyclic extrusion and compression on the mechanical property of Mg alloy ZK60
    Wang Qudong
    Lin Jinbao
    Peng Liming
    Chen Yongjun
    ACTA METALLURGICA SINICA, 2008, 44 (01) : 55 - 58
  • [29] Reducing the tension-compression yield asymmetry in a Mg-8Al-0.5Zn alloy via precipitation
    Jain, J.
    Poole, W. J.
    Sinclair, C. W.
    Gharghouri, M. A.
    SCRIPTA MATERIALIA, 2010, 62 (05) : 301 - 304
  • [30] Fatigue damage development in pure polycrystalline magnesium under cyclic tension-compression loading
    Yu, Qin
    Zhang, Jixi
    Jiang, Yanyao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (25-26): : 7816 - 7826