Effect of natural aging on the tensile properties and the toughness of friction stir welds of 2024-T3 aluminum alloy

被引:5
|
作者
Djili, Abderrahmane [1 ]
Bezzazi, Boudjema [1 ]
Zioui, Nadjet [2 ]
Haboussi, Mohamed [3 ]
机构
[1] Univ Mhamed Bougara, Unite Rech Mat Procedes & Environm UR MPE, Boumerdes, Algeria
[2] Univ Quebec Trois Rivieres, Dept Genie Mecan, Trois Rivieres, PQ, Canada
[3] Univ Sorbonne Paris Nord, LSPM, CNRS, UPR3407, F-93430 Villetaneuse, France
关键词
Aluminum alloy2024-T3; Friction stir welding; Natural aging; Toughness; MECHANICAL-PROPERTIES; HEAT-TREATMENT; AL-ALLOY; BEHAVIOR; MICROSTRUCTURE; AA7075;
D O I
10.1016/j.jajp.2023.100153
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
During friction stir welding of metallic alloys, four different microstructure zones are formed in the weld, resulting in heterogeneous mechanical properties in this latter. In the case of aluminum alloys, these properties are bound to change with aging, whether natural or artificial. In this study, changes in the toughness and tensile behavior of friction stir welds in Al 2024-T3 alloy over time are investigated. Only specimens found to be defect free, by X-ray imaging, are tested. Characterized by the area under the stress-strain curve of the material, the toughness is found to be 19% lower after 24 months of natural aging. This decrease in toughness is mainly due to a loss of ductility as the elongation of the material drops by 27% while the ultimate tensile strength increases by 9%. The fracture zone and pattern remain the same for both natural aged and freshly welded specimens. These results can be used to estimate the service life of structures using such a material, as in aeronautics.
引用
收藏
页数:6
相关论文
共 50 条
  • [41] Filiform investigations on aluminum alloy 2024-T3
    Kloet, JV
    Schmidt, W
    Hassel, AW
    Stratmann, M
    CORROSION AND CORROSION PROTECTION, 2001, 2001 (22): : 885 - 890
  • [42] Characterization of 2024-T3: An aerospace aluminum alloy
    Huda, Zainul
    Taib, Nur Iskandar
    Zaharinie, Tuan
    MATERIALS CHEMISTRY AND PHYSICS, 2009, 113 (2-3) : 515 - 517
  • [44] Natural aging in friction stir welded 7136-T76 aluminum alloy
    Kalemba, Izabela
    Hamilton, Carter
    Dymek, Stanislaw
    Materials and Design, 2014, 60 : 295 - 301
  • [45] Macrostructures and mechanical properties of ultrasonic-assisted friction stir welding joint of 2024-T3 aluminium alloy
    高嵩
    钟益斌
    武传松
    China Welding, 2015, 24 (03) : 24 - 28
  • [46] Natural aging in friction stir welded 7136-T76 aluminum alloy
    Kalemba, Izabela
    Hamilton, Carter
    Dymek, Stanislaw
    MATERIALS & DESIGN, 2014, 60 : 295 - 301
  • [47] Microstructure and mechanical properties of friction stir welded AA2024-T3 aluminum alloy
    Khodir, SA
    Shibayanagi, T
    Naka, M
    MATERIALS TRANSACTIONS, 2006, 47 (01) : 185 - 193
  • [48] Microstructure and Mechanical Properties of Friction Stir Welds on 6063-T6 Aluminum Alloy
    Jing H.
    Feng Q.
    Xu L.
    Zhao L.
    Han Y.
    Jixie Gongcheng Xuebao/Journal of Mechanical Engineering, 2020, 56 (08): : 13 - 19
  • [49] The tensile deformation and fracture behavior of friction stir welded aluminum alloy 2024
    Srivatsan, T. S.
    Vasudevan, Satish
    Park, Lisa
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 466 (1-2): : 235 - 245
  • [50] Effect of Exfoliation Corrosion on the Mechanical Properties of Friction Stir Spot Welded 2024-T3 AA Joints
    Gardi R.H.
    Kadauw A.
    Hanschel B.
    Advances in Materials Science and Engineering, 2023, 2023