Cracking and Microstructure Transition of Iron Ore Containing Goethite in Fe-C Melt Based on the HIsmelt Process

被引:6
|
作者
Wang, Guilin [1 ]
Zhang, Jianliang [1 ]
Liu, Zhengjian [1 ]
Tan, Yubo [1 ]
Wang, Yaozu [2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Intelligence Sci & Technol, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
crack; iron ore; micro-CT; non-blast furnace ironmaking; thermal decomposition; smelting reduction; THERMAL-DECOMPOSITION BEHAVIOR; SMELTING REDUCTION; MOLTEN IRON; CHROMIUM ORE; HEMATITE; KINETICS; MECHANISM; DISSOLUTION; PELLETS; CARBON;
D O I
10.3390/min13030448
中图分类号
P3 [地球物理学]; P59 [地球化学];
学科分类号
0708 ; 070902 ;
摘要
The phenomenon of cracking and deterioration of iron ore particles is a widespread scientific problem in the field of mineral processing and metallurgy. In this paper, the thermal decomposition properties of iron ore were investigated by a non-isothermal method using thermogravimetric equipment, and the crack evolution behavior of iron ore within Fe-C melt was investigated experimentally, by scanning electron microscopy and Micro-CT. The results show that the start decomposition temperature of #2 iron ore is 292.7 degrees C, which is 37.3 degrees C higher compared to that of #1 iron ore, because of its smaller pores and the difficulty of water vapor diffusion. The initial decomposition of iron ore is the decomposition goethite to form water vapor, and as heat transfer continues, hematite particles break into smaller particles and decompose to form Fe3O4. During the smelting reduction process, the Crack index (CI) of #1 iron ore was 5.50% at 4 s, and the CI index increased to 23.54% when time was extended to 16 s, and the internal evolved from locally interconnected holes to cracked structure. The iron ore maintains a relatively intact form during reduction within the Fe-C melt, and interfacial reduction reaction is dominant in the later stage.
引用
收藏
页数:15
相关论文
共 46 条
  • [21] Iron-Based Nanopowders Containing α-Fe, Fe3C, and γ-Fe Particles Synthesised in Microwave Torch Plasma and Investigated with Mossbauer Spectroscopy
    David, Bohumil
    Pizurova, Nadezda
    Schneeweiss, Oldrich
    Kudrle, Vit
    Jasek, Ondrej
    Synek, Petr
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2011, 50 (08)
  • [22] Treatment of overhaul wastewater containing N-methyldiethanolamine (MDEA) through modified Fe-C microelectrolysis-configured ozonation: Investigation on process optimization and degradation mechanisms
    Wang, Bing
    Tian, Kun
    Xiong, Xingaoyuan
    Ren, Hongyang
    JOURNAL OF HAZARDOUS MATERIALS, 2019, 369 : 655 - 664
  • [23] Evaluating strength, hydration characteristics, microstructure evolution, and sustainability of seawater-sea sand cement-based materials containing iron ore tailings
    Li, Huawei
    Liu, Feng
    Zhen, Hao
    Xiong, Zhe
    Song, Yuying
    Wang, Jinhua
    Li, Lijuan
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 457
  • [24] Crystallization process, microstructure, thermal behavior, and magnetic properties of melt-spun Fe86Cr6P6C2 ribbons
    Abadlia, L.
    Daoudi, M. I.
    Alleg, S.
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2023, 129 (07):
  • [25] Crystallization process, microstructure, thermal behavior, and magnetic properties of melt-spun Fe86Cr6P6C2 ribbons
    L. Abadlia
    M. I. Daoudi
    S. Alleg
    Applied Physics A, 2023, 129
  • [26] Efficient development of ultra-low-grade iron ore by hydrogen-based mineral phase transformation: Magnetic transition, phase transformation, and microstructure evolution
    Zhang, Xiaolong
    Niu, Zhifang
    Zhang, Qiang
    Yuanxing, Yue
    Gao, Peng
    Han, Yuexin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2025, 97 : 757 - 765
  • [27] Microstructure and property of laser clad Fe-based composite layer containing Nb and B4C powders
    Wang, Kaiming
    Du, Dong
    Liu, Guan
    Chang, Baohua
    Ju, Jiang
    Sun, Shuting
    Fu, Hanguang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 802 : 373 - 384
  • [28] Iron-carbon (Fe-C) micro-electrolysis coupling with anaerobic-anoxic-oxic (A2/O) process: Nitrogen and phosphorus removal performance and microbial characteristics
    Duan, Chongsen
    Huang, Xiao
    Gao, Jingsi
    Zhou, Yuqi
    Chen, Na
    Zhu, Jia
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2022, 10 (02):
  • [29] Pulse electric current sintering behavior of atomized cast-iron powder of Fe-C system containing hypo-eutectic carbon (III) -mechanical properties of atomized cast-iron porous sintered body
    Tomino, Hisakazu
    Kondo, Yoshihito
    Katsumura, Munehide
    Tojo, Tetsuro
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 1998, 45 (08): : 715 - 720
  • [30] Scanning Electron Microscope-Energy Dispersive X-Ray (SEM-EDX) Study of Fe-C Catalyst from Iron Sand and Biochar for Advance Oxidation Process (AOPs)
    Pitoyo, Joko
    Jamilatun, Siti
    INTERNATIONAL JOURNAL OF RENEWABLE ENERGY RESEARCH, 2024, 14 (04): : 804 - 813